Mechanical Properties ntawm 316 Stainless hlau rau cov khoom lag luam txawv teb chaws

Mar 30, 2026

Tso lus

Q1: Lub zog tensile ntawm 316 stainless hlau yog dab tsi? A1: Lub zog tensile ntawm 316 stainless hlau yog hais txog 580MPa, uas yog siab dua li ntawm 304 stainless hlau (520MPa), thiab muaj zog txhua yam zoo dua.

Q2: Dab tsi yog qhov qis -kub toughness kev ua tau zoo ntawm 316 stainless hlau? A2: Nws muaj qhov zoo heev qis- qhov kub thiab txias, uas tseem tuaj yeem tswj tau qhov hnyav ntawm -253 degree, thaum 304 stainless hlau yuav ua nkig ntawm -196 degree.

Q3: 316 stainless hlau puas tuaj yeem ua kom tawv los ntawm kev kho cua sov? A3: Tsis yog, 316 stainless hlau yog austenitic stainless hlau, uas tsis tuaj yeem hardened los ntawm kev kho cua sov; nws cov khoom siv kho tshuab tsuas tuaj yeem hloov kho los ntawm kev ua haujlwm txias.

Q4: Dab tsi yog qhov ceev ntawm 316 stainless hlau? A4: Qhov ntom ntawm 316 stainless hlau yog 7.98g / cm³, uas yog tib yam li cov hlau tsis zoo austenitic, thiab nws yooj yim los xam cov khoom hnyav ntawm cov khoom lag luam txawv teb chaws.

Q5: Dab tsi yog qhov siab - qhov kub thiab txias ntawm 316 stainless hlau? A5: Nws tuaj yeem tswj hwm tus qauv austenitic ruaj khov ntawm 800 degree, thiab muaj kev tiv thaiv oxidation zoo thaum siv sib cuam tshuam ntawm 870℃thiab tsis tu ncua ntawm 925 degree.

 