304 Stainless Steel Sheet for General Corrosion Resistance Applications304 Seamless Stainless Steel Pipe for Industrial Use201 Stainless Steel Sheet for Furniture Manufacturing

304 / 304L Stainless Hlau Tube

Hauv qab no yog cov khoom ntawm 304 / 304L stainless hlau kav uas muaj los ntawm Arch City Steel & Alloy, Inc.:

Cov khoom siv tawv hlau

Kev tiv thaiv corrosion siab

Kub kub kuj

Muaj peev xwm ua kom tsis muaj menyuam

High workability thiab machinability

Yooj yim welded los ntawm tag nrho cov txheej txheem kev lag luam

Qhov tshwm sim weld muaj zoo toughness thiab ductility

High annealing ntau, ntawm 1850℃thiab 2050℃F

Tsis yog-magnetic nyob rau hauv qhov mob annealed

Tsis hardened los ntawm kev kho cua sov

Hardness thiab tensile zog tuaj yeem nce los ntawm kev ua haujlwm txias

Kev ua haujlwm txias tuaj yeem ua rau cov hlau nplaum me ntsis

Zoo phab ntsa kam rau ua thiab straightness kam rau ua

Tus nqi -kev xaiv zoo rau feem ntau daim ntawv thov

 

Daim ntawv thov ntawm 304 / 304L Stainless hlau kav / Tubes

 

304 Stainless Steel Yeeb Nkab yog qhov tsim nyog tshaj plaws rau cov ntawv thov uas yuav tsum muaj lub zog zoo tshaj plaws thiab kev tiv thaiv corrosion zoo heev . 304 / 304L stainless hlau seamless kav tau txais dav hauv kev ua zaub mov, dej kho, petrochemical, chaw muag tshuaj, thiab tshuaj lom neeg kev lag luam rau kev txav cov kua thiab roj. Welded 304 / 304L stainless hlau raj / yeeb nkab yog qhov zoo tshaj plaws siv rau cov ncej, thiab cov ncej nrog rau cov tes tuav, sab nrauv thiab marine daim ntaub ntawv. 304 / 304L cov kav dej pom dav siv hauv cov ntawv thov uas xav tau vuam, machining, sib tsoo, sib sau, thiab polishing.

Vim tias lawv cov mills ua tiav thiab sab hauv welded seam, cov kav dej no tau siv dav rau cov haujlwm uas raug tshuaj lom neeg, acidic ntsiab lus, dej tshiab, thiab dej ntsev ib puag ncig.

 

COMPOSITION

 

Hom Tshuaj Chemical Composition % (max qhov tseem ceeb, tshwj tsis yog sau tseg)
Qhov hnyav% Cov pa roj carbon (C) Manganese (Mn) Phosphorus (P) Sulfur (S) Silicon (Si) Chromium (Cr) Nickel (Ni)
304 .08 2.00 .045 .030 1.00 18.0-20.0 8.0-11.0
304L .035 2.00 .045 .030 1.00 18.0-20.0 8.0-13.0