Qib 410 (UNS S41000) hauv Suav teb

Apr 09, 2026

Tso lus

309S – Low-Carbon High-Cr-Ni Austenitic Steel: High-Temperature Oxidation Resistant AlloyUNS S34709 – High-Carbon Niobium-Stabilized Austenitic Steel For High-Temperature Pressure ServiceUNS S32100 – Titanium-Stabilized Austenitic Steel For High-Temperature Intergranular Corrosion ResistanceUNS S31008 – Low-Carbon Ultra-High Alloy Austenitic Steel For Extreme High-Temperature Service

Kev sib xyaw

Cov kev sib xyaw ua ke ntawm qib 410 stainless hlau tau pom hauv qab no.

Table 1- Kev sib xyaw ua ke ntawm qib 410 stainless hlau

Qib   C Mn Si P S Cr Ni
410 min.
max.
-
0.15
-
1
-
1
-
0.04
-
0.03
11.5
13.5
0.75

 

Mechanical Properties

Cov khoom siv kho tshuab raug ntawm qib 410 stainless hlau tau teev nyob rau hauv cov lus hauv qab no:

Rooj 2- Mechanical zog ntawm qib 410 stainless hlau

Tempering kub (degree) Tensile zog (MPa) Yield Strength 0.2% Pov thawj (MPa) Elongation (% hauv 50 mm) Hardness Brinell (HB) Impact Charpy V (J)
Annealed * 480 min 275 nqi 16 feeb - -
204 1475 1005 11 400 30
316 1470 961 18 400 36
427 1340 920 18.5 405 #
538 985 730 16 321 #
593 870 675 20 255 39
650 300 270 29.5 225 80

 

* Annealed khoom ntawm txias tiav bar, uas hais txog qhov mob A ntawm ASTM A276.
#Tempering ntawm qib 410 steels yuav tsum tau zam ntawm qhov kub thiab txias ntawm 425-600 degree, vim muaj kev cuam tshuam tsis zoo.

Lub cev muaj zog

Lub cev muaj zog ntawm qib 410 stainless hlau nyob rau hauv cov mob annealed yog tabulated hauv qab no:

Table 3- Lub cev muaj zog ntawm annealed qib 410 stainless hlau

Qib Qhov ceev (kg / m3) Elastic Modulus (GPa) Lub ntsiab lus Coefficient ntawm Thermal Expansion (μm / m / degree) Thermal conductivity (W / mK) Kev kub ceev 0-100℃(J / kg.K) Hluav taws xob tiv thaiv (nΩ)
0-100 degree 0-315 degree 0-538 ° C ntawm 100 degree ntawm 500 degree
410 7800 200 9.9 11 11.5 24.9 28.7 460 570

Xa kev nug