SS 321 stainless hlau tshuaj muaj pes tsawg leeg yog teev nyob rau hauv cov lus hauv qab no raws li kev txheeb xyuas cam khwb cia.
| Tshuaj muaj pes tsawg leeg,% | |||||||||||
| ASTM Hom | AISI Hom (UNS) | C, Tsawg dua los yog sib npaug | Si, Less than or equal to | Mn, Tsawg dua lossis sib npaug | P, Tsawg dua los yog sib npaug | S, Tsawg dua los yog sib npaug | Cr | Ni | N, Tsawg dua los yog sib npaug | Lwm Yam Khoom | Sau ntawv |
| ASTM A240/A240M | 321 (NWS S32100) | 0.08 | 0.75 | 2.00 | 0.045 | 0.03 | 17.0-19.0 | 9.0-12.0 | 0.10 | Ntau dua lossis sib npaug rau Ti 5 × (C + N), Tsawg dua lossis sib npaug rau 0.70 | Phaj, Sheet, thiab Sawb rau Cov Nkoj Siab |
| ASTM A276A / 276M Cov Lus Qhia | 1.00 | – | Stainless hlau Bars thiab cov duab | ||||||||
| ASTM A580/A580M | – | Ntau dua lossis sib npaug Ti 5 × C | Stainless hlau hlau | ||||||||
| ASTM A959 Txuj | 0.10 | Ntau dua lossis sib npaug rau Ti 5 × (C + N), Tsawg dua lossis sib npaug rau 0.70 | Wrought Stainless hlau | ||||||||
| ASTM A473 Cov Khoom Siv Hluav Taws Xob | – | Ntau dua lossis sib npaug Ti 5 × C | Stainless hlau forgings | ||||||||
| ASTM A 314 Cov Lus Qhia Tshwj Xeeb | – | Ntau dua lossis sib npaug rau Ti 5 × (C + N), Tsawg dua lossis sib npaug rau 0.70 | Billets thiab bar rau forging | ||||||||
| ASTM A240/A240M | 321 H (UNS S32109) | 0.04-0.10 | 0.75 | 2.00 | 0.045 | 0.03 | 17.0-19.0 | 9.0-12.0 | 0.10 | Ntau dua lossis sib npaug rau Ti 4x (C + N), Tsawg dua lossis sib npaug rau 0.70 | Phaj, Sheet, thiab Sawb |
| ASTM A959 Txuj | 1.00 | 0.10 | Wrought Stainless hlau | ||||||||
| ASTM A312/A312M | TP 321 (UNS S32100) | 0.08 | 1.00 | 2.00 | 0.045 | 0.03 | 17.0-19.0 | 9.0-12.0 | 0.10 | Ntau dua lossis sib npaug rau Ti 5 × (C + N), Tsawg dua lossis sib npaug rau 0.70 | Stainless hlau kav |
| TP321H (UNS S32109) | 0.04-0.10 | 1.00 | 2.00 | 0.045 | 0.03 | 17.0-19.0 | 9.0-12.0 | 0.10 | Ntau dua lossis sib npaug rau Ti 4x (C + N), Tsawg dua lossis sib npaug rau 0.70 | ||