ASTM A358 TPRESS STORL STENY HLAU WELDED YEEB NKAB

ASTM A358 TPRESS STORL STENY HLAU WELDED YEEB NKAB

Lub npe: ASTM A358 TPRESS STORL STESS STATION STEEL WELDED yeeb nkab
Sab Nrauv Inch: 1 / 8inch-24inch
Hom: Welded Yeeb Nkab
Phab Ntsa Thickness: Sch10S ~ Sch160
Kev Xeem: Kev Ntsuas Hluav Taws Xob
Lub sij hawm xa tuaj: Tshuag 7 hnub
Pob Thauj: Ntim Hauv Bundles lossis Plywooden Kem
Xa kev nug
Tsham tam sim no

ASTM A358 Qib 316L EFW Kav Kev Taw Qhia

 

ASTM A358 Tp358 LOJ FAIS FALION WELDED (EFW) Cov yeeb nkab stainless hlau yog haum rau siab piping cov tshuab siab thiab corrosive ib puag ncig. Txoj kab yeeb nkab uas hla los ntawm 1/8 nti mus rau 100 ntiv tes (3.175 hli rau 2540 mm).
Gnee's Astm A358 Tp3Tag Fusion Welded Yeeb Welded dej muaj ntau dua 50 xyoo, yog li txo cov pa yeeb thiab kev txij nkawm. Nws muaj qhov zoo weldability thiab ua kev ua tau thiab tuaj yeem txiav, khoov thiab tsim raws li xav tau.

 

ASME SA358 GR 316L Electric Fusion Welded Yeeb Nkab

ASME SA358 GR 316L Electric Fusion Welded Pipe

Daim Ntawv Thov ntawm Astm A358 Tp336L Stainless Hlau Yeeb Nkab

Tshuaj lom neeg thiab petrochemical: conveying corrosive media xws li sulfuric acid, hydrochloric acid, thiab alkaline daws.
Liquefied nkev (lng) cryogenic pipelines.
Khoom noj khoom haus thiab cov khoom noj: kev caij tsheb thauj tau huv (xav tau sab hauv phab ntsa polishing).
Siab nkoj: ASME tau lees paub Boilers, kev hloov pauv kub.

 

TPP316L Stainless Hlau EFW Yeeb Nqe

Yog tias koj xav tau cov ncauj lus qhia ntxaws ntxaws, cov ntaub ntawv kub thiab txias cov ntaub ntawv lossis kev lag luam ittm A36L EFW Yeeb, thov hu rau peb kom tau txais cov ntaub ntawv dawb thiab cov lus tshwj xeeb. Peb muab tag nrho - Cov kev xaiv cov txheej txheem los ntawm cov khoom xaiv, kev ua kom zoo rau kev sim siab kom pab tau siab rau cov haujlwm siab!

 

Hu rau tam sim no

ASTM A358 Stainless Hlau EFW Kav Kev Ua Haujlwm Tshwj Xeeb

Tshuaj lom neeg muaj pes tsawg leeg ntawm Astm A358 TP316L EFW YEEB

Lub ntsiab Cov ntsiab lus (Luj%)
Carbon (c) Tsawg dua los yog sib npaug rau 0.03%
Manganese (mn) Tsawg dua los yog sib npaug rau 2.00%
Silicon (si) Tsawg dua los yog sib npaug rau 1.00%
Phosphorus (p) Tsawg dua los yog sib npaug rau 0.045%
Sulphur (s) Tsawg dua los yog sib npaug rau 0.030%
Chromium (cr) 16.00–18.00%
Npib tsib caug (ni) 10.00–14.00%
Molybdenum (mo) 2.00–3.00%

Cov Khoom Siv Neeg Kho Tshuab Ntawm ASTM A358 TP316L Stainless Hlau Yeeb Nkab

Ntiag tug Tus nqi
Paib lub zog (rov qab) Ntau dua los yog sib npaug rau 170 MPa
Lub zog tensile (RM) 485-620 mpa
Elongation (a) Ntau dua los yog sib npaug rau 35%

Qhov loj me & specifications

Chaw ua uas tsis tau haus Qho deb
Txheej hauv lub taub 10.3 hli - 1219 hli
Phab Ntsa Thickness 1.24 hli - 59.54 hli
Qho ntev Txheem: 6 m (tsau ntev); Customizable thaum thov

ASME muaj ntawv pov thawj Tp36L Yeeb Nkab Khoom Siv

ASME Certified TP316L Pipe Supplier

Cov qhua tuaj noj mov

Customer Visit

ASTM A358 Stainless Hlau EFW Kav Pipes Kev Ntsuam Xyuas

ASTM A358 Stainless Steel EFW Pipes Testing