SUS 303 vs SUS 304: Qhov txawv yog dab tsi?

May 27, 2026

Tso lus

SUS303 stainless hlau yog dab tsi?

SUS303 (tseem hu ua AISI 303 lossis UNS S30300) yog ib qho dawb -machining austenitic stainless hlau. Muab los ntawm cov qib SUS304 siv dav, cov hlau no ua tiav kev ua haujlwm zoo dua los ntawm kev sib ntxiv ntawm cov leej faj, txawm hais tias nws cov kev tiv thaiv corrosion thiab toughness yog me ntsis txo, ua rau nws corrosion kuj qis dua li ntawm SUS304. Nyob rau hauv lub annealed mob, cov khoom yog kiag li tsis yog -magnetic; Txawm li cas los xij, tom qab ua haujlwm txias, nws tuaj yeem pom me ntsis hlau nplaum. Feem ntau hu ua "automatic tshuab dhos qib stainless hlau," nws yog tsim rau ceev, bolts, thiab screws; shafts thiab gears; bushings thiab fittings; thiab hluav taws xob switchgear Cheebtsam.

 

Dab tsi yog SUS304 stainless hlau?

SUS304 yog qhov siv ntau tshaj plaws austenitic stainless hlau thoob ntiaj teb. Feem ntau hu ua "18/8" stainless hlau, nws yog kiag li sib npaug rau AISI 304 lossis SS304 (tus qauv qib hauv Tebchaws Meskas). Tus cwj pwm los ntawm cov ntsiab lus npib tsib xee siab, nws nthuav tawm ib qho -theem austenitic microstructure ntawm chav tsev kub, muaj cov corrosion kuj zoo heev, thiab muaj zog tiv taus xeb. Hauv nws lub xeev annealed, nws tuav cov qauv austenitic thiab feem ntau tsis yog-sib nqus; tsuas yog tom qab ua haujlwm txias tuaj yeem txhim kho me ntsis hlau nplaum. Nws tuaj yeem tsim rau hauv ntau hom khoom siv, nrog rau cov ntawv, coils, raj, tuav, xov hlau, thiab lwm yam.

 

Dab tsi yog qhov txawv ntawm SUS303 thiab SUS304?

Qhov sib txawv tseem ceeb nyob hauv lawv cov ntsiab lus sulfur. SUS303 muaj cov qib sulfur siab dua (Ntau dua lossis sib npaug li 0.15%) thiab hu ua "dawb-machining stainless hlau." SUS304 muaj cov ntsiab lus tsis tshua muaj leej faj (tsawg dua lossis sib npaug li 0.030%) thiab ua haujlwm raws li tus qauv, dav dav - lub hom phiaj stainless hlau.

 SUS303 And SUS304

 

Dab tsi yog cov khoom sib npaug rau SUS 303 stainless hlau?

JIS (Nyiv) AISI/ASTM (USA) UNS (Global) EN / DIN (Tebchaws Europe / Lub Tebchaws Yelemees) EN Lub Npe (Chemical) GB (Tuam Tshoj) ISO (International) BS (UK)
TIAB SA 303 303 S30300 1.4305 X8CrNiS18-9 06Cr18Ni9 (Y1Cr18Ni9) 303-00-I 303S31
TIAB SA 304 304 S30400 1.4301 X5CrNi18-10 06Cr19Ni10 (0Cr18Ni9) 304-00-I 304S31

 

SUS 303 vs SUS 304: Chemical Composition (wt%)

Element SUS 303 (Dawb-Machining) SUS 304 (Standard)
Cov pa roj carbon (C) Tsawg dua lossis sib npaug li 0.15 Tsawg dua lossis sib npaug li 0.08
Manganese (Mn) Tsawg dua lossis sib npaug li 2.00 Tsawg dua lossis sib npaug li 2.00
Phosphorus (P) Tsawg dua los yog sib npaug li 0.20 Tsawg dua lossis sib npaug li 0.045
Sulfur (S) Ntau dua lossis sib npaug li 0.15 Tsawg dua lossis sib npaug li 0.030
Silicon (Si) Tsawg dua lossis sib npaug li 1.00 Tsawg dua lossis sib npaug li 1.00
Chromium (Cr) 17.0 – 19.0 18.0 – 20.0
Nickel (Ni) 8.0 – 10.0 8.0 – 10.5
Molybdenum (hli) (Yeem) Tsawg dua lossis sib npaug rau 0.60 Tsis Qhia

 

SUS 303 vs SUS 304: Mechanical Properties (Annealed Condition)

Khoom TIAB SA 303 TIAB SA 304
Tensile zog (min) 520 MPa rau 520 MPa rau
Yield zog (0.2% Offset) Ntau dua lossis sib npaug li 205 MPa Ntau dua lossis sib npaug li 205 MPa
Elongation (hauv 50mm, min) Ntau dua lossis sib npaug li 40% Ntau dua lossis sib npaug li 40%
Hardness (Brinell - HB) Tsawg dua lossis sib npaug li 187 Tsawg dua lossis sib npaug li 187
Machinability Rating 75 - 80% (Zoo heev) 45% (Fair)

 

SUS 303 vs SUS 304: Machinability

Vim tias qhov sib ntxiv ntawm cov sulfur (feem ntau tsis tsawg dua 0.15%), SUS303 muaj qhov ua tau zoo dua li SUS304. Siv B1112 pub dawb- txiav hlau raws li tus qauv ntsuas (nyob ntawm 100%), SUS303 feem ntau ua tiav qhov ntsuas kev ua haujlwm ntawm kwv yees li 78%, thaum SUS304 feem ntau ntsuas ntawm 45% thiab 55%. Vim li no, SUS303 yog dav siv hauv CNC machining, tsis siv neeg tshuab dhos ua haujlwm, thiab tsim cov precision fasteners thiab fittings.

 

SUS 303 vs SUS 304: Corrosion Resistance

SUS304 muab kev tiv thaiv corrosion zoo tshaj hauv cov av noo, chloride- muaj, lossis me ntsis acidic ib puag ncig, ua rau nws tsim nyog rau cov khoom siv ua zaub mov, cov cuab yeej kho mob, thiab cov vaj tsev sab nraum zoov. Nyob rau hauv sib piv, cov sulfur inclusions tam sim no nyob rau hauv SUS303 tuaj yeem ua cov ntsiab lus pib rau pitting corrosion, tshwj xeeb tshaj yog nyob rau hauv marine ib puag ncig los yog kev siv uas cuam tshuam rau cov tshuaj lom neeg. Yog li ntawd, tag nrho cov corrosion kuj ntawm SUS303 yog qis dua li ntawm SUS304.

SUS 303 Vs. SUS 304: Corrosion Resistance

SUS 303 vs SUS 304: Weldability

SUS304 nthuav dav weldability zoo heev thiab tuaj yeem welded siv ntau yam txheej txheem xws li TIG (Tungsten Inert Gas), MIG (Hlau Inert Gas), qhov chaw vuam, thiab arc vuam, uas tsis tshua muaj kev pheej hmoo ntawm kub tawg. Txawm li cas los xij, SUS303 muaj qhov tsis zoo weldability vim hais tias cov sulfur ntxiv los txhim kho kev ua haujlwm ua rau muaj kev pheej hmoo ntawm vuam tawg thiab txo cov vuam vuam.

 

SUS 303 vs SUS 304: Cold Formability

SUS304 qhia tau zoo heev formability thiab yog heev haum rau sib sib zog nqus nqus nqus, dabtsi yog khoov, stamping, thiab lwm yam kev ua haujlwm hnyav. Hauv kev sib piv, SUS303 muaj qhov tsis zoo rau kev ua haujlwm txias txias. Yog li, SUS303 feem ntau yog siv rau cov khoom tsim los ntawm machining ntau dua li cov txheej txheem hnyav.

 

SUS 303 vs SUS 304: Daim ntawv thov

Qib Siv zoo tshaj plaws Yam khoom
TIAB SA 303 Cov ntawv thov uas yuav tsum tau siv cov machining loj lossis qhov nyuaj uas qhov kev pheej hmoo corrosion yog nruab nrab. Cov txiv ntseej, bolts, bushings, shafts, aircraft fittings, gears, thiab hluav taws xob switchgear Cheebtsam.
TIAB SA 304 Cov ntawv thov uas xav tau vuam, tiv thaiv corrosion siab, lossis khoom noj khoom haus - qib kev tu cev. Cov khoom siv ua zaub mov, cov khoom siv hauv chav ua noj, cov thawv ntim tshuaj, cov vaj tse vaj tse, thiab cov tubing kho mob.

 

 

Yog tias koj muaj qhov project- cov kev cai tshwj xeeb rau SUS304 (1.4301) stainless hlau, peb txais tos koj xaj. GNEE khaws cov ntaub ntawv tseem ceeb ntawm qhov zoo tshaj plaws - muag khoom rau koj xaiv. Cov khoom no tuaj yeem ua tiav rau hauv ntau hom khoom siv tswv yim-nrog rau cov phaj, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws chemical muaj pes tsawg leeg specifications lossis thov cov qauv dawb, thov hu rau peb lub Hoobkas tam sim. Peb muab cov nqi sib tw thiab kev pabcuam tshwj xeeb.

SUS304 2B Stainless Steel Sheet
SUS304 2B Stainless Hlau Sheet
SUS304 Stainless Steel Tube
SUS304 Stainless Hlau Tube
 
SUS304 Cold-Rolled Stainless Steel Coil
SUS304 Txias -Rolled Stainless Hlau Chev
SUS304 Stainless Steel Round Bar
SUS304 Stainless Hlau Round Bar

Ntim thiab Shipping
Ntim: Txhua lub phaj lossis kauj yog qhwv hauv cov dej noo- ntawv pov thawj, kab nrog cov yas zaj duab xis, thiab ruaj nrog steel strapping. Cov txheej txheej sab nrauv yog tiv thaiv los ntawm cov ntoo pallets lossis ntoo crates kom muaj kev nyab xeeb thaum caij tsheb mus los thoob ntiaj teb.
Labeling: Txhua pob muaj cov ntaub ntawv hais txog tus lej xov tooj cua sov, qib, qhov ntev, thiab cov qauv siv tau.
Lub sij hawm xa tuaj: Feem ntau hauv 7-15 hnub ua haujlwm tom qab tau txais cov nyiaj them ua ntej.
Shipping Methods: Hiav txwv freight (FCL / LCL), huab cua freight, los yog nthuav qhia, nyob ntawm seb tus neeg yuav tsum tau muaj.

SUS304 2B Stainless Steel Sheet
SUS304 Cold-Rolled Stainless Steel Coil

Xa kev nug