316H Austenitic Stainless Hlau - Siab -Temp Chloride-Resistant Alloy
Mar 18, 2026
Tso lus
Kev piav qhia
316H yog lub siab - carbon variant ntawm 316, engineered los ua ke cov tshuaj chloride corrosion ntawm 316 nrog enhanced siab - kub lub zog thiab creep kuj. Nrog rau cov pa roj carbon ntau ntawm 0.04-0.10%, nws ua tau zoo tshaj 316 thiab 316L hauv kev ua haujlwm ntev - lub sijhawm ua haujlwm ntawm qhov kub siab tshaj 500℃, thaum khaws cov molybdenum- txhim kho kev tiv thaiv corrosion uas ua rau 316 series zoo tagnrho rau qhov chaw hnyav. Tsis zoo li 304H, 316H muaj kev tiv thaiv zoo tshaj rau cov tshuaj chloride pitting thiab crevice corrosion, ua rau nws haum rau siab -kub siv nyob rau hauv corrosive settings{19}}xws li petrochemical nroj tsuag thiab cov chaw tsim hluav taws xob. Nws tseem tsis yog-sib nqus nyob rau hauv chav tsev kub, muaj weldability zoo, thiab muab kev txhim khu kev qha mechanical kev ua tau zoo nyob rau hauv lub thermal stress, ua rau nws ib tug tshwj xeeb tov rau high-kub, corrosive ib puag ncig.
Chemical Composition (wt%)
C: 0.04-0.10, Cr: 16.00-18.50, Ni: 10.00-14.00, Mo: 2.00-3.00, Mn Tsawg dua lossis sib npaug 2.00, Si Less dua lossis sib npaug 1.00, P Less dua lossis sib npaug rau 0.04 lossis sib npaug
Mechanical Properties
Tensile Strength Ntau dua los yog sib npaug rau 520 MPa, Yield Strength Ntau dua lossis sib npaug rau 205 MPa, Elongation Ntau dua lossis sib npaug li 40%, Hardness Tsawg dua lossis sib npaug rau 215 HB
Qhov zoo
Superior siab -kub creep zog vs. 316/316L; zoo heev chloride corrosion kuj; zoo oxidation tsis kam ntawm siab kub; tsis yog-magnetic; weldable; haum rau siab - cua sov, corrosive siab Cheebtsam.
Daim ntawv thov
High -kub tshuaj piping, petrochemical siab hlab ntsha, boiler raj, tshav kub exchangers, lub zog tsim khoom, thiab siab - cua sov corrosive industrial systems.
Qib sib npaug
AISI 316H, UNS S31609, EN 1.4406, GB 07Cr17Ni12Mo2, SUS316H
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj ntawm Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI daim ntawv ntsuam xyuas, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.