Dab tsi yog qhov txawv ntawm 1.4541 thiab 1.4301 khoom?

Nov 18, 2025

Tso lus

1.4301 Stainless hlau yog dab tsi?

1.4301 stainless hlau yog austenitic, chromium-nickel stainless hlau, tseem hu ua AISI 304 lossis V2A. Nws yog cov khoom siv ntau yam thiab siv dav vim nws zoo heev corrosion thiab kub tsis kam, zoo formability, thiab weldability. Qhov no ua rau nws tsim nyog rau ntau yam kev siv, los ntawm cov khoom siv hauv tsev xws li cutlery thiab dab dej rau cov khoom siv, architecture, thiab cov cuab yeej kho mob.

 

1.4541 Stainless hlau yog dab tsi?

TS EN 1.4541, tseem hu ua X6CrNiTi18-10 lossis AISI 321, yog titanium-stabilized austenitic stainless hlau. Nws yog tsim los muab kev zoo dua intergranular corrosion kuj thaum lub sij hawm thiab tom qab vuam, tshwj xeeb tshaj yog nyob rau hauv siab kub. Qhov sib ntxiv ntawm titanium (Ti Ntau dua lossis sib npaug li 5 × C) khi cov pa roj carbon thiab tiv thaiv chromium carbide nag lossis daus.

 

Cov khoom siv dab tsi yog 1.4301 sib npaug rau stainless hlau?

Khoom siv 1.4541 yog sib npaug rau AISI 321 stainless hlau. Nws yog titanium-stabilized austenitic stainless hlau nrog zoo heev tsis kam mus rau intergranular corrosion, zoo siab - kub lub zog, thiab zoo oxidation kuj. Yog li ntawd, nws yog ib qho tsim nyog lwm txoj rau 304 qib stainless hlau thaum post-weld annealing tsis tau lossis daim ntawv thov kub ntawm 425-900℃.

Txuj 1.4301 Ib 1.4541 Ib
EN (DIN) X5CrNi18-10 X6CrNiTi18-10
ASTM / AISI 304 321
UNS S30400 S32100
JIS SUS 304 SUS 321
ISO 11Cr18Ni10 11Cr18Ni10 Ti
GB (Tuam Tshoj) 06Cr19Ni10 06Cr18Ni11 Ti

 

1.4301 vs . 1.4541 Stainless hlau: Tshuaj muaj pes tsawg leeg

Lub ntsiab 1.4301 (AISI 304) 1.4541 (AISI 321)
Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.07% Tsawg dua lossis sib npaug li 0.08%
Chromium (Cr) 17.5–19.5% 17.0–19.0%
Nickel (Ni) 8.0–10.5% 9.0–12.0%
Titanium (Ti)

Ntau dua lossis sib npaug li 5 × C (feem ntau 0.5%)

 

1.4301 vs . 1.4541 Stainless Steel: Mechanical Properties

Khoom 1.4301 (AISI 304) 1.4541 (AISI 321)
Tensile zog (MPa) Ntau dua lossis sib npaug li 520 Ntau dua lossis sib npaug li 500
Yield zog (MPa) Ntau dua lossis sib npaug li 210 Ntau dua lossis sib npaug li 200
Elongation (%) Ntau dua lossis sib npaug li 45 Ntau dua lossis sib npaug li 40
Hardness (HB) Tsawg dua lossis sib npaug li 215 Tsawg dua lossis sib npaug li 215

 

Dab tsi yog qhov txawv ntawm 1.4541 thiab 1.4301 khoom?

Qhov sib txawv tseem ceeb yog tias 1.4541 (AISI 321) yog titanium -stabilized stainless hlau, thaum 1.4301 (AISI 304) tsis yog. Qhov no ua rau 1.4541 tiv taus ntau dua rau intergranular corrosion tom qab vuam lossis kub kub vim tias titanium khi nrog carbon, tiv thaiv kev tsim ntawm chromium carbides. Raws li qhov tshwm sim, 1.4541 yog qhov zoo dua rau cov qauv welded thiab cov ntawv thov uas muaj qhov kub thiab txias, thaum 1.4301 yog ib qho dav dav -lub hom phiaj steel rau qis- qhov kub thiab txias.

 

1.4307 SS tuaj yeem hloov 1.451 stainless hlau?
1.4307 (304L) yog ib qho qis- carbon stainless hlau uas tau hloov pauv ntau ntawm 1.4541 (321) vim nws qhov sib piv tsis kam rau intergranular corrosion, txhim kho machinability vim tsis muaj titanium, superior nto tiav, thiab txhim kho weldability.

 

Yog tias koj muaj ib qhov project xav tau rau 321 1.4541 stainless hlau bar, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Peb ua cov kab no rau hauv ntau hom khoom siv, nrog rau cov ntawv, coil, raj, bar, thiab hlau. Rau cov ncauj lus kom ntxaws tshuaj muaj pes tsawg leeg thiab kuaj dawb, thov hu rau peb lub Hoobkas hnub no. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email:sales@gneestainless.com

321 1.4541 stainless steel bar