Qib SUS410L Stainless Hlau
Feb 27, 2026
Tso lus
Kev piav qhia
Qib SUS410L yog qhov qis- carbon variant ntawm martensitic stainless hlau SUS410, optimized rau txhim kho weldability thiab intergranular corrosion kuj. Nrog rau cov ntsiab lus carbon txwv tsawg dua lossis sib npaug li 0.03%, nws txo qis chromium carbide nag lossis daus hauv tshav kub- cuam tshuam thaj tsam thaum vuam, tshem tawm qhov xav tau tom qab-weld heat treatment hauv feem ntau daim ntawv thov. SUS410L muaj 11.5-13.5% chromium, muab nruab nrab corrosion kuj nyob rau hauv atmospheric thiab tshuaj lom neeg ib puag ncig, thiab nws cov qauv martensitic ua rau nws sib nqus. Tsis zoo li tus qauv SUS410, SUS410L muaj qhov zoo dua ductility thiab weldability thaum tuav lub zog zoo thiab hnav tsis kam, tshwj xeeb tshaj yog tom qab kev kho cua sov. Nws yog tsim rau welded Cheebtsam uas yuav tsum tau nruab nrab corrosion kuj thiab tsis tau undergo tom qab vuam annealing, ua rau nws ib tug txhim khu kev qha kev xaiv rau industrial thiab mechanical daim ntaub ntawv qhov twg weld kev ncaj ncees yog ib qho tseem ceeb.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.03, Cr: 11.50-13.50, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.045, S Less dua lossis sib npaug 0.030, Ni Tsawg dua lossis sib npaug 0.75
Mechanical Properties
Tensile Strength Ntau dua los yog sib npaug rau 485 MPa, Yield Strength Ntau dua lossis sib npaug rau 170 MPa, Elongation Ntau dua lossis sib npaug li 20%, Hardness Tsawg dua lossis sib npaug rau 183 HB (annealed); Tensile Strength Ntau dua los yog sib npaug rau 690 MPa, Yield Strength Ntau dua lossis sib npaug rau 480 MPa, Elongation Ntau dua lossis sib npaug li 12%, Hardness Ntau dua lossis sib npaug rau 223 HB (kub- kho)
Qhov zoo
Superior weldability thiab intergranular corrosion kuj piv rau SUS410; zoo ductility thiab formability; Thaum tshav kub kub- kho tau los txhim kho lub zog thiab hnav tsis kam; Sib nqus; tus nqi- zoo; haum rau welded qauv.
Daim ntawv thov
Welded li qub, twj tso kua mis, shafts, fasteners, industrial machinery qhov chaw, thiab cov khoom uas yuav tsum tau muaj corrosion kuj thiab zoo weldability.
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug