SUS316L yog qhov qis-carbon iteration ntawm SUS316, optimized rau welded Cheebtsam nyob rau hauv chloride- nplua nuj ib puag ncig. Nrog rau cov ntsiab lus carbon capped ntawm 0.03%, nws tiv thaiv intergranular corrosion nyob rau hauv lub tshav kub- cuam tshuam cheeb tsam thaum vuam, tshem tawm qhov xav tau rau ncej-weld annealing. Qib no tau txais txiaj ntsig ntawm molybdenum- txhim kho corrosion kuj ntawm SUS316, muab kev ntseeg tsis sib haum xeeb rau cov qauv welded hauv ib puag ncig hnyav. Nws boasts txhim kho ductility thiab weld kev ncaj ncees piv rau SUS316, ua nws tus qauv kub rau cov khoom siv tseem ceeb hauv kev lag luam tshuaj lom neeg, dej hiav txwv, thiab kev lag luam tshuaj qhov twg corrosion tsis ua haujlwm.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.03, Cr: 16.00-18.50, Ni: 10.00-14.00, Mo: 2.00-3.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.04 lossis sib npaug 0.005,
Mechanical Properties (Annealed State)
Tensile Strength Ntau dua los yog sib npaug rau 480 MPa, Yield Strength Ntau dua lossis sib npaug rau 175 MPa, Elongation Ntau dua lossis sib npaug li 40%, Hardness Tsawg dua lossis sib npaug rau 215 HB
Core Zoo
Kev ua haujlwm ruaj khov corrosion hauv thaj chaw weld yam tsis muaj kev tshaj tawm - kho; superior intergranular corrosion kuj; tag nrho chloride tiv thaiv ntawm SUS316; zoo heev weldability thiab ductility; tsis yog-magnetic; zoo tagnrho rau hnyav welded corrosive Cheebtsam.
Tej kev siv
Chemical storage tanks, offshore platform Cheebtsam, cov khoom siv kho mob, welded heat exchangers, pharmaceutical pipelines, thiab marine nkoj fittings.
Qib sib npaug
AISI 316L, UNS S31603, EN 1.4404, GB 022Cr17Ni12Mo2.
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.