ASTM A358 qib 310 EFW kav
Txheej ntawm txoj taub: 1 \/ 8inch -24 nti
Hom: Welded Yeeb Nkab
Phab Ntsa Thickness: Sch10S ~ Sch160
Kev Xeem: Kev Ntsuas Hluav Taws Xob
Lub sij hawm xa tuaj: Tshuag 7 hnub
Pob Thauj: Ntim Hauv Bundles lossis Plywooden Kem
ASTM A358 Qib 310 EFW Kav Kev Taw Qhia
ASTM A 358 310 busion welded (hluav taws xob fusion welded) kav yog kub roj stainless hlau, kev kub siab thiab loj heev corrosive ib puag ncig. Lawv tau ua raws li ASME \/ ASTM cov qauv thoob ntiaj teb thiab tau xa hauv kev kho cua sov thiab pickled kom ntseeg tau qhov tseeb ntawm cov kav dej. Lawv muaj nyob rau hauv ntau qhov kev qhia tshwj xeeb, nrog sab nraud diameters nyob ntawm 57 hli rau 1626 hli thiab phab ntsa thicknesses xws li 2 hli rau 60 hli.
ASTM A {358 310 s stainless hlau welded kav dej muaj qhov kev ua haujlwm siab tshaj plaws ntawm 1200 degree thiab kev siv kub txuas ntxiv ntawm 1150 degree. Thaum muaj kub kub, 310s stainless hlau efw kav dej tseem tuaj yeem tswj lub zog siab thiab tawv thiab tsis muaj kev nkag mus thiab deformation.
ASTM A358 TPRED YEEB NKAB RAU DEJ KHO

Dab tsi yog qhov sib txawv ntawm 310 qib stainless hlau efw yeeb nkab thiab 310s?
Qeb 310 feem ntau yog hais txog 310s (tsis yog s31008), uas txo qhov kev pheej hmoo ntawm kev txo cov ntsiab lus carbon thiab yog tsim tshwj xeeb rau welded qauv.
{358 310 s stainless hlau welded yeeb nkab tsis tas yuav tsum tau kev kho mob ntxiv tom qab vuam kiv cua (xws li EFW kav). 310 Cov kav dej stainless hlau yog siv rau cov khoom tsis siv welded (xws li bolts-kub, casting), tab sis cov tshav kub tshav ntuj yuav tsum tau nruj me ntsis tswj tau thaum vuam.
TPP310S Stainless Hlau Efw Yeeb Nkab Nqe
Yog tias koj xav tau cov ncauj lus qhia ntxaws ntxaws, cov ntaub ntawv kub cov ntaub ntawv kub lossis cov ntawv thov kev lag luam, thov hu rau peb kom tau txais cov ntaub ntawv dawb thiab cov lus tshwj xeeb. Peb muab cov kev xaiv tag nrho los ntawm cov khoom xaiv, ua kom zoo rau kev sim thib peb-tog los pab cov phiaj xwm kub siab los pab kom siab kub ua av zoo!
ASTM A358 Stainless Hlau EFW Kav Kev Ua Haujlwm Tshwj Xeeb
ASTM A358 TPP310S Tshuaj Muaj Tshuaj Ntau
| Teem nqi | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 310S | min. | – | – | – | – | – | 24.0 | – | 19.0 | – |
| Max. | 0.08 | 2.00 | 1.50 | 0.045 | 0.030 | 26.0 | 22.0 | |||
ASTM A358 TP 310S EFW Kav Lub Cev Muaj Zog
| Teem nqi | Ntom ntom (kg \/ m3) | Elastic modulus (GPA) | Lub ntsiab lus coefficient ntawm thermal expansion (m \/ m \/ 0 c) | Thermal conductivity (w \/ mk) | Cov cua sov tshwj xeeb 0-1000 c (j \/ kg.K) | Hluav taws xob resistivity (NM) | |||
| 0-100 degree | 0-315 degree | 0-538 degree | ntawm 100 degree | ntawm 500 degree | |||||
| 310S | 7750 | 200 | 15.9 | 16.2 | 17.0 | 14.2 | 18.7 | 500 | 720 |
ASME ntawv pov thawj TPP30 YEEB NKAUJ

Cov qhua tuaj noj mov

ASTM A358 Stainless Hlau EFW Kav Pipes Kev Ntsuam Xyuas

Cim npe nrov: ASTM A358 Qeb 310 EFW Kav, Tuam Tshoj Astm A358 Qeb 310 EFW Kav Chaw Tsim Tshuaj, Chaw muag khoom, Hoobkas