Qib 310S Stainless Hlau - Ultra-High-Tsub Premium Alloy

Mar 19, 2026

Tso lus

Kev piav qhia

Qib 310S sawv cev rau qhov tseem ceeb ntawm cov pa austenitic stainless hlau kev ua tau zoo, tsim kom muaj qhov kub siab tshaj - ib puag ncig. Nrog 24.0-26.0% chromium thiab 19.0-22.0% npib tsib xee, nws muab qhov tshwj xeeb oxidation tsis kam ntawm qhov kub txog li 1100℃-qhov siab tshaj plaws ntawm cov hlau tsis zoo. Qhov qis -carbon "S" kev xaiv (tsawg dua lossis sib npaug li 0.08%) tiv thaiv kev nkag siab thiab ua kom cov weldability zoo heev, txawm tias cov ntu hnyav. Tsis zoo li cov txheej txheem kub-resistant qib, 310S tswj tshwj xeeb creep tsis kam thiab cov qauv kev ruaj ntseg ntawm ultra-siab kub, ua rau nws yog qhov kev xaiv tseem ceeb rau kev pabcuam txuas ntxiv hauv huab cua kub ib puag ncig.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.08, Cr: 24.00-26.00, Ni: 19.00-22.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.50, P Tsawg dua lossis sib npaug 0.045, S Tsawg dua lossis sib npaug 0.030

Mechanical Properties

Tensile Strength Ntau dua los yog sib npaug rau 515 MPa, Yield Strength Ntau dua lossis sib npaug rau 205 MPa, Elongation Ntau dua lossis sib npaug li 40%, Hardness Tsawg dua lossis sib npaug rau 217 HB

Qhov zoo

Superior ultra-siab-kub oxidation kuj; tshwj xeeb creep kuj ntawm 1100 degree; qis-carbon rau weld kev ncaj ncees; tsis yog-magnetic; zoo heev thermal stability.

Daim ntawv thov

Cov khoom siv rauv, qhov chaw incinerator, boiler superheaters, muaj cua sov tshuab, thiab siab - cov txheej txheem kub ua haujlwm ntawm 900-1100℃.

Qib sib npaug

UNS S31008, EN 1.4845, GB 06Cr25Ni20, SUS310S

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.