Dab tsi yog qhov sib txawv ntawm 1.4301 thiab 1.4303?
Aug 20, 2025
Tso lus
Dab tsi yog 1.4301 stainless hlau?
1.4301 (X5Cni18-10): Qhov no yog tus qauv Austenitic stainless hlau feem ntau yog hu ua nws zoo corrosion tsis kam, weldability, thiab muaj peev xwm.
Dab tsi yog 1.4303 ss?
1.4303 (x4crni18 {{4 4}} 12): Cov qib qib no tseem yog cov leeg tsis muaj pa me me, tab sis nws muaj cov ntsiab lus tsib xee ntau dua li 1.4301. Qhov no nce tsib xee cov ntsiab lus txhim kho nws txoj kev tiv thaiv kom corrosion, tshwj xeeb hauv chloride muaj ib puag ncig. Nws kuj tseem txhim kho nws cov kev haum rau cov txheej txheem txias.
Dab tsi yog qhov sib txawv tseem ceeb ntawm 1.4301 thiab 1.4303 stainless hlau?
Lub Koom Haum Me Nyuam Yaus yog cov ntsiab lus carbon: 1.4301 (304 tus hlau Stainless) muaj txog 0.08% Carbon, Thaum 1.4303 (303% carbon. Qhov no txo cov ntsiab lus ntawm cov roj carbon hauv 304L txhim kho nws cov weldability thiab ua rau nws haum rau kev siv cov ntaub ntawv siv tshuaj pleev qhov chaw uas carbide cov teeb meem.
Kev siv tshuaj lom neeg sib xyaw ntawm 1.4301 vs . 1.4303
Qhov tseem ceeb tshaj plaws yog cov ntsiab lus carbon comp . 1.4301 muaj ntau dua cov ntsiab lus carbon (txog li 0.08% muaj cov ntsiab lus roj carbon ntau dua (nce mus txog 0.03%).
| Lub ntsiab | 1.4301 (304 stainless hlau) | 1.4303 (304l stainless hlau) |
|---|---|---|
| Chromium (cr) | 18.00% - 20.00% | 18.00% - 20.00% |
| Npib tsib caug (ni) | 8.00% - 10.50% | 8.00% - 10.50% |
| Manganese (mn) | 2.000% Max | 2.000% Max |
| Carbon (c) | 0.08% Max | 0.03% max |
| Silicon (si) | 1.00% max | 1.00% max |
| Phosphorus (p) | 0.045% Max | 0.045% Max |
| Sulphur (s) | 0.030% max | 0.030% max |
| Hlau (FE) | Seem | Seem |
Cov khoom siv neeg kho tshuab ntawm 1.4301 vs . 1.4303
| Ntiag tug | 1.4301 (304 stainless hlau) | 1.4303 (304l stainless hlau) |
|---|---|---|
| Lub zog tensile | 520 MPa (yam tsawg kawg nkaus) | 510 MPa (yam tsawg kawg nkaus) |
| Paib lub zog | 210 MPa (yam tsawg kawg nkaus) | 190 MPa (yam tsawg kawg nkaus) |
| Elongation | Ntau dua los yog sib npaug rau 40% (hauv 50 mm koob gauge ntev) | Ntau dua los yog sib npaug rau 40% (hauv 50 mm koob gauge ntev) |
| Kev nyuaj | 92 HRB (siab tshaj) | 92 HRB (siab tshaj) |
| Cuam Tshuam Lub Zog | 200 j at -20℃(tsawg kawg nkaus) | 200 j at -20℃(tsawg kawg nkaus) |
Yog 1.4303 ntau resistant rau corrosion tshaj li 1.4301?
Ob phau 1.4301 thiab 1.4303 muaj cov ntsiab lus corrosion zoo vim lawv cov ntsiab lus chromium thiab npib tsib xee. Txawm li cas los xij, 1.4303 (304L) feem ntau nyiam rau welded daim ntawv thov vim tias nws cov kev siv cov pa roj carbon heel
Qhov twg yog qhov zoo dua rau vuam: 1.4301 lossis 1.4303?
1.4303 (304L stainless hlau) feem ntau zoo dua rau vuam vim nws cov ntsiab lus roj carbon. Qhov txo cov pa roj carbon cov ntsiab lus tiv thaiv nag lossis nag lossis nag lossis nag lossis daus)
Yuav 1.4301 thiab 1.4303 tau siv sib hloov pauv?
Thaum 1.4301 (304) thiab 1.4303 (304L) yog qhov sib cuam tshuam zoo heev thiab tawv ncauj ua kom zoo dua li cov ntawv thov kev siv. Ntawm qhov tod tes, 1.4303 yog qhov xav tau nyob rau hauv cov xwm txheej qhov twg weldability thiab tsawg cov ntsiab lus carbon thiab tsawg li hauv welded tso tsheb hlau luam thiab khoom siv tshuaj lom neeg.