316 - Molybdenum-Txhim kho Austenitic Steel: Lub Benchmark rau Chloride Corrosion Resistance
Mar 31, 2026
Tso lus
Txheej txheem cej luam
316 yog cov khoom siv dav siv austenitic stainless hlau, txawv los ntawm nws cov molybdenum (2.00-3.00%) ntxiv uas ua rau muaj txiaj ntsig zoo rau pitting thiab crevice corrosion hauv chloride- muaj ib puag ncig. Ua los ntawm 16.00-18.00% chromium thiab 10.00-14.00% npib tsib xee, nws tsim ib lub ntsej muag ruaj khov-centered cubic austenitic qauv, ua kom cov khoom tsis sib nqus hauv lub xeev annealed. Cov qib no muaj cov ductility zoo heev, muaj peev xwm ua kom txias, thiab weldability, tsis tas yuav tsum tsis muaj preheating los yog tom qab vuam kub kho rau feem ntau siv. Piv nrog rau 304 stainless hlau, 316 muab superior corrosion kuj nyob rau hauv seawater, ntsev pos huab, thiab me me chemical media, ua rau nws cov kev xaiv rau nruab nrab corrosive tej yam kev mob nyob rau hauv industries.
Chemical Composition (wt%)
C Tsawg dua lossis sib npaug 0.08, Si Less dua lossis sib npaug rau 1.00, Mn Tsawg dua lossis sib npaug 2.00, P Tsawg dua lossis sib npaug 0.045, S Tsawg dua lossis sib npaug 0.030, Cr: 16.00-18.00, Ni: 10.00-14.00.
Tej yam cuab yeej cuab tam (Annealed Condition)
Tensile Strength (Rm): Ntau dua lossis sib npaug li 520 MPa; Yield zog (Rp0.2): Ntau dua lossis sib npaug rau 205 MPa; Elongation (A): Ntau dua lossis sib npaug li 40%; Brinell Hardness (HB): Tsawg dua lossis sib npaug rau 187
Core Zoo
Molybdenum ntxiv txhim khu pitting thiab crevice corrosion kuj nyob rau hauv ib puag ncig chloride; non- sib nqus thiab siab ductility rau txoj kev sib sau; txhim khu kev qha weldability nrog tsawg kawg nkaus ncej- ua; balanced zog thiab corrosion kev ua tau zoo; haum rau ntau hom kev siv corrosive nruab nrab.
Daim ntawv thov
Cov ntug dej hiav txwv architectural decorations, marine hardware, tshuaj siab hlab ntsha, khoom noj khoom haus thiab kws tshuaj, pulp thiab ntawv machinery, dej kho tshuab, thiab fasteners nyob rau hauv corrosive ib puag ncig.
Qib sib npaug
UNS S31600, STS316, SUS316, EN 1.4401, GB 06Cr17Ni12Mo2
Stainless hlau Suppliers
Yog tias koj muaj qhov project xav tau rau stainless hlau, peb txais tos koj xaj. GNEE muaj cov khoom muag loj ntawm cov khoom nrov rau koj xaiv. Nws tuaj yeem ua tiav rau hauv ntau yam khoom siv, nrog rau daim hlau, coils, raj, tuav, xov hlau, thiab lwm yam. Rau cov ncauj lus kom ntxaws txog cov tshuaj muaj pes tsawg leeg thiab cov qauv dawb, thov hu rau peb lub Hoobkas tam sim ntawd. Peb muab cov nqi sib tw thiab kev pabcuam zoo heev.Email: info@gneestainless.com



Kev xeem thiab cov ntaub ntawv: Daim ntawv pov thawj hauv Hoobkas, EN 10204 3.1, daim ntawv qhia tshuaj, daim ntawv qhia kev siv tshuab, daim ntawv ntsuam xyuas kev puas tsuaj, tsis yog- daim ntawv ntsuam xyuas kev puas tsuaj, PMI xeem tsab ntawv ceeb toom, daim ntawv ntsuam xyuas pom, daim ntawv ntsuam xyuas thib peb, NABL daim ntawv pov thawj kuaj.
Ntim: Ntoo crate ntim, npuas qhwv ntim, steel strapping, los yog ntim raws li tus neeg yuav tsum tau muaj.


Xa kev nug