SUS440C - Siab-Carbon 440-Series Martensitic Alloy Rau Kev Hnav Siab Tshaj Plaws

Mar 30, 2026

Tso lus

Txheej txheem cej luam

SUS440C yog qhov siab -carbon variant ntawm JIS 440-series, xa siab tshaj plaws hnav tsis kam thiab hardness ntawm 440-series qib. Nrog 0.95-1.20% carbon thiab 16.00-18.00% chromium, nws ua tiav qhov tawv ntawm 58-60 HRC tom qab kev kho cua sov, ua rau nws zoo tagnrho rau cov ntawv thov uas xav tau kev hnav tsis kam thiab ntug tuav. Nws muaj molybdenum los txhim kho corrosion kuj thiab hardenability, thiab yog sib nqus nrog zoo machinability thaum annealed. Piv nrog rau SUS440A thiab SUS440B, nws yog qhov yooj yim rau brittleness thiab yuav tsum tau ceev faj kev kho cua sov (xws li txias txias hauv qab -70 degree), tab sis muaj unmatched hnav durability rau cov ntaub ntawv tseem ceeb.

Chemical Composition (wt%)

C: 0.95-1.20, Cr: 16.00-18.00, Mo: 0.75-1.25, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.040, S Less dua lossis sib npaug 0.075 lossis sib npaug

Tej yam khoom siv cuab yeej cuab tam (Quenched & Tempered Condition)

Tensile Strength (Rm): Ntau dua lossis sib npaug rau 1970 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 1900 MPa; Elongation (A): Ntau dua lossis sib npaug li 2%; Hardness (HRC): 58-60

Core Zoo

Qhov siab tshaj plaws hnav tsis kam thiab hardness ntawm 440- series variants; zoo heev ntug tuav rau siab -cov cuab yeej txiav; nruab nrab corrosion kuj; Sib nqus; zoo machinability nyob rau hauv lub xeev annealed; siab - qhov kub thiab txias stability; haum rau kev siv hnyav hnyav hnyav.

Daim ntawv thov

Siab -Kev ua tau zoo tactical riam, precision bearings, phais hniav, pwm, valve Cheebtsam, twj tso kua mis ncej, thiab tseem ceeb hnav qhov chaw uas yuav tsum tau heev durability thiab ntug tuav.

Qib sib npaug

EN 1.4125, UNS S44004, GB 11Cr17, AISI 440C

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug