Stainless Hlau Qib 304L - Tsawg Carbon Corrosion Resistant

Feb 05, 2026

Tso lus

Stainless Steel Grade 304 - Food Grade & Corrosion ResistantStainless Steel Grade 2205 - Duplex High Strength GradeStainless Steel Grade 430 - Magnetic Stainless Steel Grade

Chemical Composition ntawm Stainless Hlau 304

Table 1.Tshuaj muaj pes tsawg leeg rau 304 stainless hlau alloys

%

304

304L

304H

C

0.0 - 0.07

0.0 - 0.03

0.04 - 0.08

Mn

0.0 - 2.0

0.0 - 2.00

0.0 - 2.0

Si

0.0 - 1.00

0.0 - 1.00

0.0 - 1.0

P

0.0 - 0.05

0.0 - 0.05

0.0 - 0.04

S

0.0 - 0.03

0.0 - 0.02

0.0 - 0.02

Cr

17.50 - 19.50

17.50 - 19.50

17.00 - 19.00

Ni

8.00 - 10.50

8.00 - 10.50

8.00 - 11.00

Fe

Tshuav

Tshuav

Tshuav

N

0.0-0.11

0.0-0.11

0.0 - 0.10

 

Cov khoom ntawm Stainless hlau 304

Mechanical Properties ntawm Stainless hlau 304

Tab 2 a.Mechanical zog rau 304 stainless hlau alloys - daim ntawv mus txog 8 hli tuab

Qib

304

304L

304H

Tensile zog (MPa)

540 - 750

520 - 700

-

Pov thawj Stress (MPa)

230 Min

220 Min

-

Elongation A50 hli

45 Min %

45 Min %

-


Tab 2b.Mechanical zog rau 304 stainless hlau alloys - phaj los ntawm 8 - 75 hli tuab

Qib

304

304L

304H

Tensile zog (MPa)

520 - 720

500 - 700

-

Pov thawj Stress (MPa)

210 Min

200 Min

-

Elongation A5

45 Min %

45 Min %

-


Tab 2 c.Mechanical zog rau 304 stainless hlau alloys - bar thiab seem mus txog 160 mm inch / thickness

Qib

304

304L

304H

Tensile zog (MPa)

500 - 700

500 - 700

500 - 700

Pov thawj Stress (MPa)

190

175 Min

185 Min

Elongation A50 hli

45 Min %

45 Min %

40 Min %

Hardness Brinell

215 Max HB

215 Max HB

-