Stainless Steel Qib 321 - Kub Kub Resistant Qib
Feb 26, 2026
Tso lus



Kev sib xyaw
Cov txheej txheem sib xyaw ua ke rau qib 321 stainless hlau yog muab rau hauv rooj 1.
Table 1.Kev sib xyaw ua ke rau 321-qib stainless hlau
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni | N | Lwm yam | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 321 | min. max |
- 0.08 |
2.00 | 0.75 | 0.045 | 0.030 | 17.0 19.0 |
- | 9.0 12.0 |
0.10 | Ti=5(C+N) 0.70 |
| 321H | min. max |
0.04 0.10 |
2.00 | 0.75 | 0.045 | 0.030 | 17.0 19.0 |
- | 9.0 12.0 |
- | Ti=4(C+N) 0.70 |
| 347 | min. max |
0.08 | 2.00 | 0.75 | 0.045 | 0.030 | 17.0 19.0 |
- | 9.0 13.0 |
- | Nb=10(C+N) 1.0 |
Mechanical Properties
Tej yam khoom siv rau qib 321 stainless hlau yog muab rau hauv rooj 2.
Rooj 2.Mechanical zog ntawm 321-qib stainless hlau
| Qib | Tensile zog (MPa) min | Yield Strength 0.2% Pov thawj (MPa) min | Elongation (% hauv 50 mm) min | Hardness | |
|---|---|---|---|---|---|
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 321 | 515 | 205 | 40 | 95 | 217 |
| 321H | 515 | 205 | 40 | 95 | 217 |
| 347 | 515 | 205 | 40 | 92 | 201 |
Lub cev muaj zog
Cov khoom siv lub cev zoo rau qib annealed qib 321 stainless hlau yog muab rau hauv rooj 3.
Table 3.Lub cev muaj zog ntawm 321-qib stainless hlau nyob rau hauv cov mob annealed
| Qib | Qhov ceev (kg / m3) | Elastic Modulus (GPa) | Lub ntsiab lus Coefficient ntawm Thermal Expansion (μm / m / degree) | Thermal conductivity (W / mK) | Kev kub ceev 0-100℃(J / kg.K) | Hluav taws xob tiv thaiv (nΩ) | |||
|---|---|---|---|---|---|---|---|---|---|
| 0-100 degree | 0-315 degree | 0-538 ° C | ntawm 100 degree | ntawm 500 degree | |||||
| 321 | 8027 | 193 | 16.6 | 17.2 | 18.6 | 16.1 | 22.2 | 500 | 720 |
Qib Specification Sib piv
Kwv yees qib sib piv rau 321 stainless hlau ntawv yog muab rau hauv rooj 4.
Table 4.Qib specifications rau 321-qib stainless hlau
| Qib | UNS No | Laus British | Euronorm | Swedish SS | Japanese JIS | ||
|---|---|---|---|---|---|---|---|
| BS | En | Tsis muaj | Lub npe | ||||
| 321 | S32100 | 321S31 | 58B, 58C | 1.4541 | X6CrNiTi18-10 | 2337 | TIAB SA 321 |
| 321H | S32109 | 321S51 | - | 1.4878 | X10CrNiTi18-10 | - | SUS 321 H |
| 347 | S34700 | 347S31 | 58G | 1.4550 | X6CrNiNb18-10 | 2338 | TIAB SA 347 |
Tom ntej: 1.4537 Stainless hlau yog dab tsi?