1.4310 vs . 1.4305}} stainless hlau

Aug 20, 2025

Tso lus

Cov khoom siv yog li cas 1.4310 sib npaug rau?
Cov khoom siv AISI 302 yog cov hlau tsis muaj txiaj ntsig 302 yog cov hlau tsis muaj txiaj ntsig, tseem paub nyob rau hauv cov kev tsim qauv 1.4310, BS 3011 thiab X10CRNi11 thiab X10CRNi11 thiab X10CRNi11 Tus kav hlau ua kom muaj stainless hlau|302 belongs rau Pawg V2a Steels thiab tseem hu ua cov hlau caij nplooj ntoos hlav, raws li nws tau siv rau kev tsim cov txuj ci ci.

 

Dab tsi yog 1.4305 stainless hlau?
Stainless hlau hom 1.4305 yog nrov npe hu ua Qib 303 stainless hlau. Qeb 303 yog cov tshaj tawm tau yooj yim tshaj plaws ntawm txhua qib Austenitic cov qib ntawm cov hlau stainless. Lub tshuab ua haujlwm ntawm qib 303 yog vim muaj cov leej faj hauv cov hlau muaj pes tsawg leeg.

 

Tshuaj Muaj Tshuaj

Ntiag tug 1.4310 (AISI 301) 1.4305 (AISI 303)
Tshuaj Muaj Tshuaj    
Chromium (cr) 16.0 - 18.0% 17.0 - 19.0%
Npib tsib caug (ni) 6.0 - 8.0% 8.0 - 10.0%
Manganese (mn) 2.0 - 3.0% 1.75 - 2.5%
Carbon (c) 0.12 - 0.15% 0.15%
Silicon (si) 1.0% max 1.0% max
Phosphorus (p) 0.045% Max 0.2% max
Sulphur (s) 0.03% max 0.15% Max
Hlau (FE) Seem Seem

 

Cov Khoom Siv Neeg Kho Tshuab

Cov Khoom Siv Neeg Kho Tshuab 1.4310 (AISI 301) 1.4305 (AISI 303)
Tensile lub zog (mpa) 650 - 850 mpa 500 - 700 mpa
Yield zog (mpa) 275 - 500 mpa 205 - 275 mpa
Elongation 40 - 60% (hauv 50 hli) 35 - 50% (hauv 50 hli)
Kev nyuaj 92 HRB (siab tshaj) 95 hrb (siab tshaj)
Modulus ntawm elasticity (GPA) Tom ntej no 200 GPA Tom ntej no 200 GPA
Kev Cuam Tshuam Nruab nrab (qis tawv dua li 304) Nruab nrab (qis tawv dua li 304)

 

Dab tsi yog qhov sib txawv ntawm 1.4310 thiab 1.4305 stainless hlau?
Lub ntsiab lus tseem ceeb ntawm 1.4310 thiab 1.4305 stainless hlau nyob hauv lawv lub tshuab luam ntawv, tseem muaj kev ua haujlwm me me, ua rau nws haum rau kev siv xws li Springs.

 

Dab tsi yog qhov sib txawv ntawm 1.4310and 1.4307 stainless hlau?
1.4310 thiab 1.4307 yog ob qho tib si stainless hlau, tab sis 1.4310 feem ntau yog paub txog nws cov txiaj ntsig ntau dua weldability thiab corrosion tsis kam, tshwj xeeb tshaj yog nyob rau hauv cov qauv welded.


Dab tsi yog qhov sib txawv ntawm 1.4310 thiab 1.4404?
Rau 1.4310 (x10crni18 - 8) thiab en 1.440 (x2404 muaj ob qho tib si zoo tshaj plaws vim nws molybdenum cov ntsiab lus. Thaum 1.4310 yog paub rau nws lub zog siab tensile thaum txias-dov, 1.440 nce ntau dua npib tsib thiab molybdenum cov ntsiab lus ua rau nws tiv taus corrosion, tshwj xeeb tshaj yog nyob hauv chloride ib puag ncig.

 

301 1.4310 stainless steel bar

Leej twg xaiv peb?

 

Yog tias koj muaj ib qhov project xav tau rau 301 1.4310}} stainless hlau bar, peb zoo siab txais tos koj daim ntawv xaj. Gnee muaj cov khoom lag luam loj ntawm cov khoom nrov rau koj xaiv los ntawm. Peb ua cov kab ntawv no rau hauv ntau cov qauv khoom siv, suav nrog cov ntawv, xaim, bar, thiab xaim. Txhawm rau kom ntxaws tshuaj muaj pes tsawg leeg tshuaj thiab kuaj dawb, thov hu rau peb lub Hoobkas niaj hnub no. Peb muab nqi sib tw thiab kev pabcuam zoo tshaj.Uamail:sales@gneestainless.com