Dab tsi yog qhov txawv ntawm ASTM A312 TP304 thiab TP316?
Jun 03, 2026
Tso lus

Dab tsi yogASTM A312 TP304 stainless hlau round yeeb nkab?
ASTM A312 TP304 stainless hlau round yeeb nkab yog qhov feem ntau siv dav dav specifications, tshwj xeeb tshaj yog tsim los ntawm seamless, welded, thiab hnyav hnyav- ua hauj lwm austenitic stainless hlau piping npaj rau siv nyob rau hauv siab - kub thiab dav corrosive kev pab cuam ib puag ncig. Cov khoom siv kav dej no yog tsim los ntawm TP304 alloy (UNS S30400)- tus qauv "18/8" stainless hlau (muaj 18% chromium thiab 8% npib tsib xee)- thiab nta zoo heev formability, weldability, thiab zoo tiv thaiv oxidation thiab me ntsis corrosion.
Dab tsi yogASTM A312 TP316 Stainless hlau yeeb nkab?
ASTM A312 TP316 yog tus qauv kev qhia tshwj xeeb rau seamless, welded, thiab txias hnyav - ua haujlwm austenitic stainless hlau kav npaj rau siab - kub thiab kev pabcuam corrosive.
Nws yog tsim los ntawm TP316 alloy (UNS S31600), feem ntau hu ua "marine qib" stainless hlau. Nws lub ntsiab lus txhais yog qhov sib ntxiv ntawm 2.0-3.0% Molybdenum, uas muab kev tiv thaiv zoo tshaj rau pitting thiab crevice corrosion nyob rau hauv chloride ib puag ncig (xws li, seawater, ntug hiav txwv huab cua, tshuaj ua) piv rau TP304.

Dab tsi yog qhov txawv ntawm ASTM A312 TP304 thiab TP316?
ASTM A312 TP304 thiab TP316 ob leeg txhais cov seamless lossis welded austenitic stainless hlau kav, tab sis lawv txawv nyob rau hauv lawv cov tshuaj muaj pes tsawg leeg. TP316 muaj molybdenum (2-3%), uas ua rau nws zoo dua corrosion thiab pitting tsis kam tiv thaiv chlorides thiab marine ib puag ncig piv rau TP304.
UNS / EN / JIS / GB sib npaug:
TP304 ≈ UNS S30400; EN 1.4301 (AISI 304); JIS SUS304; GB 06Cr19Ni10.
TP316 ≈ UNS S31600; EN 1.4401/1.4404 (AISI 316/316L); JIS SUS316; GB
ASTM A312 TP304 vs TP316: Tshuaj muaj pes tsawg leeg
| Qib | C (max) | Mn (max) | P (max) | S (max) | Si (max) | Cr | Ni | Mo |
| TIAB SA 304 | 0.08% | 2.00% | 0.045% | 0.030% | 1.00% | 18.0–20.0% | 8.0–11.0% | - |
| TIAB SA 316 | 0.08% | 2.00% | 0.045% | 0.030% | 1.00% | 16.0–18.0% | 11.0–14.0% | 2.0–3.0% |
ASTM A312 TP304 vs TP316: Mechanical Properties
| Qib | Tensile zog, min | Yield zog, min | Elongation hauv 2 nti. (50mm), min |
| TIAB SA 304 | 75 ksi (515 MPa) | 30 ksi (205 MPa) | 35% |
| TIAB SA 316 | 75 ksi (515 MPa) | 30 ksi (205 MPa) | 35% |
Nominal phab ntsa thickness rau ASTM A312 (Seamless thiab ncaj seame welded steel kav)
| NPS | ASTM A312 WT kam rau ua,% | |
|---|---|---|
| + | – | |
| 1/8-2 1 /2 | 20.0 | 12.5 |
| 3 ~ 18, t / D Tsawg dua lossis sib npaug li 5% | 22.5 | 12.5 |
| 3~18, t/D> 5% | 15.0 | 12.5 |
| Ntau tshaj los yog sib npaug rau 20, welded | 17.5 | 12.5 |
| Ntau dua lossis sib npaug rau 20, seamless, t / D Tsawg dua lossis sib npaug li 5% | 22.5 | 12.5 |
| ≥ 20, seamless, t/D> 5% | 15.0 | 12.5 |
ASTM A312 Stainless hlau kav OD kam rau ua
| NPS | ASTM A312 OD kam rau ua | |||
|---|---|---|---|---|
| + | – | |||
| nti | mm | nti | mm | |
| 1/8~1 1 /2 > 1 1 /2~4 > 4~8 > 8~18 > 18~26 > 26~34 > 34~48 |
1/64(0.015) 1/32(0.031) 1/16(0.062) 3/32(0.093) 1/8(0.125) 5/32(0.156) 3/16(0.187) |
0.4 0.8 1.6 2.4 3.2 4.0 4.8 |
1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) 1/32(0.031) |
0.8 0.8 0.8 0.8 0.8 0.8 0.8 |
ASTM A312 TP304 vs TP316: Corrosion Resistance
Nyob rau hauv cov nqe lus ntawm corrosion kuj, TP316 ho outperforms TP304, tshwj xeeb tshaj yog nyob rau hauv ib puag ncig uas muaj chlorides thiab acidic media. TP304 muaj kev cuam tshuam ntau dua rau pitting corrosion thiab crevice corrosion, whereas TP316 muaj 2-3% molybdenum (Mo), uas pab tsim cov yeeb yaj kiab ruaj khov dua rau ntawm cov hlau tsis huv, yog li txhawb nws txoj kev tiv thaiv rau ob qho tib si pitting thiab crevice corrosion. Tus Pitting Resistance Equivalent Number (PREN) feem ntau yog siv los ntsuas cov hlau tsis muaj steel tsis kam rau pitting corrosion, nrog cov nqi siab dua qhov qhia tau zoo dua corrosion. TP304 feem ntau muaj tus nqi PREN ntawm kwv yees li 18-20, thaum TP316 feem ntau ua tiav PREN tus nqi ntawm 23-28, sawv cev rau kev txhim kho pitting corrosion kuj ntawm li 20% -40%.

Vim li cas TP316 kim dua TP304?
Tus nqi ntawm 316 stainless hlau feem ntau yog 10% mus rau 30% siab dua li ntawm 304 stainless hlau. TP316 kim dua vim tias nws muaj molybdenum thiab yuav tsum muaj cov ntsiab lus nickel ntau dua li 304. Raws li cov nqi ntawm cov khoom siv raw, 304 stainless hlau feem ntau yog li ntawm $ 3.50 txog $ 5.00 ib kilogram, thaum tus nqi ntau rau 316 stainless hlau yog $ 4.50 txog $ 6.50 ib kilogram.
Nyem kom tau txais tus nqi tshiab
TP304 vs. TP316: Qhov Zoo Tshaj Plaws rau Kev Kub Siab -?
Raws li qhov kev pabcuam cuam tshuam tsis sib xws, ob qib tuaj yeem siv rau hauv ib puag ncig qhov kub thiab txias txog li 870℃(1600℃F). Txawm li cas los xij, yog tias daim ntawv thov cuam tshuam nrog kev ua haujlwm tas mus li hauv 425–860 degree, nws raug nquahu kom ua qhov tseem ceeb ntawm qib "L" series (xws li TP304L lossis TP316L) txhawm rau tiv thaiv carbide nag lossis daus, los yog xaiv "H" qib qib kom ua tiav qib siab dua - qhov kub thiab txias.

ASTM A312 TP304 vs TP316: Daim ntawv thov
TP304: Cov kav dej, cov khoom siv ua zaub mov, cov dab dej, cov khoom vaj tsev zoo nkauj.
TP316: Kev ua tshuaj lom neeg, kev tsim kho dej hiav txwv, cov kav dej tshuaj, cov qauv hauv ntug hiav txwv.
Yog tias koj qhov project cuam tshuam nrog kev siv tshuaj lom neeg thiab koj tsis paub meej tias yuav xaiv 304 lossis 316L stainless hlau kav, thov xa mus rau cov ntaub ntawv tshawb fawb hauv qab no.
Case Study: Piping Material Upgrade Project nyob rau hauv Chlor-Alkali Chemical Plant
Hauv thaj chaw tshuaj tiv thaiv ntawm cov nroj tsuag tshuaj, lub tshuab ua dej txias uas muaj cov tshuaj chloride ions thiab cov organic acids yog thawj zaug siv. Cov kav dej qub yog tsim los ntawm TP304 stainless hlau; Txawm li cas los xij, tus nqi ntawm cov yeeb nkab phab ntsa thinning ntau tshaj qhov kev cia siab, thiab nquag xau tshwm sim ntawm qhov vuam seams. Yog li ntawd, cov kab ntau lawm raug yuam kom raug kaw tsis tu ncua los pab txhim kho vuam lossis hloov cov yeeb nkab seem.
GNEE Stainless Steel Lub Tsev Haujlwm Saib Xyuas Kev Ua Haujlwm tau ua qhov kev tshuaj xyuas metallographic ntawm cov kav dej ua tsis tiav, xaus lus tias chloride-induced localized corrosion yog thawj qhov ua rau tsis ua haujlwm. Thaum lub sij hawm hloov kho loj tom ntej, cov cheeb tsam loj tshaj plaws corroded - muaj kwv yees li 1.5 mais ntawm cov kav dej - tau hloov tag nrho nrog TP316L stainless hlau. TP316L muaj 2% mus rau 3% molybdenum (Mo), ib qho tseem ceeb uas ua rau cov hlau tsis muaj zog tiv thaiv chloride-induced pitting corrosion.

304 VS . 316L stainless hlau yeeb nkab: nqi
| Metric | Thaum lub sij hawm TP304 Service | Thaum lub sij hawm TP316L Service | Kev txhim kho |
|---|---|---|---|
| Lub Sijhawm Nruab Nrab Nruab Nrab (MTBF) | 8 muaj | 12 hli | +50% |
| Kev Tiv Thaiv Txhua Xyoo & Kho Kev Kho Kom Zoo Tshaj | 10 zaug / xyoo | 7 zaug / xyoo | -30% |
| Tus nqi kho kav txhua xyoo (Cov Khoom Siv + Kev Ua Haujlwm) | $120,000 | $84,000 | -30% |
ASTM A312 TP304 / TP316 Stainless Hlau Yeeb Nkab Chaw tsim khoom
Peb tuav cov khoom npaj txhij ntawm cov qauv tshwj xeeb (SCH 10S, SCH 40S) hauv qib TP304 thiab TP316, ua kom cov khoom xa tuaj sai li sai tau hauv 7 mus rau 15 hnub.
Kev Ua Haujlwm Kev Cai: Peb muab ntau yam ntawm tus nqi- ntxiv cov kev pabcuam, suav nrog kev txiav kom raug, yeeb nkab dabtsi yog khoov, beveling, drilling, thiab kev ua tiav nto (daim iav / txhuam).
| Yam khoom | Qib | Sab nraud Diameter (OD) | Phab ntsa Thickness (WT) | Ntev | Xaus Xaus |
| Seamless Yeeb Nkab | TP304/304L, TP316/316L | 1/8 "mus rau 30" (DN{3}} DN750) | SCH 5S, 10S, 40S, 80S, 160S, XXS | 5.8m, 6m, 11.8m, 12m lossis Custom | Plain, Beveled, Threaded |
| Welded yeeb nkab | TP304/304L, TP316/316L | 1/2 "mus rau 80" (DN{3}} DN2000) | SCH 5S, 10S, 40S, 80S | Ib leeg / Ob chav Random, lossis Kho | Plain, Beveled |
| Nto tiav | TP304/TP316 |
Pickled, Annealed, 2B, BA, No.4, 400/600/800 Daim iav Polish |



Peb muab Cov Ntawv Pov Thawj Xeem Khoom (MTC) raws li EN 10204 3.1 tus qauv. Peb ua cov kev sim hydrostatic, eddy tam sim no kuaj, kuaj ultrasonic, thiab PMI (Positive Material Identification) kom ntseeg tau tias cov tshuaj muaj pes tsawg leeg (Ni, Cr, Mo) ua raws li ASTM A312 tus qauv.


Ntim: Peb siv tus qauv- raws li kev xa tawm ntim khoom tsim nyog rau kev thauj khoom hauv hiav txwv (ntoo crates, reinforced steel thav duab crates, los yog tiv thaiv lub kaus mom kawg).