STS439 - Titanium-Stabilized Ferritic Alloy rau Welded Siab-Tsem Cheebtsam
Mar 30, 2026
Tso lus
Txheej txheem cej luam
STS439 yog titanium-stabilized ferritic stainless hlau, tsim los tshem tawm intergranular corrosion nyob rau hauv welded Cheebtsam yam tsis tas yuav tsum tau rau post-weld annealing. Nrog 17.00-19.00% chromium thiab 0.10-0.30% titanium, nws muaj superior corrosion thiab oxidation kuj piv rau STS430, tshwj xeeb tshaj yog nyob rau hauv chloride{11}}muaj thiab siab{12}}kub ib puag ncig. Nws yog hlau nplaum, muaj zoo formability thiab thermal conductivity, thiab yog haum rau loj welded lug vim nws ruaj khov weld kev ncaj ncees. Nws qhov sib npaug sib npaug ua rau nws muaj txiaj ntsig zoo xaiv rau welded industrial Cheebtsam uas yuav tsum tau txhim khu kev ntseeg siab-kub.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.07, Cr: 17.00-19.00, Ti: 0.10-0.30, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.040, S Less dua lossis sib npaug 0.050 lossis sib npaug Ni 0.040 ib
Tej yam cuab yeej cuab tam (Annealed Condition)
Tensile Strength (Rm): Ntau dua lossis sib npaug li 455 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 296 MPa; Elongation (A): Ntau dua lossis sib npaug li 32%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 170
Core Zoo
Titanium stabilization tiv thaiv intergranular corrosion hauv welds; tsis muaj ncej-weld annealing yuav tsum tau; superior corrosion thiab oxidation kuj piv rau STS430; zoo weldability thiab formability; sib nqus nrog zoo heev thermal conductivity; haum rau siab - kev pabcuam kub (txog 760 degree); tus nqi- zoo rau cov qauv welded.
Daim ntawv thov
Welded heat exchangers, boiler Cheebtsam, automotive tso manifolds, industrial piping, chemical processing equipment, coj mus muag hauv chav ua noj, thiab loj welded structural qhov chaw nyob rau hauv me me mus rau nruab nrab corrosive ib puag ncig.
Qib sib npaug
EN 1.4510, UNS S43900, GB 022Cr18Ti, AISI 439, SUS439
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug