Zeron 100 khoom yog dab tsi?

Nov 20, 2025

Tso lus

Zeron 100 khoom yog dab tsi?

Zeron 100 yog super duplex stainless hlau tsim los ntawm Rolled Alloys. Cov alloy no nthuav tawm zoo heev corrosion kuj thiab siab zog. Nws feem ntau muaj 25% chromium, 7% nickel, thiab 3.6% molybdenum, nrog ntxiv tooj liab thiab tungsten. Nws tuaj yeem ua tiav rau hauv ntau hom khoom siv, nrog rau cov phaj, coils, raj, tuav, thiab xaim.

 

Zeron 100 sib npaug li cas?

Zeron 100 yog super duplex stainless hlau nrog UNS S32760 raws li nws qhov sib npaug. Lwm qhov sib npaug sib npaug xws li Werkstoff Nr. 1.4501, thiab ntau yam ASTM thiab ASME cov qauv xws li ASTM A890, ASTM A995, thiab ASME SA351/995 rau castings. Rau cov khoom zoo sib xws, koj tuaj yeem xav txog Duplex 2507, uas yog ib tus txheeb ze ze, txawm tias Zeron 100 muaj ntau dua tooj liab thiab tungsten me ntsis.

 

Zeron 100 tshuaj muaj pes tsawg leeg

Cr Ni Mo C W Cu N Mn Si P S Fe

24.0-26.0

6.0-8.0

3.0-4.0

0.030 Max

0.5-1.0

0.50-1.0

0.2-0.3

Max 1.00 Nws

1.0 Max

0.03 Max

0.01 Max

Tshuav

 

ASTM Cov Lus Qhia

Tube & Tube Ntawv / phaj Bar

A790, A928, A789

A240

A276

 

ZERON 100 cov khoom siv

Chav ntsuas kub, tshuaj Annealed Condition

Tensile zog, ksi .2% Yield zog, ksi % Elongation hauv 50mm Hardness Max.

109

80

25

28 HRC

 

ZERON 100 Machinability

ZERON 100 combines zoo machinability nrog durability. Nws hardness ranges ntawm 260-290 HBW. Thaum nws qhov kev ua tau zoo ruaj khov nyob rau hauv qis mus rau nruab nrab qhov kub thiab txias (-50℃txog 300 degree), nws lub zog tuaj yeem txo qis dua 300℃vim kev ntxhov siab corrosion nag lossis daus, ua rau nws tsis tsim nyog rau kev siv mus sij hawm ntev hauv ib puag ncig saum toj no qhov kub thiab txias.

 

Puas yog Zeron 100 magnetic?

Tsis yog, Zeron 100 tsis yog hlau nplaum. Zeron 100 yog ib qho super duplex stainless hlau uas feem ntau tsis yog- sib nqus, txawm hais tias qee qhov kev sib nqus me me tuaj yeem tshwm sim hauv thaj chaw uas cov khoom tau txias heev - ua haujlwm. Nws tsis tshua muaj magnetic permeability ua rau nws haum rau cov ntawv thov uas sib nqus cuam tshuam yuav tsum zam.

 

Qhov txawv ntawm Zeron 100 thiab 2507 yog dab tsi?

Zeron 100 (tseem hu ua UNS S32760) thiab 2507 (UNS S32750) yog ob qho tib si super duplex stainless hlau, tab sis Zeron 100 muaj qhov corrosion kuj me ntsis vim yog ntxiv tooj liab thiab tungsten. Zeron 100 yog tsim los kom muaj kev tiv thaiv ntau dua rau kev dav dav thiab pitting corrosion thiab tau teev tseg nrog cov txiaj ntsig tsawg kawg nkaus thiab lub zog tensile yuav tsum nyob thoob plaws txhua ntu piv rau 2507.

 

UNS S32760 vs UNS S32750

S32750 muaj ntau dua chromium, molybdenum, thiab nitrogen cov ntsiab lus, ua rau muaj zog tensile zog me ntsis thiab tsis kam mus rau kev corrosion, pitting, thiab crevice corrosion. S32760 muaj ntau dua tooj liab thiab tungsten cov ntsiab lus, uas txhim kho nws cov corrosion kuj nyob rau hauv corrosive ib puag ncig, tshwj xeeb tshaj yog ib co acidic ib puag ncig, thiab muab nws ib tug ntau elongation.

 

Yog tias koj muaj ib qhov project xav tau rau Zeron 100 stainless hlau tuav, thov koj xav tso qhov kev txiav txim. GNEE Stainless yog cov khoom lag luam ywj pheej thiab cov txheej txheem ntawm Zeron 100 stainless hlau. Nrog rau cov khoom lag luam loj thiab muaj peev xwm ua tau zoo, peb tuaj yeem ua tau raws li qhov xav tau ntawm feem ntau cov haujlwm, txawm tias lawv yog cov khoom lag luam lossis cov khoom lag luam. Peb muab: Tshuag ntau thiab tsawg ntawm daim ntawv thiab slab, Tshuag lengths ntawm puag ncig tuav, tsau ntev daim ntawv thiab slab, tsau ntev puag ncig tuav, txias sib sau ntawm daim ntawv thiab slab thiab puag ncig tuav, thiab lwm yam tsim nyog kev pab cuam. Yog muaj lus nug, thov emailsales@gneestainless.com