Feb 05, 2026

Tso lus

ASTM B673 Stainless Steel 904L Seamless PipeSS 1.4539 Stainless Steel Mechanical PropertiesGrade 420J2 (UNS S42000) stainless steel

Kev sib xyaw

Cov lus hauv qab no muab cov kev sib xyaw ua ke ntawm qib 904L stainless hlau:

Table 1. Kev sib xyaw ua ke ntawm qib 904L stainless hlau

Qib

C

Mn

Si

P

S

Cr

Mo

Ni

Cu

904L

min.

max.

-

0.02

-

2

-

1

-

0.045

-

0.035

19

23

4

5

23

28

1

2

Mechanical Properties

Cov khoom siv kho tshuab raug ntawm qib 904L stainless hlau tau muab rau hauv cov lus hauv qab no:

Rooj 2.Mechanical zog ntawm qib 904L stainless hlau

Qib

Tensile zog (MPa) min

Yield Strength 0.2% Pov thawj (MPa) min

Elongation (% hauv 50mm) min

Hardness

Rockwell IB (HR B)

Brinell (HB)

904L

490

220

36

70-90 Nws

150