1.4162 stainless hlau, feem ntau hu ua LDX 2101 los yog UNS S32101, yog ib tug lean duplex stainless hlau tsim los muab tus nqi - ua ke zoo ntawm lub zog siab, zoo corrosion kuj, thiab zoo weldability. Nrog nws cov khoom sib npaug ferritic- austenitic microstructure, nws muab kwv yees li ob npaug ntawm cov khoom siv zog ntawm 304 thiab 316 stainless hlau thaum siv cov ntsiab lus nickel thiab molybdenum qis dua. Qhov no ua rau nws muaj txiaj ntsig zoo rau ob qho tib si austenitic thiab cov qauv duplex qib rau ntau yam kev siv.
Cov qib lean duplex no yog tus qauv raws li cov txheej txheem thoob ntiaj teb tseem ceeb.
| Txuj | Qib sib npaug |
|---|---|
| EN (Tebchaws Europe) | 1.4162 |
| ASTM / AISI (USA) | LDX 2101, UNS S32101 |
| Lub Npe | SIB 2101 |
Nws muaj pes tsawg leeg yog optimized nrog manganese thiab nitrogen los hloov ntau nickel thiab molybdenum kim.
| Lub ntsiab | C | Si | Mn | P | S | Cr | Ni | Mo | N | Cu |
|---|---|---|---|---|---|---|---|---|---|---|
| Cov ntsiab lus (%) | Tsawg dua lossis sib npaug li 0.04 | Tsawg dua los yog sib npaug rau 1.0 | 4.0 - 6.0 | Tsawg dua lossis sib npaug li 0.04 | Tsawg dua los yog sib npaug li 0.03 | 21.0 - 22.0 | 1.35 - 1.70 | 0.1 - 0.8 | 0.20 - 0.25 | 0.1 - 0.8 |
Nws muaj lub zog siab nrog zoo toughness thiab corrosion kuj ntawm tus nqi pheej yig.
| Khoom | Yield zog (Rp0.2) | Tensile zog (Rm) | Elongation (A) | Hardness (HB) | Kev cuam tshuam (J) |
|---|---|---|---|---|---|
| Tus nqi | Ntau dua lossis sib npaug li 450 MPa | 650 - 850 MPa | Ntau dua lossis sib npaug li 30% | Tsawg dua lossis sib npaug li 290 | Ntau dua lossis sib npaug rau 100 (20 degree) |
Cov yam ntxwv tseem ceeb thiab kev siv ntawm 1.4162 / LDX 2101
Siab zog:Muab kwv yees li ob npaug ntawm cov khoom muaj zog ntawm cov qib austenitic xws li 304L thiab 316L, tso cai rau kev txo qhov hnyav thiab cov ntu nyias nyias hauv cov qauv siv.
Tus nqi -zoo:Tsawg nickel thiab molybdenum cov ntsiab lus, ua ke nrog manganese thiab nitrogen alloying, muab kev ua tau zoo ntawm tus nqi qis dua thiab ruaj khov dua li cov pa hlau tsis zoo.
Zoo Corrosion Resistance:Muab kev tiv thaiv corrosion piv rau 304L hauv ntau qhov chaw, nrog kev ua haujlwm zoo rau kev ntxhov siab corrosion tawg vim nws cov qauv duplex.
Weldability zoo heev:Yuav tau welded siv cov txheej txheem ntau yam tsis muaj preheating, nrog zoo tiv thaiv hydrogen -induced cracking thiab txo kev pheej hmoo ntawm kub tawg.
Cov ntawv thov tseem ceeb:
Structure Engineering:Txuas hniav, tso tsheb hlau luam, silos, thiab architectural lug xav tau lub zog siab.
Kev thauj mus los:Cov tsheb thauj khoom, tsheb ciav hlau wagons, thiab cov thawv ntim khoom uas txo qhov hnyav tau zoo.
Kev kho dej:Tank, kav dej, thiab cov khoom siv hauv cov chaw kho dej thiab cov dej khib nyiab.
Kev ua zaub mov:Cov khoom siv rau kev tuav cov khoom noj uas xav tau lub zog siab thiab corrosion kuj.
Mining thiab Mineral Processing:Cov ntxaij vab tshaus, conveyors, thiab tuav cov khoom raug puas tsuaj.
Renewable Zog:Hnub ci vaj huam sib luag thav duab thiab cov qauv kev txhawb nqa.
Pulp & Ntawv:Lub tank cia thiab cov khoom siv txheej txheem.
LDX 2101 (1.4162) piv rau 304L (1.4307) li cas?
LDX 2101 muaj kwv yees li ob npaug ntawm cov khoom muaj zog ntawm 304L (450 MPa vs . 200 MPa), ua kom cov khoom hnyav hnyav thiab cov khoom siv nyias nyias. Nws cov corrosion kuj yog piv rau 304L nyob rau hauv ntau qhov chaw, nrog zoo pitting kuj (PREN 25-26 vs. 304L's 18-20) thiab zoo dua rau kev nyuaj siab corrosion cracking. Nws yog magnetic, thaum 304L tsis yog{15}}magnetic. LDX 2101 feem ntau yog tus nqi-zoo thiab tus nqi ruaj khov vim nws cov ntsiab lus qis nickel. Txawm li cas los xij, 304L muaj cov qauv zoo dua rau cov duab nyuaj thiab muaj zog dua ntawm qhov kub thiab txias. LDX 2101 feem ntau yog xaiv rau cov qauv siv uas muaj zog thiab kev lag luam yog qhov tseem ceeb.
Dab tsi yog qhov kev txiav txim siab vuam rau LDX 2101 stainless hlau?
LDX 2101 muaj qhov zoo tshaj plaws weldability vim nws qhov kev ua kom zoo. Nws tuaj yeem welded siv txhua txoj hauv kev yam tsis muaj preheating. Muab cov hlau sib txuam (piv txwv li, 22.8.3.L hom) muaj, txawm tias austenitic fillers kuj tseem siv tau rau cov ntawv thov tsawg dua. Cov ntsiab lus nitrogen siab thiab manganese stabilization txo qhov kev pheej hmoo ntawm hydrogen-induced cracking thiab kub tawg. Kev pom zoo cua sov tawm tswv yim yog 0.5-2.5 kJ / mm, nrog kev sib tshuam kub hauv qab 150 degree. Tiv thaiv roj nrog nitrogen ntxiv (feem ntau Ar + 2-3% N2) pab tswj cov ntsiab lus nitrogen hauv cov hlau vuam. Cov ntsiab lus lean alloy ua rau nws zam ntau dua rau vuam ntau dua - qib alloyed duplex, nrog lub qhov rais ua haujlwm dav dua thiab zoo heev li -welded zog yam tsis muaj kev kho cua sov tom qab vuam.




Nrhiav kev ntseeg siab ntawm 1.4162 / LDX 2101 Stainless Hlau?
GNEE Steel cov khoom siv tus nqi -zoo LDX 2101 (1.4162) lean duplex stainless hlau hauv phaj, ntawv, bar, yeeb nkab, thiab cov qauv siv rau kev thov. Peb muab cov ntaub ntawv pov thawj tag nrho (EN 10204 3.1) thiab kev txhawb nqa suav nrog kev txiav, khoov, sib sau, thiab kev pabcuam vuam. Yog tias koj muaj kev xav tau, thov koj xav tiv tauj peb.