410 Stainless Hlau Phaj|Daim ntawv
Mar 11, 2026
Tso lus



Cov ntsiab lus lag luam
| Cov ntsiab lus | Specification |
|---|---|
| Yam tsawg kawg nkaus Order Quantity: | 5 Tons |
| Nqe: | Yuav tsum sib tham |
| Ntim Cov Lus Qhia: |
Raws li thov |
| Lub sij hawm xa tuaj: | Hauv 7-10 Hnub Ua Haujlwm |
| Cov nqe lus them nqi: | T / T, L / C, Credit Card |
| Muaj peev xwm muab khoom: | 100000 Tons ib hlis twg |
| Ntawv pov thawj: | RoHS, BIS, SABS, tisi, KS, JIS, ISO9001 |
| Export rau: |
Tebchaws Asmeskas, Kaus Lim Kauslim, Lavxias Federation, United Kingdom, Is Nrias teb, Brazil, thiab lwm yam. |
Tshuaj muaj pes tsawg leeg
| Element | C | Mn | Si | Cr | Ni | P | S | Fe |
|---|
| Qhov sib txawv (%) | 0.08 – 0.15 | max 1.00 Nws | max 1.00 Nws | 11.50 – 13.50 | 0.75 max | 0.04 max | 0.03 max | Tshuav |