🧪 Chemical Composition

Element Kev sib xyaw (%)
Cov pa roj carbon (C) Tsawg dua los yog sib npaug li 0.08
Manganese (Mn) Tsawg dua lossis sib npaug li 2.00
Silicon (Si) Tsawg dua lossis sib npaug li 1.00
Phosphorus (P) Tsawg dua lossis sib npaug li 0.045
Sulfur (S) Tsawg dua lossis sib npaug li 0.030
Chromium (Cr) 22.0 - 24.0
Nickel (Ni) 12.0 - 15.0
Hlau (Fe) Tshuav
Nitrogen (N) Tsawg dua lossis sib npaug li 0.10

⚙️ Mechanical Properties

Khoom Tus nqi
Tensile Strength (Chav Kub) Ntau dua lossis sib npaug li 515 MPa
Yield zog (0.2% Offset) Ntau dua lossis sib npaug li 205 MPa
Elongation (50 hli ntsuas) Ntau dua lossis sib npaug li 40%
Kev txo qis ntawm cheeb tsam Ntau dua lossis sib npaug li 50%
Hardness (Brinell) Tsawg dua lossis sib npaug rau 217 HB
Hardness (Rockwell B) Tsawg dua lossis sib npaug li 95 HRB
Impact Zog (Charpy V-notch, 20 degree) Ntau dua lossis sib npaug li 120 J
Fatigue Limit (10^7 cycles) 240 MPa
Modulus ntawm Elasticity 200 GPa

🔬 Lub cev muaj zog

Khoom Tus nqi
Qhov ntom 7.98 g/m²
Melting Point 1400-1450 degree
Thermal conductivity (20 degree) 14.2 W/m·K
Thermal conductivity (100 degree) 16.8 W/m·K
Thermal Expansion (20-100 degree) 14.4×10-6/K
Thermal Expansion (20-300 degree) 15.9×10-6/K
Tshwj xeeb kub muaj peev xwm 500 J/kg · K
Hluav taws xob tiv thaiv (20 degree) 0.78 µΩ·m
Sib nqus Permeability 1.02 (Tsis yog-magnetic)
Curie Kub Tsis siv tau

📏 Product Specifications

Specification Muaj Kev Xaiv
Cov Khoom Muag Khoom Phaj, Sheets, Bars, Rods, Tubes, Pipes, Forgings, Coils
Phaj Thickness 6mm - 200 hli
Daim ntawv Thickness 0.5 hli - 6mm
Txoj kab uas hla 6mm - 300 hli
Tube sab nraud 6mm - 610 hli
Kev Ua Raws Cai ASTM A240, A479, A276, EN 10088-2, JIS G4305, GB / T 24511
Nto tiav 2B, BA, No.4, HL, Daim iav, Pickled, Annealed
Dimensional kam rau ua ± 0.1mm txog ± 0.5mm (nyob ntawm daim ntawv thiab loj)
Ntev Options Txheem ntev los yog txiav rau cov neeg siv khoom tshwj xeeb
Ntug tej yam kev mob Mill edge, Slit edge, Sheared edge, Nplaim txiav