Qib 439 Stainless Hlau
Feb 27, 2026
Tso lus
Kev piav qhia
Qib 439 yog titanium-stabilized ferritic stainless hlau, tsim los txhim kho intergranular corrosion kuj thiab weldability piv rau Qib 430. Nws muaj 17.0-19.0% chromium, muab zoo corrosion kuj nyob rau hauv atmospheric thiab me me tshuaj ib puag ncig, thiab yog sib nqus. Qhov sib ntxiv ntawm titanium (0.10-}0.30%) tiv thaiv chromium carbide nag lossis daus thaum lub sij hawm vuam thiab siab -kub raug, tshem tawm qhov xav tau tom qab-weld kev kho cua sov nyob rau hauv ntau daim ntawv thov. 439 muaj zoo formability, weldability, thiab machinability. Nws yog ib qho txiaj ntsig zoo rau cov qib austenitic rau cov ntawv thov uas yuav tsum tau muaj kev txhim kho corrosion thiab weldability zoo . 439 yog siv dav hauv cov tsheb siv hluav taws xob, cov khoom siv hluav taws xob, thiab cov khoom lag luam uas cov qauv welded muaj ntau thiab intergranular corrosion yog ib qho kev txhawj xeeb.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.07, Cr: 17.00-19.00, Mn Tsawg dua lossis sib npaug 1.00, Si Less dua lossis sib npaug 1.00, P Tsawg dua lossis sib npaug 0.040, S Less dua lossis sib npaug 0.030, Ti: 0.10-0.75 lossis sib npaug Ni
Mechanical Properties
Tensile Strength Ntau dua los yog sib npaug rau 450 MPa, Yield Strength Ntau dua lossis sib npaug rau 205 MPa, Elongation Ntau dua lossis sib npaug li 22%, Hardness Tsawg dua lossis sib npaug rau 183 HB
Qhov zoo
Intergranular corrosion kuj zoo dua 430; weldability zoo heev (tsis muaj ncej-weld kho cua sov yuav tsum tau nyob rau hauv feem ntau); zoo formability thiab machinability; Sib nqus; tus nqi- zoo; zoo siab -kub oxidation kuj.
Daim ntawv thov
Automotive exhaust systems, heat exchangers, furnace parts, ductwork, welded structures, and general-cov khoom siv hauv cov cheeb tsam me me.
Qib sib npaug
AISI 439, UNS S43900, EN 1.4510, GB 022Cr18Ti
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug