Thaum sofcing stainless cov ntaub ntawv, ntau tus neeg yuav khoom nug: "Dab tsi yog cov sib npaug sib npaug ntawm en 1.440 (316L) stainless hlau?" Nkag siab qhov sib txawv ntawmwrought vs. casting qibPab koj xaiv cov khoom zoo rau koj qhov project. Kab lus no piav qhia txog cov khoom sib txig sib luag, cov khoom tseem ceeb, thiab teb cov lus nug uas neeg yuav khoom muaj.
1. Dab tsi yog en 1.4404 stainless hlau?
EN 1.440 yog cov ntawv tsim tawm sab Europe rau AISI 316L stainless hlau, ib qho tsawg- cov roj carbon aus roj stainless. Nws muaj 16-18% chromium, 10-14% npib tsib, thiab 2-2.5% Molybdenum, thiab Weld cov qauv siv hauv kev ua lag luam, cov cuab yeej siv marine, khoom siv khoom noj, thiab khoom siv kho mob.
2. Dab tsi yog qhov sib npaug sib npaug ntawm 1.4404?
Lub casting sib npaug ntawm 1.4404 (316L) feem ntau yog 1.4409 (en) lossis CF3M (ASTM A743 / A744).
| Wrougrought Qib | Casting Sib Xws | Lub hom phiaj |
|---|---|---|
| 1.4404 (316L) | 1.4409 / cf3m | En / astm |
Qhov no txhais tau tias yog koj qhov project yuav tsum tau muab cov khoom sib xyaw ua ke tsis txhob muab cov khoom siv dov lossis forged, koj tuaj yeem xaiv 1.4409 lossis CF3m rau tib theem ntawm corrosion tsis kam.
Dab tsi yog qhov sib txawv tseem ceeb ntawm 1.440 thiab 1.4409?
| Ntiag tug | 1.4404 (316L Wrought) | 1.4409 (316L casting) |
|---|---|---|
| Khoom daim ntawv | Daim hlau, coils, kav dej, tuav | Li qub, twj, fittings, cov duab sib xyaw |
| Cov ntsiab lus carbon | Tsawg dua los yog sib npaug rau 0.03% | Tsawg dua los yog sib npaug rau 0.03% |
| Corrosion Kuj | Zoo tshaj | Zoo tshaj |
| Cov Khoom Siv Neeg Kho Tshuab | Me ntsis siab dua | Me ntsis qis dua vim yog cov qauv nrum |
| Cov Ntawv Thov | Tso Tsheb Hlau Luam, Pipelines, Sheet Hlau | Lub cev tso qoob loo, lub cuab yeej valve, tsis kam lees |
Cov lus nug yuav khoom
Q1: yog 1.4409 tib yam li 1.4404?
Tsis yog, 1.4409 tsis yog tib yam li 1.4404. Ob qho tib si yog Austenitic stainless hlau, tab sis 1.4409 feem ntau muaj lub zog zoo dua li 1440) thiab ua kom muaj zog zoo dua li 1.440)
Q2: CF3M piv rau 316L yog dab tsi?
CF3M yog lub Attm casting qib sib npaug ntawm 316L, muab cov tshuaj tiv thaiv corrosion zoo heev.
Q3: Uas muaj cov tshuab ua kom zoo dua qub, 1.4404 lossis 1.4409?
1.4409 muaj kev siv tshuab ntau dua li 1.4404. Feem ntau, 1.440 muaj lub zog tensile ntawm 500-700 MPa thiab tau cog lus lub zog ntawm 53 MPa lossis siab dua, txhim kho nws txoj kev ntxhov siab.
Q4: Qhov twg yog 1.4409 (CF3M) siv feem ntau?
Nyob rau hauv lub cev lub cev, li qub, flanges, thiab cam khwb cia fittings uas muaj nyob rau hauv geometry yog xav tau.
Lub casting sib npaug ntawm 1.4404 stainless hlau (316L) yog 1.4409 / CF3m. Thaum ob tus menyuam kawm qib sib koom nrog kev sib xyaw ua ke thiab kev xaiv corrosion, kev xaiv yog yog nyob ntawm seb koj puas xav tau cov khoom siv / siv cov khoom siv lossis nrum seem.