UNS S43100 Stainless hlau

Feb 27, 2026

Tso lus

Kev piav qhia

UNS S43100 yog npib tsib xee-cov kabmob martensitic stainless hlau nrog txhim kho toughness, ductility, thiab corrosion kuj piv rau tus qauv 410 thiab 420. Nws muab lub zog siab tom qab kev kho cua sov nrog zoo corrosion kuj, ua rau nws haum rau siab - kev nyuaj siab structural Cheebtsam. Nws yog sib nqus thiab muaj kev sib zog zoo dua li lwm qib martensitic, zoo tagnrho rau cov ntawv thov uas yuav tsum tau muaj zog thiab kav ntev.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.20, Cr: 15.00–17.00, Ni: 1.25–2.50, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.040, S Tsawg dua lossis sib npaug 0.030

Mechanical Properties

Tensile Strength Ntau dua los yog sib npaug rau 725 MPa, Yield Strength Ntau dua lossis sib npaug rau 515 MPa, Elongation Ntau dua lossis sib npaug li 15%, Hardness Tsawg dua lossis sib npaug rau 241 HB

Qhov zoo

Siab zog thiab toughness; corrosion kuj zoo dua 410/420; kub- kho tau; Sib nqus.

Daim ntawv thov

Shafts, gears, li qub, twj, aerospace Cheebtsam, fasteners, thiab siab -stress mechanical qhov chaw.

Qib sib npaug

AISI 431, EN 1.4057, GB 17Cr16Ni2

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug