Dab tsi yog Cov Khoom Ntawm EN 1.4002 Stainless Hlau?
Apr 02, 2026
Tso lus
1.4002 stainless hlau, feem ntau hu ua 405 lossis UNS S40500, yog qhov qis -carbon ferritic stainless hlau tsim tshwj xeeb rau cov ntawv thov uas yuav tsum tau ua rau siab oxidation thiab zoo corrosion kuj nyob rau hauv ib puag ncig me me, nrog kev txhim kho weldability piv rau siab dua -carbon .ferritic grades Nws cov ntsiab lus qis dua thiab aluminium ntxiv pab tiv thaiv kom tawv nqaij thaum vuam thiab txo qhov cuam tshuam rau intergranular corrosion, ua rau nws haum rau welded Cheebtsam nyob rau hauv nruab nrab kub kev pab cuam.
Qib sib npaug rau 1.4002 stainless hlau
| Txuj | Qib sib npaug |
|---|---|
| EN (Tebchaws Europe) | 1.4002 |
| ASTM / AISI (USA) | 405, UA S40500 |
| JIS (Nyiv) | SUS 405 |
| Lub Npe | 405 |
Cov tshuaj muaj pes tsawg leeg ntawm 1.4002 stainless hlau
| Element | C | Si | Mn | P | S | Cr | Al |
|---|---|---|---|---|---|---|---|
| Cov ntsiab lus (%) | Tsawg dua los yog sib npaug li 0.08 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug li 0.04 | Tsawg dua lossis sib npaug li 0.03 | 11.5 - 14.5 | 0.10 - 0.30 |
Cov khoom ntawm 1.4002 stainless hlau
| Khoom | Yield zog (Rp0.2) | Tensile zog (Rm) | Elongation (A) | Hardness (HB) |
|---|---|---|---|---|
| Tus nqi | Ntau dua lossis sib npaug li 205 MPa | 380 - 550 MPa | Ntau dua lossis sib npaug li 20% | Tsawg dua los yog sib npaug li 190 |
Cov yam ntxwv tseem ceeb thiab kev siv ntawm 1.4002 / 405
Txhim kho Weldability:Kev sib xyaw ua ke ntawm cov pa roj carbon tsawg thiab txhuas ntxiv ua rau txhim kho weldability piv rau lwm cov qib ferritic, txo qhov nyiam ntawm cov qoob loo loj hlob thiab tawv tawv hauv tshav kub- cuam tshuam cheeb tsam.
Zoo Siab -Tub kub Oxidation Resistance:Muab kev tiv thaiv txaus rau scaling thiab oxidation ntawm qhov kub siab txog li 650 degree, haum rau nruab nrab -kev siv kub.
Tsawg Ua Haujlwm Hardening Rate:Tsom pom kev ua haujlwm qis dua li qib austenitic, uas tuaj yeem ua tau zoo rau qee yam kev ua haujlwm.
Sib nqus thiab nqi-zoo:Muaj zog sib nqus thiab txuag nyiaj ntau dua npib tsib xee- muaj cov qib austenitic.
Cov ntawv thov tseem ceeb:
Thaum tshav kub kub Exchangers:Cheebtsam hauv nruab nrab- cov khoom siv hluav taws xob hloov pauv kub.
Cov khoom siv Petrochemical:Cov tais diav, hauv ob sab phlu, thiab sab hauv hauv kab thiab cov hlab ntsha.
Cov khoom siv Annealing:Rauv qhov chaw, pob tawb, thiab cov khoom siv ua haujlwm ntawm qhov kub nruab nrab.
Chav Nozzles:Cheebtsam hauv chav tshuab.
Automotive:Cov pa hluav taws xob cov khoom hauv qis dua - qhov kub thiab txias.
Architectural:Kho kom zoo nkauj daim ntaub ntawv qhov twg weldability yuav tsum tau.
405 (1.4002) piv rau 410 (1.4006) thiab 304 (1.4301) li cas?
Dab tsi yog qhov kev txiav txim siab vuam rau 405?
Qhov ntsuas kub li cas yog 405 haum rau?
Nrhiav kev ntseeg siab ntawm 1.4002 / 405 Stainless Hlau?

1.4002 Stainless hlau yeeb nkab

1.4002 Stainless Hlau Phaj

1.4002 Stainless hlau Bar
Xa kev nug