Stainless hlau - Qib 316 (UNS S31600)

Feb 26, 2026

Tso lus

201 Stainless Steel Strip - Processing Performance and Industrial Application316 Stainless Steel Profile - Marine Engineering and Corrosion ResistanceHot Rolled 440 Stainless Steel Plate

Cov khoom tseem ceeb

Cov khoom no tau teev tseg rau cov khoom lag luam tiaj tus (phaj, ntawv thiab coil) hauv ASTM A240 / A240M. Zoo sib xws tab sis tsis tas yuav zoo ib yam khoom yog teev rau lwm yam khoom xws li yeeb nkab thiab bar hauv lawv cov specifications.

Kev sib xyaw

Table 1.Kev sib xyaw ua ke rau qib 316 ntawm stainless hlau.

Qib   C Mn Si P S Cr Mo Ni N
316 Min - - - 0 - 16.0 2.00 10.0 -
Max 0.08 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316L Min - - - - - 16.0 2.00 10.0 -
Max 0.03 2.0 0.75 0.045 0.03 18.0 3.00 14.0 0.10
316H Min 0.04 0.04 0 - - 16.0 2.00 10.0 -
max 0.10 0.10 0.75 0.045 0.03 18.0 3.00 14.0 -

 

Mechanical Properties

Rooj 2.Mechanical zog ntawm 316 qib stainless hlau.

Qib Tensile Str (MPa) min Yield Str 0.2% Pov thawj (MPa) min Ntev (% hauv 50 mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
316 515 205 40 95 217
316L 485 170 40 95 217
316H 515 205 40 95 217

 

Lus Cim: 316H kuj muaj qhov yuav tsum tau ua rau cov nplej loj ntawm ASTM tsis muaj . 7 lossis coarser.

Lub cev muaj zog

Table 3.Cov khoom siv lub cev zoo rau 316 qib stainless hlau.

Qib Qhov ceev (kg / m3) Elastic Modulus (GPa) Txhais tau tias Co-eff ntawm Thermal Expansion (µm/m/degree) Thermal conductivity (W / mK) Kev kub ceev 0-100℃(J / kg.K) Elec Resistivity (nΩ)
0-100 degree 0-315 degree 0-538 ° C Ntawm 100 degree Ntawm 500 degree
316/L/H 8000 193 15.9 16.2 17.5 16.3 21.5 500 740

 

Qib Specification Sib piv

Rooj 4.Qib specifications rau 316 qib stainless hlau.

Qib UNS No Laus British Euronorm Swedish SS Japanese JIS
BS En Tsis muaj Lub npe
316 S31600 316S31 58H, 58J 1.4401 X5CrNiMo17-12-2 2347 TIAB SA 316
316L S31603 316S11 - 1.4404 X2CrNiMo17-12-2 2348 SUS 316L
316H S31609 316S51 - - - - -

 

Xa kev nug