410/410s Kub Rolled Stainless Hlau Phaj
Feb 24, 2026
Tso lus



SS 410 Phaj Sib npaug Qib:
| Txuj | Werkstoff Nr. | UNS | JIS | EN |
|---|---|---|---|---|
| SIB 410 | 1.4006 | S41000 | SIB 410 | X12Cr13 |
Tshuaj muaj pes tsawg leeg ntawm 410 Stainless hlau phaj
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni |
|---|---|---|---|---|---|---|---|---|
| SIB 410 | Tsawg dua lossis sib npaug li 0.08-0.15 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua lossis sib npaug li 0.040 | Tsawg dua los yog sib npaug li 0.03 | 11.5-13.5 | – | 0.75 Max |
Mechanical Properties ntawm SS 410 Phaj
| Qib | Tensile zog | Yield zog | Elongation | Hardness | Khoov lub kaum sab xis |
|---|---|---|---|---|---|
| Kem 1 Tus nqi | >450 Mpa ib | >205 Mpa ua | > 20% | < HRB96 | 180 degree |
Nrhiav rau pem hauv ntej los ua ib qho ntawm koj cov kub dov 410/410s stainless hlau phaj lwm tus neeg nyob hauv Suav teb! Tiv tauj peb rau kub dov 410/410s stainless hlau phaj nqe!
Tiv tauj peb
410s Stainless Hlau Phaj Cov Ntaub Ntawv
410 (13Cr) muaj qhov zoo corrosion kuj thiab machining zog thiab yog ib tug dav - lub hom phiaj steel thiab tej cuab yeej steel . 410S yog qib steel uas txhim kho corrosion kuj thiab formability ntawm 410 steel . 410F2 yog ib tug txhuas- dawb- txiav hlau uas tsis txo cov corrosion kuj ntawm 1010 J yog 1010 siab-lub zog hlau uas ntxiv txhim kho corrosion kuj ntawm 410 stainless hlau thiab yog siv rau turbine hniav thiab siab - qhov kub thiab txias Cheebtsam.
410S Tib qib los ntawm txawv teb chaws tus qauv
S41008 SUS410S
Ss 410S Phaj Chemical Chemical Component:
| Qib | C | Mn | Si | P | S | Cr | Mo | Ni |
|---|---|---|---|---|---|---|---|---|
| SIB 410s | Tsawg dua los yog sib npaug li 0.08 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua los yog sib npaug rau 1.0 | Tsawg dua lossis sib npaug li 0.040 | Tsawg dua los yog sib npaug li 0.03 | 11.5-13.5 | – | 0.6 Max |