Qib 316 Stainless Hlau
316 yog molybdenum-cov kabmob austenitic stainless hlau, hloov kho dua tshiab ntawm 304, nrog kev txhim kho pitting thiab crevice corrosion kuj, tshwj xeeb tshaj yog haum rau chloride- thaj chaw nplua nuj.
Chemical Composition (wt%):C Less tshaj los yog sib npaug rau 0.08, Cr: 16.0-18.5, Ni: 10.0-14.0, Mo: 2.0-3.0, Mn Less tshaj los yog sib npaug rau 2.0, Si Less dua los yog sib npaug rau 1.0, P Less dua los yog sib npaug rau 0.045, S Less tshaj los yog sib npaug rau 0.0.
Mechanical Properties:Tensile zog Ntau tshaj los yog sib npaug rau 515MPa, Yield zog Ntau tshaj los yog sib npaug rau 205MPa, Elongation Ntau tshaj los yog sib npaug rau 40%, Hardness Tsawg dua los yog sib npaug rau 217 HB.
Kev Ua Haujlwm Zoo:Superior corrosion kuj (tshwj xeeb tshaj yog nyob rau hauv marine / tshuaj ib puag ncig) tshaj 304 series; zoo formability, weldability thiab tsawg-kub toughness.
Daim ntawv thov:Marine hardware, tshuaj ua khoom siv, khoom noj khoom haus machinery, kev tsim kho ntug hiav txwv dej, chaw ua tshuaj.
Qib sib npaug:AISI 316, UNS S31600, EN 1.4401, GB 06Cr17Ni12Mo2.
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug