ASTM A312 TP321H Stainless Polished Steel Yeeb Nkab
Khoom siv: Stainless hlau
Nto kho: polished
Ntu puab: Round
OD: 1/8 "-20"
Kev xa khoom: Tshuaj annealed thiab pickled
Pob Thauj: Sab Nraud Dub, ob sab nrog lub hau xaus
Cov Lus Qhia Tshwj Xeeb: 6mm-505mm
ASTM A312 Tp321h Stainless Polished Steel Yeeb Nkab Taw
ASTM A312H TP321H Polished Stainless Hlau Yeeb yog ib qho titanium stabilized ectrolytically polished rau saum npoo tsawg dua los yog sib npaug rau 0.4μm. Nws tau muaj qhov siab huv thiab corrosion tsis kam thiab yog siv dav hauv cov zaub mov, tshuaj, semiconductor thiab kub kev lag luam.
ASTM A312 Tp321h stainless hlau electropolished yeeb nkab

Qhov Zoo ntawm STM A312 Tp321h huv cov qhob
ASTM A312 TP32H titanium stabilized kub stabilized kub stort steel yeeb (UN tsis muaj pa roj carbon) yog cov pa roj carbon monuple of 18cr-8Ni Austenitic steel. Titanium lub caij nyoog inhibits cov nag lossis daus, txhim kho cov kev tiv thaiv kev cuam tshuam nrog kev ua kom haum thiab qhov kub thiab txias nce mus txog 870 degree).
ASTM A312 TP32H Stainless Hlau Polished Steel Yeeb muaj lub zog siab thiab tuaj yeem tiv taus ntau dua thiab muaj zog. Nyob rau tib lub sijhawm, nws yog ib qho yooj yim rau cov txheej txheem, txiav, weld thiab khoov, thiab tuaj yeem ua rau kav dej thiab ntau thiab rau ntau qhov kev thov sib tw.
Vim li cas thiaj xaiv GNEE
Gnee tshwj xeeb hauv kev tsim khoom ntawm seamless / Welded (EFW / EFW) CART kev cai lij choj xws li hluav taws xob kev kos duab kom ntseeg tau qhov tseeb thiab ua kom muaj zog. Raws li DIN 1.4878 tus neeg xa khoom, cov khoom ua haujlwm nrog ASMVC cov qauv, muab cov kev txhawb nqa customized thiab kev txhawb nqa thoob ntiaj teb.
ASTM A312 TP 321 ultra- Cov Khoom Siv Tshiab Tshiab
| Lub hom phiaj | ASTM A312 / ASME SA312 (Seamless), Astm A358 (Welded) |
| Teem nqi | Tp321h (uns uns s32109) |
| Tshuaj Muaj Tshuaj | {{0- C: 0.04-0.10%, Ti: 9-12%, thiab ntau dua lossis sib npaug lossis sib npaug ntawm 1.0% |
| Cov Khoom Siv Neeg Kho Tshuab | {{0 {{}} tawm lub zog: ntau dua los yog sib npaug rau 205 MPa (hauv chav temp) |
| {{0- tensile lub zog: ntau dua los yog sib npaug rau 515 MPa | |
| {{0 {}} elongation: ntau dua los yog sib npaug rau 30% | |
| Qho loj | {{0- od: 6.03 hli rau 610 hli (0.237 "rau 24") |
| {{0-} Ntsa Thickness: 0.5 hli rau 25 hli (Teem Sij Hawm Rau XXH) | |
| Nto tas | {{0-} polished: ra tsawg dua lossis sib npaug rau 0.4μm (mechanical polishing) |
| Puab | Puag ncig, square, duab plaub, hydraulic |
| Kawg ua tiav | Tiaj kawg, beveled kawg, threaded |
| Kev Kho Cua Sov | Siv Annealed (1010-1120 Qib) + sai sai txias |
| Ntawv muaj | ASME BPVC, ISO 9001, FDA, 3A, en 10204 3.1 / 3.2 |
UNR UNS UNRNEAMLESS YEES

Cov qhua tuaj noj mov

Ntim ntawmASTM A312 Tp322h annealed raj

Cim npe nrov: ASTM A312 TP32H Stainless Polished Steel Yeeb Nkab, Tuam Tshoj ASTM A312H Stainless Polished Steel Yeeb Nkab Cov Chaw Tsim Tshuaj, Chaw muag khoom, Hoobkas