Kev sib piv ntawm Stainless Hlau 304 thiab 316L

Kev sib piv ntawm Stainless Hlau 304 thiab 316L
304 stainless hlau (18/8 chromium-nickel alloy) yog ib qho kev xaiv ntau yam thiab tsim nyog rau kev siv txhua hnub; thaum 316L stainless hlau (nrog ntxiv molybdenum thiab qis carbon cov ntsiab lus) muaj superior corrosion kuj, tshwj xeeb tshaj yog nyob rau hauv marine los yog hnyav tshuaj ib puag ncig, ua rau nws zoo tagnrho rau marine fittings, chemical processing equipment, thiab kho mob, txawm hais tias nws yog kim dua. Lub "L" hauv 316L sawv cev rau cov pa roj carbon tsawg, uas txo cov vuam corrosion thiab ua rau nws tsim nyog rau vuam ntau dua li tus qauv 316 stainless hlau.
Dab tsi yog 304 sawv cev hauv stainless hlau?
304 stainless hlau yog austenitic stainless hlau, feem ntau hu ua "18/8 stainless hlau" vim hais tias nws muaj pes tsawg leeg muaj tsawg kawg yog 18% chromium thiab 8% npib tsib xee. Nws muaj cov corrosion kuj zoo heev, formability, thiab durability, ua rau nws siv dav hauv cov khoom siv hauv chav ua noj, khoom noj khoom haus, cov khoom siv hauv tsev, thiab cov khoom siv dav siv . 304 stainless hlau paub txog nws cov khoom tsis yog- cov khoom sib nqus, yooj yim ntxuav, thiab tsis kam xeb thiab ntau yam tshuaj, txawm hais tias nws tuaj yeem raug rau pitting corrosion nyob rau hauv ib puag ncig chloride.

304 Stainless hlau
304 stainless hlau yog austenitic stainless hlau uas muaj kwv yees li 18% chromium thiab 8% mus rau 10.5% npib tsib xee. Qhov no muaj pes tsawg leeg muab zoo heev corrosion kuj thiab zoo formability.
304 stainless hlau paub txog nws lub zog tensile siab thiab oxidation tsis kam, ua rau nws haum rau ntau yam kev siv. Txawm li cas los xij, nws muaj qhov tsis zoo corrosion kuj nyob rau hauv ib puag ncig chloride piv rau 316 stainless hlau.
316L Stainless hlau
316L yog qhov tsawg- carbon variant ntawm 316 stainless hlau. Nws muaj cov ntsiab lus zoo sib xws tab sis nrog cov ntsiab lus siab tshaj plaws ntawm 0.03%.
Cov ntsiab lus qis dua yuav txo qhov kev pheej hmoo ntawm carbide nag lossis daus thaum vuam, ua 316L yog qhov kev xaiv zoo tshaj plaws rau kev siv vuam. Nws tuav tib yam corrosion kuj zoo li 316 stainless hlau tab sis ua tau zoo dua nyob rau hauv siab - qhov kub thiab txias.
Kev sib piv ntawm cov khoom ntawm 304 thiab 316L stainless hlau
| Khoom | 304 Stainless hlau | 316L Stainless hlau |
|---|---|---|
| Cov Cheebtsam | 18% Chromium, 8% Nickel | 16-18% Chromium, 10-14% Nickel, 2-3% Molybdenum, Tsawg Carbon (tsawg dua lossis sib npaug li 0.03%) |
| Cov ntsiab lus carbon | Tsawg dua lossis sib npaug li 0.08% | Tsawg dua lossis sib npaug li 0.03% |
Kev sib piv ntawm corrosion kuj ntawm 304 thiab 316L stainless hlau
| Khoom | 304 Stainless hlau | 316L Stainless hlau |
|---|---|---|
| Corrosion Resistance | Zoo, tiv taus atmospheric corrosion, dej, tsis muaj zog acids, thiab tsis muaj zog alkalis | Piv rau 316, nrog kev ua haujlwm zoo dua vuam thiab corrosion kuj ntawm welds. Resistant rau seawater, chlorides, thiab muaj zog corrosive media zoo li cov organic acids. |
| Pitting Resistance | Tsawg dua, nws yooj yim rau pitting hauv ib puag ncig chloride | Siab, piv rau 316; molybdenum zoo tiv thaiv pitting. |
| Crevice Corrosion Resistance | qis | Siab |
Corrosion Resistance:
304 stainless hlau nthuav tawm zoo corrosion kuj nyob rau hauv feem ntau ib puag ncig, tab sis yog raug rau chloride corrosion, tshwj xeeb tshaj yog nyob rau hauv marine los yog tshuaj ua ib puag ncig.
316L stainless hlau muaj kev tiv thaiv corrosion zoo tshaj, tshwj xeeb tshaj yog nyob rau hauv cov tshuaj chloride- nplua nuj ib puag ncig xws li marine ib puag ncig, ua rau nws zoo tagnrho rau cov ntug hiav txwv dej thiab tshuaj lom neeg kev lag luam.
Tensile zog:
304 stainless hlau: Tensile zog yog kwv yees li 505 MPa.
316L stainless hlau: Zoo ib yam li 316 stainless hlau, tab sis muaj zog me ntsis vim cov ntsiab lus qis dua.
Yield zog:
304 stainless hlau: Yield zog yog kwv yees li 215 MPa.
316L stainless hlau: Vim tias cov ntsiab lus qis dua, lub zog tawm los yog qis dua li ntawm 316 stainless hlau.
Hardness sib piv ntawm 304 thiab 316L stainless hlau:
| Khoom | 304 Stainless hlau | 316L Stainless hlau |
|---|---|---|
| Tensile zog | Ntau dua lossis sib npaug li 515 MPa | Ntau dua lossis sib npaug li 485 MPa |
| Yield zog | Ntau dua lossis sib npaug li 205 MPa | Ntau dua lossis sib npaug li 170 MPa |
| Elongation | Ntau dua lossis sib npaug li 40% | Ntau dua lossis sib npaug li 40% |
| Hardness | Siab dua, tab sis qis dua 316 | qis dua, yooj yim rau tshuab |
Daim ntawv thov thiab cov khoom tsim nyog rau 304 thiab 316L stainless hlau
| Kev thov cheeb tsam | 304 Stainless hlau | 316L Stainless hlau |
|---|---|---|
| Kev ua zaub mov | Dav siv nyob rau hauv cov khoom ua zaub mov, tableware, thiab kitchenware | |
| Kev lag luam tshuaj | Siv dav hauv cov khoom siv tshuaj lom neeg thiab cov kav dej | Siv rau hauv cov khoom siv tshuaj corrosive heev, piping, thiab ntim khoom |
| Marine Engineering | Tsis haum rau thaj chaw marine | Dav siv nyob rau hauv cov khoom siv marine, nkoj Cheebtsam, thiab subsea pipelines |
| Cov cuab yeej kho mob | Siv hauv cov cuab yeej kho mob thiab cov cuab yeej phais | Haum rau ib puag ncig corrosive heev hauv cov khoom siv kho mob |
| Kev tsim kho thiab kho kom zoo nkauj | Siv nyob rau hauv architectural kho kom zoo nkauj, railings, thiab handrails | Haum rau ib puag ncig corrosive heev nyob rau hauv architectural daim ntaub ntawv |
Vim li cas thiaj xaiv Gnee ua koj cov khoom siv stainless hlau?
✅ Tshaj 18 xyoo ntawm kev xa tawm, nrog cov khoom muag rau ntau tshaj 80 lub teb chaws
✅ ISO, SGS, thiab BV tau ntawv pov thawj
✅ Muaj thoob ntiaj teb Tshuag ntawm 304, 316, 316L, thiab 321 alloy kav, phaj, thiab tuav
✅ Customized processing services available, xws li txiav, polishing, CNC machining, thiab ntim
✅ Kev xa khoom sai hauv 7-15 hnub, txhawb nqa los ntawm cov neeg koom tes thoob ntiaj teb
📦 Ntim thiab Shipping
Tag nrho cov khoom siv stainless hlau tau ntim raws li hauv qab no:
Ntoo pallets lossis ntoo crates
Moisture -cov ntaub ntawv pov thawj
Sau npe nrog tus lej xov tooj cua sov, tus qauv, thiab qhov ntev
Shipped thoob ntiaj teb los ntawm hiav txwv, huab cua, los yog xa tawm
Gnee Steel yog ib lub chaw muag khoom ntawm Stainless Steel 304, muab ntau yam khoom xws li: Cov kav dej: Seamless kav: Qhov ntau thiab tsawg: 4 - 219 hli; Thickness: 0.5 - 20 hli; Welded kav: Qhov ntau thiab tsawg: 5.0 - 1219.2 hli; Thickness: 0.5 - 20 hli; Phaj: Phaj thickness 0.1 txog 100 hli; Phaj dav 10-2500 mm; Daim kab xev; Alloy round bars: Txoj kab uas hla 3-800 mm; Flat tuav: Thickness 2-100 mm; Dav: 10-500 mm; Hexagonal tuav: 2-100 hli; Hlau thiab extruded profiles. Peb koom tes nrog steel mills los muab peb cov neeg muas zaub nrog Stainless Steel 304, uas nws cov khoom ua tau raws li los yog ntau tshaj cov qauv kev lag luam, xws li ASTM, ASME, SAE, AMS, ISO, DIN, EN, thiab BS cov qauv.
Gnee Steel stocks thiab muag Stainless hlau 304, kav, raj, daim hlau, strips, nplooj ntawv, puag ncig tuav, tiaj tuav, forged billets, hexagonal steel, nyob ntawm tej, thiab extruded profiles. Thov koj xav tiv tauj peb ntawm email ntawmsales@gneestainless.comrau ib nqe lus.

Xa kev nug