Dab tsi yog 249 TPp3?

Aug 29, 2025

Tso lus

Dab tsi yog sa 249 cov khoom siv?

ASTM A249 / A249MDuav Nominal -} phab ntsa {} Thicker} Tickness welded steels ua los ntawm cov kev siv welded, supertheater, super hloov tub, lossis condenser tub.

 

Dab tsi yogSA 249 TP 316L Stainless Hlau Welded Yeeb Nkab?
ASME SUAB 249 TP 319 TP 316L Stainless Hlau Welded Yeeb yog ib hom stainless hlau yeeb nkab tsim los asme sa 249 specifications thiab txuas nrog vuam. Cov yeeb nkab no yog qhov qis-} pabbon version ntawm 316 stainless hlau version ntawm 316 stainless hlau alloy thiab muaj kev tiv thaiv zoo, tshwj xeeb tshaj yog nyob rau hauv cov chaw hnyav. Nws yog feem ntau siv nyob rau hauv high - qhov kev siv hluav taws xob, cov ntaub ntawv cua sov, thiab cov ntawv thov nrog cov dej qab zib.

SA 249 TP 316L Stainless Steel Welded Pipe

 

ASME SA 249 TPRESS HLAU HLAU STEELLE HLAV RAJ SPECICTIONS

Lub hom phiaj ASME SA249
Hom raj raj Welded Tube
Teem nqi TP 316L
Tag Annealing pickling
Ci Plig Annealing
Polished
Sab nraud ntawm lub taub 6 txog 219.1 hli
Qhov tuab 0.5 txog 8 hli

SA 249 316 l swj raj tshuaj muaj pes tsawg leeg

Sa 249 C Mn P S Si Ni Cr Mo N
316L 0.035 2.00 0.045 0.030 1.0 10-14 16-18 2-3  
1.4404 0.03 2.00 0.040 0.015 1.0 10-13 16.5-18.5 2-2.5 0.11

ASME SA 249 TP 316L Tub Lub Cev Cov Khoom Siv Neeg Kho Tshuab

 
Tensile kev ntxhov siab (MPA)
Yield kev ntxhov siab (MPA) Elongation (%) Elongation (%)
Sa 249 316 l 485 170 35 25
1.4404 490-690 190 40 30

 

 

Daim ntawv thov

Asme Sa 249 Takeless cov raj tau thov siv rau hauv cov condenser, TUBS tuaj yeem ua haujlwm nyob rau hauv ib puag ncig cua sov thiab lwm yam kev xaiv kub, thiab nws yog ruaj thiab tus nqi -} Ua tau zoo.

 

ASME sa249 Qib 316L Welded Yeeb Nkab yog tsim los ntawm cov phaj dov los yog sawb thiab mam li welded siv cov khoom siv khw vuam. Cov kav dej no yuav tsum tau sim ua ntej siv high- siab nruab. ASME SA249 GR 316L ERW WELDED PIPES yog tsim nrog kev ntev ntev, uas muaj hluav taws xob hluav taws xob dhau los ntawm cov hlau txheej rau weld lawv nyob rau hauv qhov chaw. Cov kav dej no tuaj yeem welded nyob rau hauv qhov chaw tsis muaj cov chaw muab tub lim. Yog koj muaj lus nug txog peb cov khoom lag luam lossis xav tau nqe lus, thov hu rau peb hnub no! Email:sales@gneestainless.com

 

Asme Sa 249 Tp3Echl Stainless Hlau Tube Hauv Tswj Zoo

ASME SA 249 TP316L Stainless Steel Tube In Quality Control

Ntim thiab Cim Cim
Ntim rau hauv cov pob lossis cov ntoo ntoo ntoo qhwv hauv yas, thiab tsim nyog tiv thaiv rau hiav txwv - tsim nyog.

ASTM A249 TP316L Stainless Steel Tubes PE Fabric Bundles
ASTM A249 TPRESS KHWIC HLAU STEEL STUMPES PE Npuag Bundles
ASTM A249 TP316L wooden case packages
ATM A249 TP316L Cov Pob Rooj Ntoo Cov Khoom Ntoo

Xa kev nug