UNS S31600 Stainless Hlau - Molybdenum{1}}Alloyed Chloride Corrosion Shield

Mar 20, 2026

Tso lus

Product Overview

UNS S31600 yog molybdenum- txhim kho austenitic stainless hlau, tsim los daws cov kev txwv ntawm S30400 hauv chloride- thaj chaw nplua nuj. Featuring 2.0-3.0% molybdenum nrog rau 16-18.5% chromium thiab 10-14% npib tsib xee, nws muab qhov zoo tshaj pitting thiab crevice corrosion kuj, ua rau nws zoo tagnrho rau marine, ntug hiav txwv dej, thiab tshuaj ua cov chaw. Qib no khaws cov khoom tsis yog{15}} sib nqus, ductile austenitic qauv, nrog zoo heev kub-kub toughness thiab fabricability. Tsis zoo li S30400, S31600 thrives nyob rau hauv hnyav, ntsev-laden atmospheres thiab me me tshuaj daws teeb meem, ua hauj lwm raws li tus mus-rau upgrade rau daim ntaub ntawv uas yuav tsum tau txhim kho corrosion durability.

Chemical Composition (Mass Fraction, %)

C Tsawg dua lossis sib npaug 0.08, Cr: 16.00-18.50, Ni: 10.00-14.00, Mo: 2.00-3.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug rau 0.04 lossis sib npaug 0.04 lossis sib npaug sib 0.11

Mechanical Properties (Annealed Condition)

Tensile Strength Ntau dua lossis sib npaug ntawm 520 MPa; Yield zog ntau dua los yog sib npaug rau 205 MPa; Elongation Ntau dua lossis sib npaug li 40%; Hardness Tsawg dua los yog sib npaug rau 215 HB

Core Zoo

Tshwj xeeb chloride-induced pitting/crevice corrosion kuj; superior kev ua tau zoo nyob rau hauv marine / tshuaj ib puag ncig; zoo tsawg-kub toughness; tsis yog-magnetic; muaj peev xwm ua tau ntau yam thiab vuam; ruaj nyob rau hauv hnyav atmospheric tej yam kev mob.

Tej kev siv

Marine hardware, chemical processing equipment, desalination systems, coastal construction, pharmaceutical machinery, and food processing units with salt exposure.

Qib sib npaug

AISI 316, EN 1.4401, GB 06Cr17Ni12Mo2, SUS316

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug