EN 1.4301 yog feem ntau siv austenitic stainless hlau raws li European EN tus qauv, lees paub tias yog European tus neeg ua haujlwm ntawm qib AISI 304. Nws tau ua kev zoo siab rau nws qhov tshwj xeeb sib npaug ntawm kev tiv thaiv corrosion, formability, weldability, thiab tus nqi -effectiveness, ua cov khoom siv pob zeb hauv ntiaj teb kev tsim khoom. Qib no yog tsim los tiv thaiv corrosion nyob rau hauv atmospheric, dej tshiab, thiab feem ntau me me corrosive ib puag ncig, thaum tuav zoo heev txias ua hauj lwm kev ua tau zoo thiab structural stability. Tsis zoo li cov alloys tshwj xeeb rau cov xwm txheej hnyav, EN 1.4301 tsom rau kev muab kev ntseeg siab, txhua yam - nyob ib puag ncig kev ua tau zoo, ua rau nws tsim nyog rau cov neeg siv khoom thiab cov khoom siv hnyav.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.08, Cr: 18.00-20.00, Ni: 8.00-11.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug 0.045, S Less dua lossis sib npaug 0.015, sib npaug
Tej yam cuab yeej cuab tam (Annealed Condition)
Tensile Strength (Rm): Ntau dua lossis sib npaug li 520 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 205 MPa; Elongation (A): Ntau dua lossis sib npaug li 40%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 201
Core Zoo
Kev sib xyaw ua ke zoo heev ntawm kev tiv thaiv corrosion, formability, thiab weldability, yoog mus rau ntau yam kev tsim khoom los ntawm stamping mus rau vuam; tus nqi- zoo rau kev tsim khoom loj thaum ua kom muaj kev tiv thaiv corrosion; tsis yog- sib nqus ntawm chav tsev kub, ua tau raws li cov ntawv thov electromagnetic tshwj xeeb; yooj yim kom ua tiav siab - zoo nto tiav (ci, iav-xws li) rau cov khoom siv kho kom zoo nkauj.
Daim ntawv thov
Cov dab dej hauv chav ua noj, cov khoom siv hauv tsev, cov kav dej hauv tsev, cov khoom siv ua zaub mov, cov thawv ntim tshuaj, cov khoom siv hauv tsev zoo tib yam, fasteners, thiab cov khoom siv stainless hlau txhua hnub.
Qib sib npaug
AISI 304, UNS S30400, GB 06Cr19Ni10, SUS304
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.