SUS440B - Nruab nrab-Carbon 440-Series Martensitic Alloy Rau Kev Txhim Kho Hnav Kev Ua Haujlwm
Mar 30, 2026
Tso lus
Txheej txheem cej luam
SUS440B yog qhov nruab nrab -carbon variant ntawm JIS 440-series, muab kev hnav siab dua li SUS440A thaum tuav zoo toughness. Nrog 0.75-0.95% carbon thiab 16.00-18.00% chromium, nws ua tiav qhov hardness ntawm 56-58 HRC tom qab kev kho cua sov, ua rau nws tsim nyog rau cov ntawv thov uas yuav tsum tau siv zog ntxiv. Nws muaj molybdenum los txhim kho corrosion kuj thiab hardenability, thiab yog sib nqus nrog zoo machinability thaum annealed. Piv rau SUS440A, nws yuav tsum tau ua tib zoo kho cua sov kom tsis txhob brittleness, tab sis muab kev hnav zoo tshaj plaws rau kev siv hnyav.
Chemical Composition (wt%)
C: 0.75-0.95, Cr: 16.00-18.00, Mo: 0.75-1.25, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.040, S Less dua lossis sib npaug 0.075 lossis sib npaug
Tej yam khoom siv cuab yeej cuab tam (Quenched & Tempered Condition)
Tensile Strength (Rm): Ntau dua lossis sib npaug rau 1930 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 1860 MPa; Elongation (A): Ntau dua lossis sib npaug li 3%; Hardness (HRC): 56-58
Core Zoo
Siab hnav tsis kam tshaj SUS440A; zoo toughness thiab corrosion kuj; cua sov- kho tau kom siab hardness; Sib nqus; zoo machinability nyob rau hauv lub xeev annealed; zoo heev ntug tuav rau hnyav- cov cuab yeej txiav; haum rau hnav- daim ntawv thov hnyav.
Daim ntawv thov
Hnyav- rab riam, bearings, iav, valve Cheebtsam, cov cuab yeej phais, cov cuab yeej txiav, thiab cov khoom precision uas yuav tsum tau ua kom muaj kev tiv thaiv zoo thiab kev tiv thaiv corrosion.
Qib sib npaug
EN 1.4125, UNS S44003, GB 9Cr18Mo, AISI 440B
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug