347 vs . 347H vs . 347HFG: Qhov txawv tseem ceeb
 

Kev xaiv ntawm 347, 347H, thiab 347HFG stainless hlau ncaj qha cuam tshuam rau cov khoom siv lub neej, kev ua haujlwm tsis zoo, vuam kev ua tau zoo, thiab ua raws li ASME boiler thiab lub nkoj siab. Xaiv qhov tsis ncaj ncees lawm qib yuav ua rau ua tsis tiav ntxov ntxov, nce nqi kho, lossis tsis lees paub thaum kuaj xyuas qhov project.

info-580-345

Dab tsi yog347 stainless hlau?

347 stainless hlau yog niobium (columbium) stabilized austenitic stainless hlau. Nws nta cov ntsiab lus siab tshaj plaws ntawm 0.08% thiab tsim nyog rau kev tiv thaiv corrosion thiab nruab nrab - qhov kub thiab txias txog li 800℃F (427℃). Nws yog dav siv nyob rau hauv hnyav welded khoom, aircraft tso tshuab, siab -kub tshuaj ua, thiab siab manufacturing industries.

Dab tsi yog347H cov khoom?

347H stainless hlau yog qhov siab - carbon version ntawm cov hlau, yuav tsum muaj cov ntsiab lus carbon ntawm 0.04% thiab 0.10%. Qhov siab dua cov pa roj carbon monoxide no ua kom muaj zog ntxiv thiab kev ntxhov siab- cov khoom tawg, ua rau nws zoo tagnrho rau ASME- tswj cov hlab ntsha ntawm qhov kub siab tshaj 1000℃F (540℃).

info-612-373
347HFG Stainless Steel

Dab tsi yog 347HFG stainless hlau?

347HFG yog ib qho khoom siv ruaj khov, niobium-stabilized austenitic stainless hlau tshwj xeeb tsim los rau siab - kev pabcuam kub. Qhov "H" nyob rau hauv qib qib qhia tau hais tias muaj cov ntsiab lus ntawm cov pa roj carbon monoxide uas txhais tau tias muab kev tiv thaiv zoo tshaj plaws, thaum "FG" sawv cev rau "Fine Grain." Qhov zoo no - cov qauv nplej muab cov khoom zoo tshaj - qhov kub thiab txias zog thiab ductility thaum txhim kho formability. Nws yog tshwj xeeb tshaj yog zoo- haum rau complex superheater thiab reheater raj hauv ultra-supercritical boilers.

 

 

ASTM A213 TP347 / TP347H / 347HFG Stainless Hlau Tubes Tshuaj Chemical Composition

Qib 347 347H 347 HFG
UNS npe S34700 S34709 S34710
Cov pa roj carbon (C) Max. 0.08 0.04–0.10 0.06–0.10
Manganese (Mn) Max. 2.00 2.00 2.00
Phosphorus (P) Max. 0.04 0.04 0.04
Sulfur (S) Max. 0.03 0.03 0.03
Silicon (Si) Max. 0.75 0.75 0.75
Chromium (Cr) 17.0–20.0 17.0–20.0 17.0–20.0
Nickel (Ni) 9.0–13.0 9.0–13.0 9.0–13.0
Molybdenum (hli) - -
Nitrogen (N) - - -
Hlau (Fe) Bal. Bal. Bal.
Niobium (Nb) txz|| |-- 1.10 8 xC-1.10 8 xC-1.10

 

Qhov txawv ntawm 347 thiab 347H yog dab tsi?

Thawj qhov sib txawv ntawm 347 thiab 347H stainless hlau yog lawv cov ntsiab lus carbon. Qib 347 yog niobium-stabilized austenitic stainless hlau nrog cov ntsiab lus siab tshaj plaws ntawm 0.08%, thaum 347H yog qhov siab -carbon version (0.04% mus rau 0.10%) tsim tshwj xeeb rau superior siab - qhov kub thiab txias tsis kam.

 

A213 TP347 TP347H 347HFG Stainless Hlau Mechanical Properties

      Tensile zog Tensile zog Yield zog Yield zog      
Alloy UNS Spec MPa ksi ua MPa ksi ua Elongation hauv 2 ntiv tes (min.)% Grain Size Req. Khaub ncaws
HBW
347 S34700 ASTM
A213
515 75 205 30 35 - 192
347H S34709 ASME SA 213 515 75 205 30 35 7 o rwj 192
347 HFG S34710 - 550 80 205 30 35 7 o rwj 192

 

347 vs . 347H vs . 347HFG: Kub kub

Khoom 347 Stainless hlau 347H Stainless hlau 347HFG Stainless hlau
Qhov siab tshaj qhov kev pabcuam kub Txog 870℃(1600℃F) Mus txog 900℃(1650℃F) Txog 950℃(1740℃F)
Pom zoo Ntev -Lub Sijhawm Ua Haujlwm Kub Tsawg dua lossis sib npaug li 550 degree 550-750 degree 600-850 degree

 

347 vs . 347H vs . 347HFG: Corrosion Resistance

Qib 347, 347H, thiab 347HFG nthuav tawm qhov sib piv tsis zoo rau kev cuam tshuam ntawm intergranular corrosion nyob rau hauv ob qho tib si annealed thiab welded tej yam kev mob. Txawm hais tias qib 347H thiab 347HFG muaj cov ntsiab lus carbon ntau dua (0.04% - 0.10% piv rau Tsawg dua lossis sib npaug li 0.08% rau qib 347), qhov yuav tsum tau ua rau ntau tshaj niobium kom ntseeg tau tias cov chromium txaus txaus los tuav cov zaj duab xis passive. Yog li ntawd, nyob rau hauv tus txheej txheem kev khiav hauj lwm tej yam kev mob, tsis muaj qhov sib txawv loj nyob rau hauv lawv susceptibility rau weld lwj los yog rhiab heev.

 

347 vs . 347H vs . 347HFG: Kev lag luam daim ntawv thov

Kev lag luam sector AISI 347 (Standard) AISI 347H (High Carbon) 347 HFG (Fine Grain)
Lub zog tiam Tsawg-siab boiler Cheebtsam thiab cov qauv kev txhawb nqa. Superheater thiab Reheater raj hauv cov pa roj carbon monoxide- raug rho tawm haujlwm. Ultra-Supercritical (USC) fais fab nroj tsuag boiler raj (High-pressure/High-heat).
Roj & Gas / Refinery Cov kua dej Catalytic Cracking (FCC) units, hydrocracker raj. Rauv cov kav dej, cov tshuab distillation, thiab siab -temp piping systems. Tshwj xeeb siab - kev pabcuam hydrogen thiab hnyav roj kho dua tshiab.
Aerospace Aircraft pa manifolds, dav hlau cav qhov chaw, thiab collector rings. Rocket engine Cheebtsam thiab siab - cua sov qauv fasteners. (Tsis tshua muaj siv nyob rau hauv aerospace; tsom rau qhov chaw ib puag ncig).
Kev ua tshuaj lom neeg Reactor hlab ntsha, cia tank rau cov organic chemicals/acids. High -kub tshuaj reactors thiab kub exchanger plhaub. Tshwj xeeb siab -temp tshuaj piping qhov chaw oxidation yog qhov txaus ntshai.
Automotive Hnyav- lub luag haujlwm tsheb thauj khoom thiab cov catalytic converter vaj tse. High -kev ua tau zoo ntawm kev sib tw tso pa tawm headers. (Tsis yog tus qauv rau tsheb).

 

Yuav Ua Li Cas Xaiv Ntawm 347, 347H thiab 347HFG?

Yog tias koj qhov project cuam tshuam nrog kev pabcuam txuas ntxiv siab dua 600℃lossis poob hauv ASME Tshooj I lossis siab - qhov ntsuas hluav taws xob tsim hluav taws xob, 347H lossis 347HFG feem ntau pom zoo tshaj tus qauv 347. Rau qhov xav tau tshaj plaws creep- cov ntawv thov kev pabcuam nrog kev tsim lub neej ntev, 347HFG muaj cov khoom siv zoo tshaj plaws rau lub sijhawm ntev dua -

 

347, 347H, thiab 347HFG Stainless Steel Heat Exchanger Tubes Chaw tsim tshuaj paus

GNEE Stainless Steel yog ib lub chaw tsim khoom tshwj xeeb ntawm cov hlau tsis muaj steel hlau kub exchanger tubs, ua cov qib xws li ASME SA213 TP347/TP347H, ASTM A312 347/347H, ASTM A213 347H (seamless), thiab EN 10216-5 (4510/1. Peb tsim seamless raj, U-tubes, thiab coiled tubing nyob rau hauv SA213 TP347 / TP347H specifications, nrog ib tug txheej txoj kab uas hla ntawm 6-530 hli, phab ntsa thickness ntawm 0.5-30 hli, thiab ntev mus txog 25,000 hli. Thov xa peb cov lus nug kom paub meej ntxiv. Peb tuav cov khoom lag luam dav dav ntawm 347/347H stainless hlau raj hauv Suav teb los txhawb cov haujlwm ceev.

Hu rau tam sim no

ASTM A213 TP347 Stainless Steel Pipe
ASTM A213 TP347 Stainless hlau yeeb nkab
347/347H Stainless Steel U-Tube
347/347H Stainless hlau U-Tube
347/347H Stainless Steel Coiled Tubing
347/347H Stainless Hlau Coiled Tubing