Stainless Hlau Qib 2205 - Duplex High Strength Qib

Mar 23, 2026

Tso lus

How to calculate the service life of SS 316L heat exchanger tubes?UNS S30400 Stainless Steel – General-Purpose Corrosion-Resistant Core AlloyGrade 347H Stainless Steel – High‑Strength Niobium‑Stabilized Heat‑Resistant Alloy

 

Tshuaj muaj pes tsawg leeg

Cov lus hauv qab no teev cov alloy 2205 stainless hlau tshuaj muaj pes tsawg leeg raws li kev txheeb xyuas cam khwb cia.

   Tshuaj muaj pes tsawg leeg,%
Lub teb chawsSteel Qib (UNS)TxujC, ≤Si, ≤Mn, ≤P, ≤S, ≤CrNiMoN
Teb Chaws Asmeskas2205 (UNS S32205, UNS S31803)ASTM A276 / A276M; ASTM A240/A240M0,0301,002,000,0300,02022.0-23.04,5-6,53.0-3.50.14-0.20

Lub cev muaj zog

Nco tseg:

1 g/cm3=1 kg/dm3=1000 kg/m3;

1 μΩ·m=1 Ω·mm²/m

1 GPa=1 kN/mm2

Lub cev muaj zog
Ceev, g/cm3 (lb/in3)7,83 (0.283)
Melting point,℃(° F)1385-1440 (2525-2630)
Sib nqusYog lawm
Hluav taws xob tiv taus, μΩ·m0.85 (20 ° F) (68 ° F)
0.90 (100 degree) (212 ° F)
0.95 (200 degree) (392 ° F)
1.0 (300 degree) (572 ° F)
Lub peev xwm kub tshwj xeeb, J / (kg·K)470 (20 degree) (68 ° F)
500 (100 degree) (212 ° F)
530 (200 degree) (392 ° F)
560 (300 degree) (572 ° F)
Thermal conductivity, (W / m · K)15.0 (20 ° F) (68 ° F)
15.9 (100 degree) (212 ° F)
17.0 (200 degree) (392 ° F)
18.0 (300 degree) (572 ° F)
Modulus ntawm elasticity, Gpa190 (20 degree) (68 ° F)
180 (100 degree) (212 ° F)
175 (200 degree) (392 ° F)
171 (300 degree) (572 ° F)
Qhov nruab nrab coefficient ntawm thermal expansion, (10-6 / K)13.5 (20-100 ° F) (68 ° F - 212 ° F)
14.0 (20-200 ° F) (68 ° F - 392 ° F)
14.6 (20-300 degree) (68 ° F - 572 ° F)

Mechanical Properties

Duplex 2205 stainless hlau txhua yam khoom nyob rau hauv chav tsev kub nyob rau hauv ntau yam kev mob thiab tsis kam mus rau intergranular corrosion, xws li yield zog, tensile zog, thiab hardness, thiab lwm yam.

   Mechanical zog
Lub teb chaws (Region)TxujAISI Hom (UNS)0.2% pov thawj lub zog, MPa (ksi), ≥Tensile zog, MPa (ksi), ≥Elongation nyob rau hauv 50mm (2 nyob rau hauv.), % ≥Brinell Hardness (HBW), ≤Rockwell Hardness (HRC), ≥Cov xwm txheej & Ua tiav
Teb Chaws AsmeskasASTM A276/A276M2205 (UNS S32205, UNS S31803)450 (65)655 (95)25290-Annealed, kub-ua tiav lossis txias-ua tiav
ASTM A240/A240M450 (65)655 (95)2529331-