ASTM A213 TP347 SS Kub Exchanger Tube

ASTM A213 TP347 SS Kub Exchanger Tube

Txuj: ASTM A213 / ASME SA213
Qib: TP347
Kev tsim khoom: Cold Drawn lossis Cold Rolled
Tube Hom: Ncaj Tubes lossis U-Bent Tubes
Sab nraud txoj kab uas hla (OD): 1/2 "(12.7 mm) - 5" (127 mm)
Teem caij / Phab ntsa: BWG 14, 16, 18 los yog teev cov zauv thickness
Length: 6 meters, 12 meters, los yog customized Ib/ob chav Random Length.
Kev kho cua sov: Cov tshuaj Annealed ntawm min . 1900℃F (1040 degree) ua raws li sai quenching.
Nto tiav: Pickled & Annealed, Bright Annealed
Xaus: Plain Ends, Deburred
Qauv: Muaj
Thauj Pob: Txheem Hiav Txwv - Tsim nyog ntim
Xa kev nug
Tsham tam sim no

SS 347 Tube Chaw tsim khoom, ASTM A213 TP347 Tubes

Raws li ib tug ntawm cov ua manufacturers, lwm tus neeg, thiab exporters ntawm ASTM A213 stainless hlau seamless raj, GNEE Stainless hlau muab siab -zoo A213 TP347 stainless hlau tshav kub exchanger raj. Los ntawm cov tshuaj annealing ntawm 1060℃-1080 degree, peb lav qhov ruaj khov grain loj naj npawb ntawm 7 los yog coarser. Lub creep- tawg lub zog siab tshaj 60 MPa nyob rau hauv 700℃ib puag ncig, muab cov khoom muaj kev nyab xeeb rau siab -siab boiler ua haujlwm.

 

Peb kuj tseem tswj hwm cov niobium- rau- cov pa roj carbon piv saum toj 10 × C, kom ntseeg tau tias cov raj hla dhau ASTM A262 Practice E corrosion test nrog 100% kev ua tiav. Featuring zoo heev oxidation thiab corrosion kuj, tshwj xeeb tshaj yog nyob rau hauv siab - kub ib puag ncig mus txog 1500℃F, nws cov kev ua tau zoo tshaj qib 321 stainless hlau, ncua cov cuab yeej pab lub neej ntawm 25%.

 

Tsis tas li ntawd, cov txheej txheem Bright Annealing (BA) tau ua ntawm A213 TP347 stainless hlau hlab hauv qhov chaw ntshiab hydrogen kom ntseeg tau tias sab hauv qhov roughness (Ra) tsawg dua 0.8 μm. Daim iav no- qib kev huv huv zoo tiv thaiv cov pa roj carbon deposition thiab txo cov kua dej poob los ntawm kwv yees li 8-10% piv rau cov qauv pickled raj. Sab nraud txoj kab uas hla (OD) kam rau ua ntawm peb muab ASTM A213 TP347 stainless hlau round raj yog ± 0.08 hli (zoo tshaj rau tus qauv ± 0.15 hli), thiab phab ntsa thickness eccentricity yog tswj nyob rau hauv 5%. Qhov no ua kom 100% du haum nrog cov ntawv raj, txo koj lub sijhawm npaj vuam los ntawm 15-20%.

ASTM A213 TP347 Boiler Tube
Tom ntej: ASTM A213 TP347 Boiler Tube
ASTM A213 TP347 Superheater Tube
ASTM A213 TP347 Superheater Tube

 

Rau 347 SS U-tubes, peb ua qhov chaw hluav taws xob tiv thaiv kev ntxhov siab-kev kho cua sov ntawm qhov khoov thiab 300 hli ncaj raj ntu. Kev ntsuas hardness ua kom ntseeg tau tias qhov siab tshaj plaws hardness nyob rau hauv qhov kev hloov pauv tsis pub dhau 190 HV, ua kom muaj txiaj ntsig zoo ntawm kev pheej hmoo ntawm kev ntxhov siab corrosion cracking (SCC) nyob rau hauv siab - kub ua haujlwm.

ASTM A213 TP347 U Tube
ASTM A213 TP 347 U Tube
TP347 U-tubes for heat exchangers
TP347 U- raj rau cua sov exchangers

Specification

ASTM A213 SS 347 Seamless Tube Chemical Composition

UNS No Qib C Si Mn P S Cr Mo Ni N Lwm yam
S34700 347 0.08 0.75 2.00 0.045 0.030 17.00/19.00 – 9.00/13.00 – Cb:10xC1.00


ASTM A213 TP347 Stainless Hlau Seamless Tube Mechanical Properties

Element TIAB SA 347
Qhov ntom 8.0 g / cm3
Melting Range 1454℃(2650℃F)
Tensile Stress Psi - 75000, MPa - 515
Yield Stress (0.2% Tawm) Psi - 30000, MPa - 205
Elongation 35 %
Hardness (Brinell) 201

 

SS347 Tube ASTM A213 Tolerances

Specification Tso cai sab nraud qhov sib txawv hauv mm Tso cai phab ntsa Thickness Variation Exact Length Tolerance nyob rau hauv mm Kev sim
Nominal Dia Tshaj Hauv qab % Tshaj % Hauv qab Tshaj Hauv qab
ASTM -A213 TP347
Seamless Boiler
Superheater thiab
Thaum tshav kub kub Exchanger Tubes
Hauv qab 25.4 .1016 .1016 +20 -0 3.175 0 Flattening Test
25.4-38.1 Ib .1524 .1524 +22 -0 3.175 0 Kev Ntsuas Siab
38.1-50.8 Ib .2032 .2032 +22 -0 3.176 0 Flare Test
50.8-63.5 ib .254 .254 +2 -0 4.46 0 Hardness Test
63.5-76.2 ib .3478 .3478 +22 -0 4.76 0 100% Hydrostatic xeem
76.2-101.6 ib .381 .381 +22 -0 4.76 0 Xa mus rau ASTM A-450

 

Surface condition

ASTM A213 ASME SA-213 TP347 Stainless hlau raj yuav tsum tau khaws tsis muaj nplai.
Thaum ci annealing yog siv, pickling yog tsis tsim nyog.
Txhua qhov tshwj xeeb ua tiav yuav tsum tau ua raws li kev pom zoo ntawm tus neeg muag khoom thiab tus neeg yuav khoom.

Nyem kom tau txais cov qauv dawb 

 

Qhov kev pabcuam siab tshaj plaws ntawm TP347 raj yog dab tsi?

Qhov siab tshaj plaws kev pabcuam kub rau tus qauv TP347 (thiab TP347H) stainless hlau raj yog 1650℃F (899 degree) rau kev pabcuam txuas mus ntxiv hauv oxidizing ib puag ncig.Txawm li cas los xij, rau kev siv code ntev ntev (xws li hauv boilers lossis siab hlab ntsha hauv qab ASME Boiler thiab Pressure Vessel Code), qhov kev pom zoo siab tshaj plaws rau kev siv qhov kub thiab txias yog 15 mus rau 18 feem ntau txwv. mechanical thiab anti-sensitization zog.

 

Qhov txawv ntawm TP347 thiab TP347H yog dab tsi?

Thawj qhov sib txawv ntawm TP347 thiab TP347H yog lawv cov ntsiab lus carbon. TP347 muaj qhov siab tshaj plaws ntawm 0.08% carbon, thaum TP347H (qhov "H" qhia txog cov pa roj carbon ntau) muaj li ntawm 0.04% thiab 0.10% carbon. Cov ntsiab lus carbon siab dua no muab TP347H zoo dua nkag siab thiab siab - qhov kub thiab txias.

 

TP347 Stainless Hlau Boiler Tube Daim Ntawv Thov

TP347 seamless raj yog siv nyob rau hauv kev xav tau ib puag ncig qhov twg ob qho tib si corrosion kuj thiab siab - qhov kub thiab txias yuav tsum muaj:

Fais fab Generation Boilers: Superheater thiab reheater tubes, qhov twg chav kub tuaj yeem tshaj 600℃(1112℃F).

Thaum tshav kub kub Exchangers: Hauv kev ua tshuaj lom neeg, petrochemical, thiab roj & roj kev lag luam rau kev tuav cov txheej txheem corrosive ntws ntawm qhov kub siab.

Fossil Roj thiab Nuclear Fais Fab Cog: Rau cov khoom tseem ceeb uas raug rau siab - siab zog.

 

TP347 Stainless Steel Boiler Tube Application

 

ASTM A213 TP347 Tube Nqe Ib Kg

ASTM A213 TP347 tube nqi feem ntau yog li ntawm $ 4.00 txog $ 6.50 ib kg (los yog $ 4,000 txog $ 6,500 ib metric ton) rau kev txiav txim ntau. Khw muag khoom, kho, lossis me me hauv tsev tuaj yeem khiav ntawm $ 6.00 thiab $ 9.00 toj ib kg, nyob ntawm phab ntsa thickness, sab nraud (OD), thiab ntim khoom.

Nyem kom tau TP347/347H FOB nqi

Kev Tswj Xyuas Zoo

Peb ua 100% handheld spectroscopic PMI kuaj ntawm txhua lub raj, tsis yog cia siab rau random sampling.
Ntxiv rau qhov kev sim ntsuas hydrostatic, peb lub raj tau dhau 100% Eddy Current Testing (ECT) thiab Ultrasonic Testing (UT). Peb muaj peev xwm txheeb xyuas qhov tsis xws luag hauv me me li 5% ntawm phab ntsa tuab, ua kom xoom- tsis raug kev ncaj ncees nyob rau hauv siab - siab boiler kev ua haujlwm.

hydrostatic test 

Kev kuaj hydrostatic

347 SS Pipe PMI Test 

347 SS Yeeb Nkab PMI Test

zoo ntim

Peb cov kav dej SS 347 tau ntim rau hauv fumigated ntoo crates ntxiv nrog steel thav duab, muaj cov khoom sib cais sab hauv los tiv thaiv kev sib cuag thiab cuam tshuam ntawm cov kav dej. Peb siv siab -lub zog, inset yas kawg lub kaus mom muaj peev xwm tiv taus 50kg cuam tshuam; cov no xyuas kom meej cov yeeb nkab beveled xaus tswj zoo meej roundness, tso cai rau tam sim vuam thaum tuaj txog.
Txhua pob khoom ruaj ntseg nrog dual siab -lub zog nylon nqa pluaj los tiv thaiv qhov khawb nto los ntawm cov hlua hlau. Tsis tas li ntawd, txhua lub yeeb nkab yog laser- cim nrog tus cim QR code txuas nrog nws daim ntawv pov thawj Mill Test (MTC), ua rau koj ntawm - pab pawg neeg tuaj yeem tshawb xyuas cov xov tooj cua sov tam sim thiab cov ntaub ntawv ntsuas ntawm lub xov tooj ntawm tes.

TP347 Stainless Steel Seamless Pipe
TP347 SS Pipe
 

Cim npe nrov: ASTM A213 TP347 SS Heat Exchanger Tube, Tuam Tshoj ASTM A213 TP347 SS Heat Exchanger Tube manufacturers, lwm tus neeg, Hoobkas

Xa kev nug