AISI 420B \/ C Stainless Hlau Seamless Yeeb Nkab
Khoom siv: Stainless hlau
Nto Kho: Polish, Sandblasting, Pickling
Puab: Round
Technicial: Cuav Rolling \/ Kos Duab
Sab nraud txoj kab uas hla: 3. 18-810 hli
Phab Ntsa Thickness: {0. {{{1} hm mm
Qhov loj me: 8 "{{-72"} "{2}} dn1800) \/219.1mm {6} mm
Txheem: ASTM A312, ASTM A213, ASTM A269, thiab lwm yam.
Pob Thauj: Nrog lub hau yas rau ob qho kawg, ntim rau hauv pob
Khoom Piav Qhia
AISI 420B thiab 420C stainless hlauyog cov qib siab carbon martensitic qib paub txog lawv cov hardness zoo heev, hnav tsis zoo, thiab mob corrosion tsis kam. Cov ntaub ntawv no zoo tagnrho rau kev tsim cov khoom siv dag ntxias tau siv hauv cov ntawv thov siab xws li cov khoom siv kho tshuab, cov cuab yeej kho tsheb, thiab cov cuab yeej kho kom haum.
420 Martensitic Stainless Hlau Yeeb Nkab

Cov Ntaw Ntaw Ntawm Aisi 420B \/ C Stainless Hlau Seamless Kav
Siab hardness thiab lub zog
AISI 420B \/ C Pipes Ua kom tiav siab dua tom qab kev kho cua sov (nce txog HRC 52-58), ua rau lawv ua kom tsis kam.
Zoo heev tasinability
Nyob rau hauv annealed mob, cov kav dej no muaj zoo machinability thiab qhov seem ruaj khov thaum lub sijhawm fabrication.
Moderate corrosion tsis kam
Nrog rau 12-14% chromium cov ntsiab lus, 420B \/ c stainless hlau muab tsim cov tshuaj lom neeg thiab cov me me los yog passivated.
Zoo saum npoo ua tiav
Seamless kav tuaj yeem muab rau hauv polished, pickled, lossis ci annealed cov xwm txheej kom tau raws li cov tsos mob thiab kev ua tau zoo.
Vim li cas thiaj xaiv GNEE
Cov khoom lag luam zoo: txhua pob ntawm cov kav dej yog nrog en 10204 3. 1 lub sij hawm ntsuas (1.5 lub sij hawm ua haujlwm siab rau 30 feeb
Kev xa tawm ceev ceev: 500 tons ntawm cov ntsiab lus tseem ceeb (xws li φ25.4 × 1. "yuav xa ncaj qha rau hauv 3-7 hnub tom qab tso ib qho kev txiav txim. Cov pob pob me me yog kev txhawb nqa (tsawg kawg nkaus xaj ntawm 100 meters).
AISI 420A Stainless Hlau Tube Specifications
Tshuaj Muaj Tshuaj
| Teem nqi | C (%) | CR (%) | MN (%) | SI (%) | P (%) | S (%) |
|---|---|---|---|---|---|---|
| 420B | 0.28–0.36 | 12.0–14.0 | Tsawg dua los yog sib npaug rau 1. 00 | Tsawg dua los yog sib npaug rau 1. 00 | Tsawg dua los yog sib npaug rau 0. 04 | Tsawg dua los yog sib npaug rau 0. 03 |
| 420C | 0.36–0.45 | 12.0–14.0 | Tsawg dua los yog sib npaug rau 1. 00 | Tsawg dua los yog sib npaug rau 1. 00 | Tsawg dua los yog sib npaug rau 0. 04 | Tsawg dua los yog sib npaug rau 0. 03 |
Cov ntsiab lus carbon ntau dua hauv 420C muab txawm ntau dua hardness thiab hnav tsis kam piv rau 420b.
Cov Khoom Siv Neeg Kho Tshuab (Cov cua sov kho mob)
| Ntiag tug | 420B | 420C |
|---|---|---|
| Lub zog tensile | 800-1000 MPa | 850-1100 MPA |
| Paib lub zog | Ntau dua los yog sib npaug rau 600 MPa | Ntau dua los yog sib npaug rau 650 MPa |
| Hardness (HRC) | 50–55 | 54–58 |
| Elongation (%) | Ntau dua los yog sib npaug rau 10 | Ntau dua los yog sib npaug rau 8 |
Qhov ntau thiab tsawg
| Sab nraud ntawm lub taub (od) | Phab Ntsa Thickness | Qho ntev |
|---|---|---|
| 6 hli - 120 hli | {{0 {}}. 5 hli - 10 hli | mus txog 6 meters |
1.4021 stainless hlau yeeb nkab tsum