Kuv tuaj yeem qhia tau li cas yog tias kuv cov hlau tsis muaj steel yog 1.4062?
Mar 18, 2026
Tso lus
Taw qhia rau 1.4062 Stainless Hlau
1.4062 stainless hlau, feem ntau hu ua 2304 los yog UNS S32304, yog ib tug lean duplex stainless hlau uas muaj tus nqi - zoo tshuav nyiaj li cas ntawm lub zog siab, zoo corrosion kuj, thiab zoo heev tiv thaiv kev nyuaj siab corrosion cracking. Nrog nws cov ferritic -austenitic microstructure, nws muab kwv yees li ob npaug ntawm cov txiaj ntsig zoo ntawm cov qib austenitic zoo li 304L thiab 316L, thaum xav tau qis nickel thiab molybdenum cov ntsiab lus. Qhov no ua rau nws yog ib qho kev siv nyiaj txiag rau cov ntawv thov uas cov ntsiab lus siab dua ntawm cov qauv duplex 2205 tsis tsim nyog.
Specification ntawm 1.4062 stainless hlau
Qib sib npaug ntawm 1.4062 stainless hlau
| Txuj | Qib |
|---|---|
| EN European | 1.4062 / X2CrNiN22-2 |
| ASTM / UNS | S32202 |
| Lub Npe | Lean Duplex 2304 |
Muaj cov ntaub ntawv: coils, nplooj ntawv, phaj, tuav, welded raj, profiles.
Chemical Composition (ntau feem pua ntawm EN 10088-1) ntawm 1.4062 stainless hlau
| Element | C | Si | Mn | P | S | Cr | Ni | Mo | N |
|---|---|---|---|---|---|---|---|---|---|
| Cov ntsiab lus | Tsawg dua lossis sib npaug li 0.030 | Tsawg dua lossis sib npaug li 1.00 | Tsawg dua lossis sib npaug li 2.00 | Tsawg dua lossis sib npaug li 0.040 | Tsawg dua lossis sib npaug li 0.010 | 21.5‑23.5 | 1.0‑3.0 | 0.2‑0.8 | 0.14‑0.24 |
PREN ≈25–28. Ultra-low carbon txo qhov kev pheej hmoo ntawm intergranular-corrosion tom qab vuam. Balanced austenite-ferrite microstructure muab lub zog zoo thiab nruab nrab chloride-corrosion kuj.
Mechanical Properties ntawm 1.4062 stainless hlau
| Khoom | Tus nqi |
|---|---|
| Tensile zog Rm | 620-820 MPa |
| 0.2% Offset Yield zog Rp0.2 | Ntau dua lossis sib npaug li 450 MPa |
| Elongation A | Ntau dua lossis sib npaug li 25% |
| Brinell Hardness HBW | Tsawg dua lossis sib npaug li 290 |
Yield zog kwv yees li ob zaug ntawm 316L austenitic hlau. Tsis hardenable los ntawm kev kho cua sov. Tsis txhob cuam tshuam mus ntev hauv 300-950℃los tiv thaiv sigma-theem embrittlement. Kev daws annealing ntau: 950-1050 degree, yuav tsum tau ua kom txias sai.
Lub cev muaj zog (20 degree) ntawm 1.4062 stainless hlau
| Yam khoom | Parameter |
|---|---|
| Qhov ntom | 7.80 g / cm³ |
| Modulus ntawm Elasticity | 200 GPa |
| Coefficient ntawm Linear Expansion | 13.5 × 10⁻⁶ /℃(20-100 degree) |
| Thermal conductivity | 14.8 W/(m·K) |
| Melting ntau | 1370-1420 degree |
| Microstructure | Austenitic-ferritic duplex, sib nqus |
| Max nruam kev pab kub | Tsawg dua los yog sib npaug li 300 degree |
Cov yam ntxwv tseem ceeb ntawm 1.4062 / 2304stainless hlau
Lub zog zoo li cas 1.4062 stainless hlau muaj?
1.4062 muab cov khoom siv zog ntau dua. Nws lub zog tawm los mus txog 400 MPa, ze li ob npaug ntawm 304L thiab 316L austenitic stainless hlau ntawm 200 MPa. Lub zog zoo tshaj no tso cai rau cov phab ntsa nyias nyias thiab txo qhov hnyav tag nrho rau cov qauv siv thiab cov kav dej.
1.4062 corrosion kuj zoo li cas?
1.4062 muab kev sib npaug corrosion ntawm 304L thiab 316L, nrog tus nqi PREN ib txwm ntawm 24-26. Nws muaj kev tiv thaiv zoo heev rau kev ntxhov siab corrosion tawg hauv qab chloride- muaj cov kev pabcuam.
Dab tsi yog 1.4062 tus nqi kom zoo dua piv nrog cov qauv duplex steel?
Qib no muaj cov nqi zoo tshaj -kev ua tau zoo. Nrog qis nickel thiab molybdenum muaj pes tsawg leeg, nws yog kev lag luam ntau dua li tus qauv 2205 duplex steel, thaum muab kev ua tau zoo tag nrho tshaj li cov pa austenitic stainless hlau.
Puas yog 1.4062 txhawb kev vuam yooj yim?
Yog lawm, 1.4062 muaj kev txhim khu kev qha weldability. Nws tuaj yeem welded nrog cov txheej txheem vuam cov txheej txheem siv cov khoom siv hlau tsim nyog. Weld cheeb tsam khaws cov khoom ruaj khov thiab corrosion, thiab tsis muaj kev tshaj tawm -weld cua sov yuav tsum tau kho.
Daim ntawv thov ntawm 1.4062 / 2304stainless hlau
1. Kev kho dej & kev siv dej ua haujlwm
Cov kav dej haus-dej, cov kav dej khib nyiab hauv nroog, cov tso tsheb hlau luam, cov kav dej hauv tsev, cov kav dej hauv tsev, cov kav dej txuas rau cov nroj tsuag desalination rau cov kua qaub nruab nrab. Thinner-wall design pab txo cov nqi ntawm qhov project.
2.Architectural & structural engineering
Footbridges, kev sib tsoo teeb meem, architectural load-bearing Cheebtsam, leveraging siab zog rau lub teeb yuag.
3.Pulp, ntawv & khoom noj khoom haus kev lag luam
Daim ntawv-tshuab claddings, txheej txheem tso tsheb hlau luam, kua txiv hmab txiv ntoo thiab zaub mov-qib cov nkoj cia rau kev pabcuam zaub mov. -4.Coastal-marine auxiliary chaw: Off-coastal structural Cheebtsam thiab auxiliary piping rau ntug hiav txwv ntsev-fog ib puag ncig (tsis yog rau hnyav-chloride lub ntsiab seawater txheej txheem kab). -
5.Pressure nkoj & cia tank
Cov tso tsheb hlau luam nruab nrab-tso siab thiab cov roj cia cov nkoj ua raws li PED cov cai rau kev pabcuam me me.
6.Automotive & kev lag luam dav dav
Automotive structural qhov chaw thiab welded sib dhos nyob rau hauv nruab nrab-corrosion tej yam kev mob, tsis muaj kev kho cua sov tom qab vuam yuav tsum tau.
Khoom noj khoom haus qib pipelines

ib puag ncig-tiv thaiv pipelines
industrial pipelines
Exporter Profileua 1.4062stainless hlau
Raws li tus kws tshaj lij stainless hlau tsum, GNEE muab ib qho kev daws teeb meem rau 1.4062 stainless hlau. Peb cov khoom muaj xws li daim hlau & coils, puag ncig tuav, seamless thiab welded raj, flanges thiab customized-made forgings. Cov khoom no tau siv dav hauv kev tiv thaiv corrosion engineering xws li tshuaj lom neeg, petrochemical, dej kho, marine thiab seawater desalination chaw. Cov kev pabcuam muaj nqis ntxiv nrog rau kev txiav-rau-loj, beveling thiab polishing muaj. Multi-layer rust-proof standard seaworthy packing ua kom muaj kev nyab xeeb ntawm kev xa khoom mus rau qhov chaw thoob plaws ntiaj teb.

1.4482 stainless hlau raj

stainless hlau phaj

1.4482 stainless hlau tuav
Yog tias koj xav tau kev txhawb nqa txog qhov project, kev pom zoo xaiv cov khoom siv lossis cov lus hais txog qhov project, thov koj xav tiv tauj peb. GNEE pab pawg kws tshaj lij thiab kev muag khoom yuav muab cov kev daws teeb meem zoo sib xws rau koj.
FAQ
2304 (1.4062) piv rau 304L (1.4307) thiab 316L (1.4404) li cas?
2304 muaj kwv yees li ob npaug ntawm cov khoom muaj zog ntawm ob qho tib si 304L thiab 316L (400 MPa vs . 200 MPa), ua kom muaj kev txuag hnyav hauv cov qauv tsim thiab tso cai rau cov khoom siv thinner. Nws cov corrosion kuj nyob ntawm 304L thiab 316L, nrog PREN 24-26 muab cov pitting zoo dua li 304L (PREN 18-20) tab sis tsawg dua 316L (PREN 24-26 nyob ntawm seb muaj pes tsawg leeg). Nws muab kev tiv thaiv zoo tshaj plaws rau chloride kev nyuaj siab corrosion cracking piv rau ob qib austenitic . 2304 feem ntau yog tus nqi zoo dua li 316L thiab tus nqi ruaj khov vim qis nickel cov ntsiab lus. Txawm li cas los xij, 304L thiab 316L muab cov qauv zoo dua rau cov duab nyuaj thiab muaj zog dua ntawm qhov kub thiab txias heev . 2304 feem ntau yog xaiv los ua ib qho kev siv zog ntau dua rau 304L, lossis ua lwm txoj hauv kev lag luam rau 316L qhov twg nws cov corrosion kuj txaus.
Dab tsi yog qhov kev txiav txim siab vuam rau 2304 (1.4062) duplex stainless hlau?
Vuam 2304 yuav tsum tswj xyuas qhov sib npaug ferrite-austenite microstructure rau cov khoom zoo. Cov kev coj ua uas pom zoo suav nrog kev siv qhov sib txuam lossis me ntsis dhau ntawm- cov hlau nplaum uas muaj hlau (feem ntau yog 2209 hom), tswj cov khoom siv hluav taws xob (0.5-2.5 kJ/mm), thiab tswj qhov kub ntawm qhov sib txawv hauv qab 150℃. Tiv thaiv roj nrog nitrogen ntxiv (feem ntau Ar + 2-3% N2) pab tswj cov ntsiab lus nitrogen thiab txhawb kev tsim cov austenite hauv cov hlau vuam. Preheating feem ntau tsis tas yuav tsum tau ua, thiab tom qab-weld kev kho cua sov tsis tsim nyog. Cov ntsiab lus qis qis ua rau 2304 zam ntau dua rau vuam ntau dua - qib alloyed duplex, nrog lub qhov rai ua haujlwm dav dua thiab txo qhov kev pheej hmoo ntawm kev tsim cov theem tsis zoo. Rau qhov zoo tshaj plaws corrosion kuj nyob rau hauv ib puag ncig hnyav, over-alloyed muab tub lim hlau yuav raug txiav txim siab los them rau ib qho kev poob nitrogen thaum lub sij hawm vuam.
Xa kev nug