STS316L - Ultra-Low Carbon Austenitic Alloy Rau Welded Structures hauv Corrosive Ib puag ncig

Mar 30, 2026

Tso lus

Txheej txheem cej luam

STS316L yog ib qho ultra- cov pa roj carbon tsawg ntawm STS316, nrog cov ntsiab lus carbon tsawg dua lossis sib npaug li 0.03% uas tshem tawm qhov kev pheej hmoo ntawm kev sib tsoo ntawm kev sib tsoo tom qab vuam lossis siab - qhov kub thiab txias. Zoo li STS316, nws muaj 2.00-3.00% molybdenum rau superior pitting thiab crevice corrosion kuj nyob rau hauv chloride ib puag ncig, thiab 16.00-18.00% chromium ntxiv rau 10.00-14.00% npib tsib xee los tsim cov qauv austenitic ruaj khov. Nws yog non-magnetic, muaj ductility zoo heev, formability, thiab weldability, thiab yuav tsum tsis muaj kev kho cua sov tom qab vuam, ua rau nws zoo tagnrho rau loj welded lug nyob rau hauv hnyav corrosive ib puag ncig. Nws cov ntsiab lus qis carbon kuj tseem txhim kho nws cov tawv nqaij, tshwj xeeb tshaj yog nyob rau qhov kub thiab txias.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.03, Cr: 16.00-18.00, Ni: 10.00-14.00, Mo: 2.00-3.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.040, sib npaug 0.040 lossis sib npaug sib 0.10

Tej yam cuab yeej cuab tam (Annealed Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug li 485 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 170 MPa; Elongation (A): Ntau dua lossis sib npaug li 40%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 217

Core Zoo

Ultra- cov ntsiab lus carbon tsawg tiv thaiv intergranular corrosion tom qab vuam; tsis muaj kev tshaj tawm -weld cua sov yuav tsum tau kho; zoo heev pitting thiab crevice corrosion kuj nyob rau hauv ib puag ncig chloride; tsis yog- sib nqus thiab siab ductility; zoo weldability thiab formability; superior qis-kub toughness; haum rau loj welded lug thiab hnyav corrosive daim ntaub ntawv.

Daim ntawv thov

Loj welded chemical cia tanks, seawater desalination khoom, tshuaj thiab zaub mov ua pipelines, offshore platform Cheebtsam, cryogenic cia cov hlab ntsha, thiab cov cuab yeej kho mob yuav tsum tau muaj corrosion kuj thiab weldability.

Qib sib npaug

EN 1.4404, UNS S31603, GB 022Cr17Ni12Mo2, AISI 316L, SUS316L

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips