EN 1.4401 yog molybdenum- alloyed austenitic stainless hlau, sib haum rau AISI 316, muaj koob npe nrov rau nws cov kev tiv thaiv corrosion zoo tshaj hauv cov tshuaj chloride- muaj ib puag ncig. Nws muaj 16.0-18.0% chromium, 10.0-14.0% nickel, thiab 2.0-3.0% molybdenum- ib qho tseem ceeb ntxiv uas txhim kho pitting thiab crevice corrosion kuj, deb tshaj EN 1.4301. Nws cov qauv austenitic ruaj khov ua kom cov khoom tsis sib nqus ntawm chav tsev kub, thaum muab lub zog tensile zoo, ductility, thiab toughness - txawm tias qhov kub thiab txias. Tsis zoo li EN 1.4301, EN 1.4401 thrives nyob rau hauv marine, ntug hiav txwv dej, thiab tshuaj ib puag ncig, thaum tuav zoo formability thiab weldability. Nws yog qhov xav tau hloov kho dua tshiab rau cov ntawv thov uas tus qauv kev tiv thaiv corrosion tsis txaus, ntsuas kev ua tau zoo thiab kev ua haujlwm zoo.

Chemical Composition (wt%)

C Tsawg dua lossis sib npaug 0.08, Cr: 16.00-18.00, Ni: 10.00-14.00, Mo: 2.00-3.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug rau 0.04 lossis sib npaug 0.04 lossis sib npaug sib 0.11

Mechanical Properties

Tensile Strength Ntau dua los yog sib npaug rau 520 MPa, Yield Strength Ntau dua lossis sib npaug rau 205 MPa, Elongation Ntau dua lossis sib npaug li 40%, Hardness Tsawg dua lossis sib npaug rau 215 HB

Qhov zoo

Superior pitting / crevice corrosion kuj nyob rau hauv ib puag ncig chloride; ua tau zoo heev nyob rau hauv marine / tshuaj chaw; zoo tsawg-kub toughness; tsis yog-magnetic; yooj yim rau daim ntawv thiab weld; ruaj dua EN 1.4301 hauv cov xwm txheej hnyav.

Daim ntawv thov

Cov khoom siv hauv hiav txwv, cov tshuab ua tshuaj lom neeg, cov khoom siv ua zaub mov, cov khoom siv tshuaj, kev tsim kho ntawm ntug dej hiav txwv, thiab chloride- thaj chaw muaj kev lag luam nplua nuj.

Qib sib npaug

AISI 316, UNS S31600, GB 06Cr17Ni12Mo2, SUS316

 

Stainless hlau Suppliers

Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com

1.4547 Stainless Steel  bar1.4547 Stainless Steel coils1.4547 Stainless Steel plate

 

Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.

1.4547 Stainless Steel sheets1.4547 Stainless Steel strips

Xa kev nug