UNS S44000 Stainless hlau
Feb 27, 2026
Tso lus
Kev piav qhia
UNS S44000 yog siab - carbon martensitic stainless hlau nrog siab hardness, zoo heev hnav tsis kam, thiab nruab nrab corrosion kuj. Nws muaj chromium thiab molybdenum rau kev txhim kho pitting tsis kam piv rau 410 thiab 420. Nws tuaj yeem ua cua sov-kho kom siab tawv heev thiab dav siv hauv siab - hnav daim ntaub ntawv. Nws yog hlau nplaum thiab muaj kev ua tau zoo nyob rau hauv qhov chaw me me corrosive, tab sis tsis zoo tagnrho rau cov mob hnyav chloride.
Chemical Composition (wt%)
C: 0.60–0.95, Cr: 16.00–18.00, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.045, S Tsawg dua lossis sib npaug 0.030, Mo Less dua lossis sib npaug 1.25
Mechanical Properties
Tensile Strength Ntau dua los yog sib npaug rau 760 MPa, Yield Strength Ntau dua lossis sib npaug rau 550 MPa, Elongation Ntau dua lossis sib npaug li 10%, Hardness Tsawg dua lossis sib npaug rau 269 HB
Qhov zoo
Hardness heev thiab hnav tsis kam; kub- kho tau; zoo polishability; Sib nqus; nruab nrab corrosion kuj.
Daim ntawv thov
Bearings, li qub, cov cuab yeej txiav, cov cuab yeej precision, riam, thiab siab - coj cov khoom siv tshuab.
Qib sib npaug
AISI 440, EN 1.4116 / 1.4125
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug