904L DIN1.4539 X1NiCrMoCuN25-20-5 Stainless Hlau Phaj Sheet

Mar 18, 2026

Tso lus

304 Austenitic Stainless Steel – All-Purpose Corrosion-Resistant Alloy For Everyday UseWhat is 1.4162 Stainless Steel?What is 1.4462 Stainless Steel?

Kev sib xyaw

Cov lus hauv qab no muab cov kev sib xyaw ua ke ntawm qib 904L stainless hlau:

Table 1. Muaj ntau yam ntawm qib 904L stainless hlau

Qib C Mn Si P S Cr Mo Ni Cu
904L

min.

max.

-

0.02

-

2

-

1

-

0.045

-

0.035

19

23

4

5

23

28

1

2

Mechanical Properties

Cov khoom siv kho tshuab raug ntawm qib 904L stainless hlau tau muab rau hauv cov lus hauv qab no:

Rooj 2. Mechanical zog ntawm qib 904L stainless hlau

Qib Tensile zog (MPa) min Yield Strength 0.2% Pov thawj (MPa) min Elongation (% hauv 50mm) min Hardness
Rockwell IB (HR B) Brinell (HB)
904L 490 220 36 70-90 Nws 150

Lub cev muaj zog

Lub cev lub cev ntawm qib 904L stainless hlau yog tabulated hauv qab no:

Table 3. Cov khoom siv lub cev zoo ntawm qib 904L stainless hlau

Qib Qhov ntom
(kg / m3)
Elastic Modulus
(GPa)
Txhais tau tias Co-eff ntawm Thermal Expansion (µm/m/degree) Thermal conductivity
(W/m.K)
Tshwj xeeb kub 0-100 degree
(J/kg.K)
Elec Resistivity
(nΩ.m)
0-100 degree 0-315 degree 0-538 ° C Thaum 20 degree Ntawm 500 degree
904L 7900 190 15 - - 11.5 - 500 952