Yog tias koj tab tom yuav 316 stainless hlau kav, ib qho tseem ceeb tshaj plaws kom nkag siab yog cov yeeb nkab tuab, feem ntau hu ua yeeb nkab teem caij (SCH). Xaiv qhov raug thickness ncaj qha cuam tshuam rau lub siab ua haujlwm, durability, thiab qhov project nqi.

Hauv phau ntawv qhia no, peb piav qhia cov txheej txheem thickness ranges, specifications, thiab yuav ua li cas xaiv txoj kev xaiv rau koj daim ntawv thov.

 

Dab tsi yog SS 316 stainless hlau tubing?

SS 316 yog austenitic stainless hlau uas muaj molybdenum (2.0% - 2.5%). Piv rau SS 304, nws muaj kev tiv thaiv zoo tshaj rau cov tshuaj chloride, kua qaub, thiab dej hiav txwv corrosion, ua rau nws haum rau cov tshuaj thiab petrochemical pipelines, tshav kub exchangers thiab siab piping, marine thiab offshore lug, thiab zaub mov thiab kws ua kab.

 

Dab tsi yog Thickness ntawm 316 Stainless Hlau Yeeb Nkab?

Phab ntsa tuab ntawm 316/316L stainless hlau kav nws txawv heev nyob ntawm daim ntawv thov tshwj xeeb; rau cov kev qhia tshwj xeeb, phab ntsa tuab feem ntau yog li ntawm 0.6 hli mus rau 12.7 hli (kwv yees li 0.024 "mus rau 0.5"), txawm hais tias hnyav - cov kav dej muaj peev xwm ua rau phab ntsa tuab tshaj 50 hli. Cov yeeb nkab phab ntsa tuab feem ntau txhais los ntawm "Schedule" tooj (xws li Sch 5S, 10S, 40S, 80S), nrog rau cov Nominal Pipe Size (NPS) specifications spanning a range from 1/8" to 36".

SCH 5 / SCH 10 → Nyias phab ntsa (lub teeb yuag, tsis tshua muaj siab)
SCH 40 → Txheem thickness (kev siv dav dav)
SCH 80 → Thick wall (kev siv siab)
SCH 160 / XXS → Ntxiv tuab (hnyav heev)

Qhov tseeb phab ntsa thickness txawv nyob ntawm cov yeeb nkab txoj kab uas hla (NPS).

 

Qhov txawv ntawm ASME B36.19 thiab ASME B36.10 yog dab tsi?

Hauv kev lag luam stainless hlau, tuab yog tswj hwm los ntawm Schedule (Sch) system, feem ntau txhais los ntawm ASME B36.19 (rau stainless) thiab ASME B36.10 (rau carbon steel).

Rau ib qho twg muab Nominal Pipe Size (NPS), Sab Nraud Diameter (OD) tseem nyob tas li, tsis hais qhov tuab. Raws li tus lej Teem caij nce (xws li, los ntawm Sch 10S mus rau Sch 80S), phab ntsa thickness yuav loj dua, thiab Internal Diameter (ID) txo.

316 Stainless hlau yeeb nkab Thickness daim ntawv

NPS (Inches) Sab nraud txoj kab uas hla (mm) Sch10S (mm) Sch40S (mm) Sch80S (mm)
1/8" 10.3 1.24 1.73 2.41
1/4" 13.7 1.65 2.24 3.02
3/8" 17.1 1.65 2.31 3.20
1/2" 21.3 2.11 2.77 3.73
3/4" 26.7 2.11 2.87 3.91
1" 33.4 2.77 3.38 4.55
1-1/2" 48.3 2.77 3.68 5.08
2" 60.3 2.77 3.91 5.54
3" 88.9 3.05 5.49 7.62
4" 114.3 3.05 6.02 8.56
6" 168.3 3.40 7.11 10.97

 

Qhov txawv ntawm 316 SCH 40 yeeb nkab thiab SCH 80 yog dab tsi?

Thawj qhov sib txawv ntawm Schedule 40 (SCH 40) thiab Schedule 80 (SCH 80) cov kav dej ua los ntawm 316 cov khoom nyob rau hauv qhov tseeb tias SCH 80 nta cov phab ntsa tuab dua thiab cov kab me me, thiab muaj qhov ntsuas siab dua SCH 40. SCH 40 feem ntau suav hais tias yog cov qauv kev qhia tshwj xeeb 8} raws li kev siv qis dua 80- txawv los ntawm nws qhov kev txhim kho lub zog thiab kev ua haujlwm ntev-yog tsim tshwj xeeb rau kev lag luam ib puag ncig uas muaj kev kub siab, hnyav hnyav, lossis cov kab mob corrosive heev.

 

Dab tsi yog "12.5% ​​Wall Tolerance" hauv ASTM A312?

According to the ASTM A312 standard for seamless stainless steel pipe, the wall thickness is allowed a negative tolerance of 12.5%. For example, if the nominal thickness is 10mm, a pipe arriving at 8.75mm is technically compliant. If your safety code requires a strict minimum, you must specify "Minimum Wall" instead of "Nominal Wall."

 

Ntawm GNEE, peb yog ntau tshaj li cov kav dej xa khoom; peb muab "npaj-rau-siv" piping solutions. Txawm hais tias koj yog lub luag haujlwm rau kev kaw thiab kev saib xyuas, kev cog qoob loo tshuaj lom neeg, lossis siab -txoj haujlwm sab nraud, peb muaj ntau yam ntawm 316 stainless hlau cov khoom ua raws li ASTM A312 / A213 cov qauv.

 

Daim ntawv khoom Technical Specifications Loj & Teem caij ntau yam
316 Seamless Yeeb Nkab ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASME SA312 / ASTM A312 / ASTM A312 / ASTM A312 / ASME SA312) NPS 1/8 "mus rau 30"; SCH 5S to XXS
316 welded yeeb nkab ASTM A312 / A358 (EFW) Txheem NPS 1/2 "mus rau 60"; Loj Diameter Specialists
316 Kub Exchanger Tubes ASTM A213 / A269 / ASTM A213 / ASTM A213 / TS OD 6mm txog 114.3mm; U-Kov Muaj

 

316 stainless hlau kav tsim los ntawm GNEE muaj cov ntsiab lus molybdenum ntau dua lossis sib npaug li 2.0% thiab ua raws li cov cai ntawm NACE MR0175 / ISO 15156 tus qauv. Txhua qhov kev txiav txim yog nrog los ntawm EN 10204 3.1 Cov Khoom Siv Xeem Ntawv Pov Thawj (MTC).

EN 10204 3.1 Material Test Certificate


Peb muab cov kev pabcuam hauv qab no:
Precision Txiav thiab Beveling: Npaj rau tam sim vuam thaum unpacking.
Nto Polishing.
Tsis yog-Kev Ntsuas Kev Ua Phem (NDT): Peb muab 100% Kev Ntsuas Ultrasonic (UT), Eddy Current Testing (ET), thiab cov kev pabcuam kuaj dej.
GNEE muaj kev sib tw kawg CIF cov lus hais, uas suav nrog kev ntim khoom seaworthy (fumigated ntoo crates / VCI los tiv thaiv- xeb zaj duab xis) thiab cov ntaub ntawv raug cais cov khoom raws li HS Code 7304.41, kom ntseeg tau tias kev lis kev cai du rau koj cov khoom xa tuaj.