ASTM A312 TP321 Stainless Hlau Bright Annealed Seamless Yeeb Nkab Rau Kev Lag Luam Roj
Nov 04, 2025
Tso lus
ASTM A312 TP321 seamless steel kav peb muab yog tsim los ntawm extruding kub steel billets, ua rau lub seamless raj yam tsis muaj pob qij txha los yog welds. Los ntawm ci ntsa iab annealing, cov kav dej ua tiav qhov chaw du thiab meej qhov ntev, ua rau lawv tsim nyog rau kev siv hauv petrochemical, siab - cov cuab yeej kub, thiab kev thauj mus los hauv xov xwm corrosive.
Cov kav dej no ua raws li cov qauv xws li ASME SA-312 thiab ASTM A312. EN 1.4541 (sib npaug rau TP321) cov kav dej tuaj yeem hloov kho ntau yam duab thiab ntau thiab tsawg raws li cov neeg siv khoom xav tau. Cov kav dej feem ntau yog siv rau hauv cov pob qij txha txuas ntxiv, cov khoom siv hluav taws xob sib hloov, cov khoom siv rau cov khoom siv hluav taws xob, cov khoom siv dav hlau dav hlau, cov tshuab raj, thiab cov ntawv siv zoo sib xws.
Yog tias koj muaj lus nug txog peb cov khoom lossis xav tau kev daws teeb meem, thov koj xav tiv tauj peb.Email:sales@gneestainless.com

Specification ntawm ASTM A312 TP321
| ASTM / ASME Specification | ASTM A312 / ASTM SA 312 Cov Lus Qhia |
| Dimensional Standards | ANSI/ASME B36.19M, ANSI/ASME B36.10M |
| Ntau hom thiab cov duab | Hydraulic, Square, Hex, Honed, Round, Rectangle |
| Feem ntau hom | 100% X Ray Welded, Seamless, CDW, Fabricated, ERW, Welded |
| Pipe End Hom | Plain Ib Kawg, Plain Ob Qhov Kawg, Bevel me kawg, Treaded ntawm kawg, Beveled kawg, Bevel ib kawg, Bevel loj kawg, Beveled ib kawg, Treaded Ob kawg, Bevel ob xaus |
| Technical Conditions ntawm Cov Yeeb Nkab | Cold Drawn, Bright Annealed, Annealed thiab Pickled, Polished |
| Mechanical Surface Finishing | 2B, No.4, No.1, No.8 Daim iav tiav lossis kev cai tiav raws li cov neeg siv khoom xav tau |
| Phab ntsa Thickness Schedule Chart |
SCH 5, SCH 10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
ASTM A312 TP321 Stainless hlau Bright Annealed Seamless Yeeb Nkab Siv Tshuaj Siv
| Qib | UNS npe | Cov pa roj carbon | Manganese | Phosphorus | Sulfur | Silicon | Chromium | Nickel | Nitrogen |
| TIAB SA 321 | S32100 | 0.08 | 2 | 0.045 | 0.03 | 1 | 17.0 - 19.0 | 9.0 - 12.0 | 0.1 |
ASTM A312 TP321 Tensile Requirements
| Qib | UNS npe | Tensile zog | Yield, min | ||
| ksi ua | MPa | ksi ua | MPa | ||
| TIAB SA 321 | S32100 | ||||
| Welded | 75 | 515 | 30 | 205 | |
| Seamless | |||||
| t Tsawg dua los yog sib npaug rau 0.375 in. [9.50 hli] |
75 | 515 | 30 | 205 | |
| t 0,375 ib. [9.50 hli] |
70 | 485 | 25 | 170 |
Annealing Requirements
| Qib | UNS npe | Thaum tshav kub kub kho kub | Cov Cuab Yeej Cuab Yeej / Kev Ntsuas Kev Ntsuas |
| TIAB SA 321 | S32100 | 1900℃F [1040 degree] | dej los yog lwm yam ceev ceev |
Yeeb thiab Filler Hlau Specification
| Qib | UNS npe | Filler Metal (AWS A5.9 Class) | UNS Lub Npe (Filler Metal) |
| TIAB SA 321 | S32100 | TIAB SA 321 |
S32180, W32140 |
ASTM A312 TP321 Bright Annealed Seamless Yeeb Nkab Nqe Sau
| Loj (OD × Phab ntsa Thickness) | Ntev (mm) | Nto tiav | Nqe (USD / Meter) | Txuj | Lus hais |
|---|---|---|---|---|---|
| 12.7 × 1.0 hli (1/2 ") | 6000 | Bright Annealed (BA) | $6.50 – $7.20 | ASTM A 312 Cov Lus Qhia | Hauv Tshuag |
| 19.05 × 1.5 hli (3/4 ") | 6000 | Bright Annealed (BA) | $8.20 – $9.00 | ASTM A 312 Cov Lus Qhia | Smooth sab hauv |
| 25.4 × 2.0 hli (1 ") | 6000 | Bright Annealed (BA) | $10.30 – $11.00 | ASTM A 312 Cov Lus Qhia | Uniform thickness |
| 38.1 × 2.5 hli (1-1/2 ") | 6000 | Bright Annealed (BA) | $14.50 – $15.50 | ASTM A 312 Cov Lus Qhia | Qib siab kub |
| 50.8 × 3.0 hli (2 ") | 6000 | Bright Annealed (BA) | $19.80 – $21.00 | ASTM A 312 Cov Lus Qhia | Tshuaj piping |
| 76.2 × 3.0 hli (3") | 6000 | Bright Annealed (BA) | $28.50 – $30.00 | ASTM A 312 Cov Lus Qhia | Welded los yog seamless |
| 101.6 × 3.6 hli (4 ") | 6000 | Bright Annealed (BA) | $36.00 – $38.50 | ASTM A 312 Cov Lus Qhia | Thaum tshav kub kub exchanger tube |
| 168.3 × 4.5 hli (6 ") | 6000 | Bright Annealed (BA) | $55.00 – $58.00 | ASTM A 312 Cov Lus Qhia | Customized txiav muaj |
Yog tias koj muaj qee qhov kev xav tau rau 321 stainless hlau kav, thov koj xav tso qhov kev txiav txim. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Lawv tuaj yeem ua tiav rau hauv ob qho tib si seamless thiab welded daim ntawv. Rau cov ncauj lus kom ntxaws tshuaj muaj pes tsawg leeg thiab kuaj dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email:sales@gneestainless.com
Ntim nrog cov ntawv tsis muaj dej thiab cov hlua hlau, ua tau raws li tus qauv xa tawm hiav txwv freight ntim, haum rau ntau txoj kev xa khoom, lossis kho raws li cov neeg siv khoom xav tau.