1.4117 stainless hlau, feem ntau hu ua 440A lossis UNS S44002, yog siab -carbon martensitic stainless hlau uas muaj qhov sib npaug zoo ntawm hardness, corrosion resistance, thiab toughness. Raws li tus tswv cuab qis dua ntawm 440 series, nws muab me ntsis qis dua hardness dua 440B thiab 440C tab sis muaj kev txhim kho toughness thiab zoo corrosion kuj vim tsawg chromium carbides. Qhov no ua rau nws tsim nyog rau cov ntawv thov uas xav tau kev hnav tsis zoo, kev tuav tuav zoo, thiab kev tiv thaiv corrosion txaus, xws li cutlery, bearings, cov cuab yeej phais, thiab cov khoom siv valve.
Qib sib npaug ntawm 1.4117 stainless hlau
| Txuj | Qib sib npaug |
|---|---|
| EN (Tebchaws Europe) | 1.4117 |
| ASTM / AISI (USA) | 440A, UA S44002 |
| JIS (Nyiv) | SUS 440A |
| Lub Npe | 440A |
Tshuaj muaj pes tsawg leeg ntawm 1.4117 stainless hlau
| Element | C | Si | Mn | P | S | Cr | Mo |
|---|---|---|---|---|---|---|---|
| Cov ntsiab lus (%) | 0.60 - 0.75 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug li 0.04 | Tsawg dua lossis sib npaug li 0.03 | 16.0 - 18.0 | Tsawg dua lossis sib npaug li 0.75 |
Mechanical zog ntawm 1.4117 stainless hlau
| Qhov xwm txheej | Yield zog (Rp0.2) | Tensile zog (Rm) | Elongation (A) | Hardness (HRC) |
|---|---|---|---|---|
| Annealed | ~ 450 MPa | ~ 740 MPa | ~ 15% | ~ 25 HRC |
| Hardened & Tempered | Ntau dua lossis sib npaug li 550 MPa | Ntau tshaj lossis sib npaug li 700 MPa | Ntau dua lossis sib npaug li 12% | 52 - 56 HRC |
Cov yam ntxwv tseem ceeb thiab kev siv ntawm 1.4117 / 440A
Zoo sib npaug ntawm Hardness thiab Toughness:Cov ntsiab lus qis dua muab me ntsis qis dua qhov nyuaj tshaj li 440B lossis 440C tab sis muaj cov tawv tawv zoo dua, ua rau nws tsis nkig thiab tiv taus ntau dua.
Nruab nrab Corrosion Resistance:Muaj kev tiv thaiv corrosion zoo dua li 440B thiab 440C vim tsawg dua chromium carbides hauv microstructure, nrog kev ua haujlwm zoo ib yam li 420 hauv feem ntau ib puag ncig.
Sib nqus thiab Hardenable:Muaj zog sib nqus thiab teb zoo rau kev kho cua sov, nrog zoo los ntawm - muaj peev xwm hardening.
Zoo hnav tsis kam:Muab kev hnav tsis taus txaus rau ntau daim ntawv thov yam tsis muaj qhov brittleness ntawm qib siab dua carbon.
Cov ntawv thov tseem ceeb:
Cov tais diav:Nruab nrab-ntau riam, hniav, txiab, thiab cov tais diav hauv chav ua noj yuav tsum muaj qhov sib npaug ntawm ntug tuav thiab tawv.
Bearings:Pob bearings thiab kev sib tw rau kev thov tsawg dua.
Surgical Instruments:Cov cuab yeej xav tau cov npoo ntse thiab zoo corrosion kuj.
Valve Cheebtsam:Cov rooj zaum, cov pob, thiab cov stems nyob rau hauv kev siv me me.
Cov cuab yeej muaj:Gauges, ntsuas cov cuab yeej, thiab tshuab qhov yuav tsum tau muaj kev ruaj ntseg.
Cov cuab yeej kho hniav:Cov cuab yeej xav tau kom tsis muaj menyuam tsis taus thiab zoo ntug tuav.
440A (1.4117) piv rau 440B (1.4112) thiab 440C (1.4125) li cas?
Dab tsi yog qhov pom zoo kho cua sov rau 440A stainless hlau?
Dab tsi yog qhov kev txiav txim siab vuam rau 440A?
Nrhiav kev ntseeg siab ntawm 1.4117 / 440A Stainless Hlau?

1.4117 Stainless hlau kav

1.4117 Stainless Hlau Phaj

1.4117 Stainless Hlau Coils
Xa kev nug